The Characteristics of High-entropy Alloys and their Latest Development AITranslate

School of Materials Science and Engineering, Xi'an University of Training and Technology;Department of Material Engineering, Sichuan Vocational and Technical College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Multi-principal element high-entropy alloy is introduced from its definition, properties and application. And the latest development of high-entropy alloy is emphatically reviewed, and its development orientation is pointed out.

KeyWords AITranslate

multi-principal element high-entropy alloy microstructure properties application the latest development

1Hsu Yu-Jui,Chiang Wen-Chi, Wu Jiann-Kuo. Corrosion behavior of FeCoNiCrCux high-entropy alloys in 3.5 sodium chloride solution[J]. Materials Chemistry and Physics, 2005,92: 112-117.

2Huang Ping- Kang, Yeh Jien- Wei. Effects of nitrogen content on structure and mechanical properties of multielement (AlCrNbSiTiV) N coating[J]. Surface & Coatings Technology, 2009,203 : 1 891-1 896.

3李伟,刘贵仲,郭景杰.AlFeCuCoNiCrTi_x高熵合金的组织结构及电化学性能[J].特种铸造及有色合金,2009(10):941-944. 被引量:29

4刘源,陈敏,李言祥,陈祥.Cr含量对AlTiFeNiCuCr_x多主元高熵合金凝固模式和微观结构的影响[J].特种铸造及有色合金,2008(S1):87-89. 被引量:8

5王春伟,唐健江,欧子义,苏广才,欧德群,夏薇.AlCoCrCuFeNi-x高熵合金微观组织及硬度的研究[J].铸造技术,2010,31(12):1584-1587. 被引量:12

6李安敏,张喜燕.AlCrCuFeNi高熵合金的组织与硬度研究[J].广西大学学报:自然科学版,2008,33(2):189-192. 被引量:13

7Shun Tao-Tsung, Hung Cheng-Hsin, Lee Che-Fu. The effects of secondary elemental Mo or Ti addition in Al0.3 CoCrFeNi high-entropy alloy on age hardening at 700 ℃ [J]. Journal of Alloys and Compounds, 2010,495:55-58.

8周云军,张勇,王艳丽,陈国良.多组元Al_x(TiVCrMnFeCoNiCu)_(100-x)高熵合金系微观组织研究[J].稀有金属材料与工程,2007,36(12):2136-2139. 被引量:15

9李亚峰,孔利军,甘章华,袁泽喜.FeNiMnCuC_(0.2)Al_x高熵合金结构及性能研究[J].武汉科技大学学报,2009,32(1):60-63. 被引量:5

10Tang Wei-Yeh, Chuang Ming-Hao, Chen Hsuan-You, et al. Microstructure and mechanical performance of new Al0.5 CrFe1. 5 MnNi0.5 high- entropy alloys improved by plasma nitriding[J]. Surface & Coatings Technology, 2010,204:3 118-3 124.

1安旭龙,刘其斌,郑波.激光熔覆制备高熵合金MoFeCrTiWAl_xSi_y涂层的组织与性能[J].红外与激光工程,2014,43(4):1140-1144. 被引量:22

2王智慧,秦晓婷,贺定勇,崔丽,蒋建敏,周正.等离子熔覆CoCrFeMnNiC_x高熵合金的组织结构[J].中国表面工程,2014,27(4):64-69. 被引量:9

3安旭龙,刘其斌,郑波.碳化钨对激光熔覆高熵合金的影响[J].强激光与粒子束,2014,26(12):249-254. 被引量:15

4张丽,沙明红,张峻巍,陈子尚,李胜利.Al含量对Al_xCoCrFeNiTi_(0.5)激光涂层组织和耐磨性的影响[J].材料热处理学报,2015,36(12):185-189. 被引量:13

5李栋梁,周芳,余师豪.激光熔覆FeCrNiMnMo_xB_(0.5)高熵合金涂层组织与耐蚀性能[J].强激光与粒子束,2016,28(2):190-195. 被引量:18

6安旭龙,刘其斌.WC颗粒对激光熔覆高熵合金SiFeCoCrTi涂层的组织及性能的影响[J].稀有金属材料与工程,2016,45(9):2424-2428. 被引量:12

7程一丹,要玉宏,陈建,王晓博.高熵合金Al_xFeCrCoNi微观组织与力学性能研究[J].西安工业大学学报,2018,38(2):140-146.

8曹振飞,齐海波,高珣,门晓玲.碳含量对CrMnFeCoNi高熵合金组织和性能的影响[J].应用激光,2018,38(3):367-371. 被引量:6

9梁方,吕连灏,竺培显,曾维平.铅/锡/钢层状复合材料的Miedema模型和Toop模型热力学分析[J].湖南有色金属,2019,35(1):44-47. 被引量:1

10薛雨杰,李双元,王正品,陈建.热轧对CoCrNi中熵合金微观组织和性能的影响[J].西安工业大学学报,2019,39(2):179-184. 被引量:7

1刘卫东,米国发,李雷.合金成分对激光熔覆高熵合金涂层影响的研究进展[J].特种铸造及有色合金,2022,42(7):847-855.

