Present Status and Prospect of Surface Metallic Coating Technology of Cermet Particles AITranslate

Sichuan University;Sichuan University;Sichuan University;Sichuan University;Sichuan University;Sichuan University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

s:The paper has reviewed present status of the surface metal coating technology of cermet particles.Discussions are made on the basic principles,effect and application of various methods.It is pointed out that chemical plating and fluidized- bed CVD are well established now.The future development of the technology is prospected.

KeyWords AITranslate

ceramic particle surface metallic coating technology application prospect

1王玲.用化学镀实现陶瓷微粒表面金属化[J].材料保护,1998,31(7):16-17. 被引量:22

2王恩泽,鲍崇高,邢建东,祁小群.包镍Al_2O_3颗粒的获得及其在复合材料制备中的应用[J].西安交通大学学报,1999,33(1):84-87. 被引量:14

3刘兵海,古宏晨,丛德滋.粒子复合技术在材料制备技术中的应用[J].硅酸盐通报,1999,18(3):60-63. 被引量:6

4田彦文,邵忠财,翟玉春,李保山.化学镀法制备Ni包覆ZrO_2微粉[J].腐蚀科学与防护技术,1998,10(6):355-357. 被引量:10

5Takeshima Eiki et al.靶的运动机构[P].JP Pat:05194064.1993—08—06.

6何芬,胡永海.钴包碳化钨复合粉研制初探[J].稀有金属,1995,19(5):398-400. 被引量:1

7Vossen J L et al.薄膜加工工艺[M].北京:机械工业出版社,1987..

8李争显.表面技术的现状及新工艺[J].稀有金属快报,2001,20(8):1-5. 被引量:8

9Hojo Junichi.Preparation of metal-coated ceramics particles by agglomeration coating technique[J]. Journal of the Japan Society, of Powder and Powder Metallurgy, 1989, 36(4):411.

10Hojo Junichi, et al. Metal and carbide coatings of ceramics particles using chemical plating techniques[J] .Journal of the Japan Society of Powder and Powder Metallurgy, 1993, 40 (12):1 185.

1彭倩,邱绍宇,武兵书,郑学斌,张东博,姜超.碳化硼涂层材料研究进展[J].金属热处理,2005,30(10):7-13. 被引量:9

2刘猛,李顺,白书欣,赵恂,熊德赣.SiC_p/Cu电子封装材料研究进展[J].材料导报,2013,27(19):130-134. 被引量:9

1陈刚,章嵩,王传彬,沈强,张联盟.碳化硼陶瓷的放电等离子烧结及其力学性能[J].人工晶体学报,2009,38(1):165-169. 被引量:6

2杨水长,廖志君,刘振良,范强,伍登学,卢铁城.碳化硼薄膜的电子束蒸发制备及表面分析[J].稀有金属材料与工程,2009,38(A02):564-567. 被引量:4

3魏琪,高明,李辉,卢兰志.碳化硼对电弧喷涂涂层性能的影响[J].焊接学报,2010,31(11):65-68. 被引量:1

4王淑云,陆益敏,刘旭,黄国俊,郭延龙,万强,田方涛.碳化硼薄膜的激光法制备及性能[J].强激光与粒子束,2013,4(4):895-897. 被引量:3

5陈旭杰.(SiC_P+Gr_P)/Cu复合材料的制备与性能研究[J].热加工工艺,2014,43(8):117-119. 被引量:2

6苏明甫,廖志君,谢兰东,于小河,林涛,伍登学,卢铁城.电子束蒸发沉积制备碳化硼薄膜的化学结构研究[J].四川大学学报:自然科学版,2014,51(3):563-568. 被引量:1

7张贾伟,张国平,孙蓉,李世玮,汪正平.基于OLED器件的封装材料研究进展[J].集成技术,2014,3(6):92-101. 被引量:11

8燕振君,赵龙海,华鹏,李先芬,周伟.高硅铝合金脉冲激光焊接工艺研究[J].有色金属加工,2015,44(2):15-19. 被引量:3

9尚伦霖,王立平,张广安,蒲吉斌.磁控溅射沉积BC_x薄膜的摩擦学性能[J].中国表面工程,2015,28(5):16-23. 被引量:2

10冯翀龙,刘维良,李阳城,曾小军,徐兆良.水基流延B_4C陶瓷材料制备工艺研究[J].陶瓷学报,2015,36(5):511-515. 被引量:2

1У.,КИ,王颂才.自热鼓风炉熔炼的技术经济效果和应用前景[J].有色科技,1990(4):59-64.

2李雪静.电磁搅拌器的分类及应用[J].机械工程师,2014(7):248-249. 被引量:1

3何洪声.冶金反应工程学在喷射冶金技术中的应用[J].云南冶金,2001,30(1):26-31. 被引量:1

4刘强,李卫东,徐春柏,马光宇.轧钢加热炉综合节能技术浅析[J].冶金能源,2016,35(4):38-41. 被引量:10

5钱跃进,张永治,高里存.高铝矾土对镁质干式振动料抗熔渣渗透性能的影响[J].耐火材料,2006,40(2):153-154. 被引量:2

6刘柱领,王永春,邵勇.降低吨铝直流电耗的研究[J].世界有色金属,2012(9):41-43.

7刘建华,张杰,李康伟.气泡去除夹杂物技术研究现状及发展趋势[J].炼钢,2017,33(2):1-9. 被引量:16

Basic Information:

DOI:

Chinese Library Classification Number:TF213.74[冶金工程]

Citation Information:

s:The paper has reviewed present status of the surface metal coating technology of cermet particles.Discussions are made on the basic principles,effect and application of various methods.It is pointed out that chemical plating and fluidized- bed CVD are well established now.The future development of the technology is prospected.

quote

GB/T 7714-2015 [1] DONG Zhi-hong, FAN Hong-yuan, LI Wei, et al. Present Status and Prospect of Surface Metallic Coating Technology of Cermet Particles[J]. Rare Metals and Cemented Carbides, 2003(3): 27-30.
MLA [1] DONG Zhi-hong, et al., "Present Status and Prospect of Surface Metallic Coating Technology of Cermet Particles." Rare Metals and Cemented Carbides, no. 3, 2003, pp. 27-30.
APA [1] DONG Zhi-hong, FAN Hong-yuan, LI Wei, SHEN Bao-luo, XIANG Wen-xin, & YING Shi-hao. (2003). Present Status and Prospect of Surface Metallic Coating Technology of Cermet Particles. Rare Metals and Cemented Carbides(3), 27-30.
IEEE [1] DONG Zhi-hong, FAN Hong-yuan, LI Wei, SHEN Bao-luo, XIANG Wen-xin, and YING Shi-hao, "Present Status and Prospect of Surface Metallic Coating Technology of Cermet Particles," Rare Metals and Cemented Carbides, no. 3, pp. 27-30, 2003. keywords: {ceramic particle;surface metallic coating technology;application;prospect}