Electrodeposited Binder-free Mn-Co-S Nanosheets toward High Specific-Energy Aqueous Asymmetric Supercapacitors AITranslate
Abstract AITranslate
A simple single-step electrodeposition technique was followed for the three-dimensional (3D)-interconnected binary metallic manganese-cobalt sulfide nanosheets on nickel foam (MnCoS@NF). The architecture and chemical composition of the as-synthesized binder-free electrodes were analyzed by field-emission scanning electron microscopy (FESEM), high-resolution transmission electron microscopy (HRTEM), X-ray photoelectron spectroscopy (XPS), and X-ray diffraction (XRD). The MnCoS@NF achieves exceptionally high specific capacitance (1952.8 F g–1 at 2 A g–1) along with high cycle stability in a three-electrode cell measurement. Furthermore, an aqueous asymmetric supercapacitor (AAS) device was designed using electrodeposited MnCoS@NF in combination with reduced graphene oxide-coated NF (rGO@NF) as a positrode and negatrode, respectively. This device was able to provide very high specific energy (105.1 W h kg–1) at a specific power (7.25 kW kg–1) along with high cyclic stability (93.9% of specific capacitance retained after 3000 consecutive GCD cycles), which demonstrates its excellent candidature in supercapacitor applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00644
Chinese Library Classification Number:
Citation Information:
A simple single-step electrodeposition technique was followed for the three-dimensional (3D)-interconnected binary metallic manganese-cobalt sulfide nanosheets on nickel foam (MnCoS@NF). The architecture and chemical composition of the as-synthesized binder-free electrodes were analyzed by field-emission scanning electron microscopy (FESEM), high-resolution transmission electron microscopy (HRTEM), X-ray photoelectron spectroscopy (XPS), and X-ray diffraction (XRD). The MnCoS@NF achieves exceptionally high specific capacitance (1952.8 F g–1 at 2 A g–1) along with high cycle stability in a three-electrode cell measurement. Furthermore, an aqueous asymmetric supercapacitor (AAS) device was designed using electrodeposited MnCoS@NF in combination with reduced graphene oxide-coated NF (rGO@NF) as a positrode and negatrode, respectively. This device was able to provide very high specific energy (105.1 W h kg–1) at a specific power (7.25 kW kg–1) along with high cyclic stability (93.9% of specific capacitance retained after 3000 consecutive GCD cycles), which demonstrates its excellent candidature in supercapacitor applications.
quote
| GB/T 7714-2015 | [1] Manas Mandal, Krishna Chattopadhyay, Sarbaranjan Paria, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00644. |
| MLA | [1] Manas Mandal, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00644. |
| APA | [1] Manas Mandal, Krishna Chattopadhyay, Sarbaranjan Paria, Adwaita Kundu, Malay Chakraborty, Souvik Mal, Wonjae Shin, Sachindranath Das, Changwoon Nah, & Swapan Kumar Bhattacharya. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00644 |
| IEEE | [1] Manas Mandal, Krishna Chattopadhyay, Sarbaranjan Paria, Adwaita Kundu, Malay Chakraborty, Souvik Mal, Wonjae Shin, Sachindranath Das, Changwoon Nah, and Swapan Kumar Bhattacharya, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00644. keywords: {MnCoS nanosheets electrodeposition asymmetric supercapacitors specific energy rate capability} |