2王逸飞,张艳,王振旭,陈景润,陈德旭,张静,杨诗雨.热处理对氮间隙固溶CoCrFeMnNi高熵合金组织及性能的影响[J].特种铸造及有色合金,2022,42(1):55-59.

3刘径舟,刘洪喜,邸英南,蔺健全,郝轩宏,王悦怡,陈林,张晓伟.碳含量对激光熔覆CoCrFeMnNiC_(x)高熵合金涂层摩擦磨损和耐蚀性能的影响[J].中国表面工程,2020(6):118-127. 被引量:9

4张雪,崔洪芝,王明亮,赵玉桥,孙康.Al含量对Al_xCoCrFeNi系高熵合金组织和耐蚀性能的影响[J].材料热处理学报,2018,39(12):29-36. 被引量:9

5崔天晓,石岩.激光熔覆制备高熵合金的研究现状及发展趋势[J].机械工程师,2015(2):199-201. 被引量:7

6周芳,刘其斌,郑波.Si,Al对激光熔覆MoFeCrTiW高熵合金涂层组织性能的影响[J].强激光与粒子束,2015,27(11):266-271. 被引量:18

7王智慧,王兴阳,贺定勇,崔丽,周正,赵秋颖.等离子熔覆AlCoCrCuFeNiMnV_(0.2)C_x高熵合金的组织结构[J].材料热处理学报,2015,36(11):233-237. 被引量:2

8李刚,张井波,刘囝,宋艳东,郭玉洁,付晓帆.铬铁原矿粉激光制备高熵合金复合涂层的组织与性能[J].表面技术,2019,48(3):228-233. 被引量:2

9李栋梁,周芳,余师豪.激光熔覆FeCrNiMnMo_xB_(0.5)高熵合金涂层组织与耐蚀性能[J].强激光与粒子束,2016,28(2):190-195. 被引量:18

10周芳,刘其斌,郑波.Si、Al添加对MoFeCrTiW高熵合金涂层组织性能的影响[J].中国激光,2016,43(2):52-59. 被引量:11

1杨庚,王荣峰,吴瑞瑞.高熵合金的基础理论研究成果及应用[J].热加工工艺,2015,44(24):33-36. 被引量:11

2张霞,孙宏飞,郭娜娜,李冲.多主元高熵合金的研究进展[J].热加工工艺,2013,42(18):13-14. 被引量:16

3温丽华,寇宏超,王一川,常辉,李金山,胡锐,周廉.Al_xCoCrCuFeNi多主元高熵合金的组织与力学性能[J].特种铸造及有色合金,2009,29(6):579-581. 被引量:23

4李伟,刘贵仲,沈灿军,罗晓艳.多主元AlFeCuCoNiCrTi_(1.5)合金的研究[J].桂林电子科技大学学报,2009,29(2):117-121. 被引量:2

5罗晓艳,刘贵仲,吴鹏,钟文华.多主元AlFeCoNiCrV合金退火状态下硬度及电化学性能的研究[J].材料导报:纳米与新材料专辑,2010,24(2):546-548.

6陈敏,刘源,李言祥,陈祥.多主元高熵合金AlTiFeNiCuCr_x微观结构和力学性能[J].金属学报,2007,43(10):1020-1024. 被引量:52

7罗晓艳,刘贵仲,高原.多主元AlFeCoNiCrTiV_(0.5)高熵合金退火态的硬度及电化学性能[J].机械工程材料,2011,35(4):87-90. 被引量:5

8毛炜乾,刘贵仲,郭景杰,谢红波,郝聪敏.Al_xCoCrFeNi_2Ti_y高熵合金高温氧化行为的研究[J].稀有金属与硬质合金,2015,43(5):44-48. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG132[一般工业技术—材料科学与工程]

Citation Information:

Multi-principal element high-entropy alloy is introduced from its definition, properties and application. And the latest development of high-entropy alloy is emphatically reviewed, and its development orientation is pointed out.

quote

GB/T 7714-2015 [1] QIU Xing-wu, ZHANG Yun-peng. The Characteristics of High-entropy Alloys and their Latest Development[J]. Rare Metals and Cemented Carbides, 2012(1): 44-47.
MLA [1] QIU Xing-wu, and ZHANG Yun-peng. "The Characteristics of High-entropy Alloys and their Latest Development." Rare Metals and Cemented Carbides, no. 1, 2012, pp. 44-47.
APA [1] QIU Xing-wu, & ZHANG Yun-peng. (2012). The Characteristics of High-entropy Alloys and their Latest Development. Rare Metals and Cemented Carbides(1), 44-47.
IEEE [1] QIU Xing-wu and ZHANG Yun-peng, "The Characteristics of High-entropy Alloys and their Latest Development," Rare Metals and Cemented Carbides, no. 1, pp. 44-47, 2012. keywords: {multi-principal element high-entropy alloy;microstructure;properties;application;the latest development}