Facile Preparation of Ti3C2Tx MXene@Zn–Mn Ferrite Composites with Enhanced Microwave Absorption Performance AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology;Zhongshan Institute of Modern Industrial Technology of SCUT; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the development of the fifth-generation (5G) communication technology, electromagnetic wave pollution in the military and civilian fields is becoming increasingly severe. To achieve highly efficient electromagnetic wave absorption (EMA), electromagnetic wave absorbing materials must be studied, including composites with both electric and magnetic loss mechanisms. Here, Ti3C2Tx MXene@Zn–Mn ferrite (MXene@ZMF) composites were prepared by using a facile coprecipitation method incorporating magnetic ZMF nanoparticles coated onto the surface or inserted into the multilayers of MXene. The dielectric and magnetic losses and good impedance matching of these MXene@ZMF composites enhanced microwave absorption. The microwave absorption mechanism was established. The composite with 80 wt % MXene (denoted as MXene@ZMF-80%) exhibits enhanced EMA performance with a minimum reflection loss (RLmin) of −69.86 dB at a frequency of 16.93 GHz and a maximum effective absorption bandwidth of 2.32 GHz. Therefore, this work provides a simple method for the design and fabrication of hybrid microwave absorbers employing dielectric and magnetic losses, beneficial for solving electromagnetic pollution problems.

KeyWords AITranslate

MXene Zn−Mn ferrite composite electromagnetic wave absorption mechanism
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01168

Chinese Library Classification Number:

Citation Information:

With the development of the fifth-generation (5G) communication technology, electromagnetic wave pollution in the military and civilian fields is becoming increasingly severe. To achieve highly efficient electromagnetic wave absorption (EMA), electromagnetic wave absorbing materials must be studied, including composites with both electric and magnetic loss mechanisms. Here, Ti3C2Tx MXene@Zn–Mn ferrite (MXene@ZMF) composites were prepared by using a facile coprecipitation method incorporating magnetic ZMF nanoparticles coated onto the surface or inserted into the multilayers of MXene. The dielectric and magnetic losses and good impedance matching of these MXene@ZMF composites enhanced microwave absorption. The microwave absorption mechanism was established. The composite with 80 wt % MXene (denoted as MXene@ZMF-80%) exhibits enhanced EMA performance with a minimum reflection loss (RLmin) of −69.86 dB at a frequency of 16.93 GHz and a maximum effective absorption bandwidth of 2.32 GHz. Therefore, this work provides a simple method for the design and fabrication of hybrid microwave absorbers employing dielectric and magnetic losses, beneficial for solving electromagnetic pollution problems.

quote

GB/T 7714-2015 [1] Chi Yu, Junhao Peng, Jianhua Guo, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01168.
MLA [1] Chi Yu, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01168.
APA [1] Chi Yu, Junhao Peng, Jianhua Guo, Zhenhang Yin, Shixuan Lv, & Xinghua Jiang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01168