daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Garnet Composite Solid Electrolyte with Cotton Modified by Metal Chelator as a Template for Flexible Solid-State Lithium Metal Batteries Garnet Composite Solid Electrolyte with Cotton Modified by Metal Chelator as a Template for Flexible Solid-State Lithium Metal Batteries AITranslate

Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Most current commercial lithium-ion batteries use organic electrolytes, which have considerable safety issues owing to their toxicity, easy combustion, degradation under high pressure, and corrosiveness. Therefore, safer lithium metal batteries with higher energy density have attracted considerable research attention. Composite solid-state electrolytes combining inorganic ceramics and organic polymers have superior performance; however, challenges such as low ionic conductivity, limited electrochemical windows, and low cycling stability remain to be addressed. Herein, we report a method of graft modification of cotton templates via the metal chelator EDTA (ethylenediaminetetraacetic acid). EDTA adsorbs metal ions from LLZO (Li7La3Zr2O12) precursors to prepare LLZO ceramic fabrics (LLZO CF) with cotton/EDTA as templates. Thus, LLZO ceramic fabric composite solid-state electrolytes (LLZO CF-CSE) with a double-layer cast structure are formed. This LLZO CF-CSE increases the lithium-ion conductivity (3.5 × 10–4 S cm–1 at 50 °C) and widens its electrochemical window (5.2 V). The initial specific capacity of a LiFePO4/Li battery with LLZO CF-CSE reaches 144.5 mAh g–1 at 50 °C, and the capacity remains at 117.6 mAh g–1 after 300 cycles, translating into a capacity retention rate of 99.44% under 1C charge/discharge conditions. Our work presents a method to prepare high-performance, safe, and stable cycling composite solid-state electrolytes.

KeyWords AITranslate

ceramic fabric cotton template metal chelator graft modification solidstate electrolyte lithium metal batteries
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00103

Chinese Library Classification Number:

Citation Information:

Most current commercial lithium-ion batteries use organic electrolytes, which have considerable safety issues owing to their toxicity, easy combustion, degradation under high pressure, and corrosiveness. Therefore, safer lithium metal batteries with higher energy density have attracted considerable research attention. Composite solid-state electrolytes combining inorganic ceramics and organic polymers have superior performance; however, challenges such as low ionic conductivity, limited electrochemical windows, and low cycling stability remain to be addressed. Herein, we report a method of graft modification of cotton templates via the metal chelator EDTA (ethylenediaminetetraacetic acid). EDTA adsorbs metal ions from LLZO (Li7La3Zr2O12) precursors to prepare LLZO ceramic fabrics (LLZO CF) with cotton/EDTA as templates. Thus, LLZO ceramic fabric composite solid-state electrolytes (LLZO CF-CSE) with a double-layer cast structure are formed. This LLZO CF-CSE increases the lithium-ion conductivity (3.5 × 10–4 S cm–1 at 50 °C) and widens its electrochemical window (5.2 V). The initial specific capacity of a LiFePO4/Li battery with LLZO CF-CSE reaches 144.5 mAh g–1 at 50 °C, and the capacity remains at 117.6 mAh g–1 after 300 cycles, translating into a capacity retention rate of 99.44% under 1C charge/discharge conditions. Our work presents a method to prepare high-performance, safe, and stable cycling composite solid-state electrolytes.

quote

GB/T 7714-2015 [1] Ying Zeng, Xingxing Zhai, Yingsong Yu, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00103.
MLA [1] Ying Zeng, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00103.
APA [1] Ying Zeng, Xingxing Zhai, Yingsong Yu, Dehua Li, & Yi Hu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00103
IEEE [1] Ying Zeng, Xingxing Zhai, Yingsong Yu, Dehua Li, and Yi Hu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00103. keywords: {ceramic fabric cotton template metal chelator graft modification solidstate electrolyte lithium metal batteries}