It is a challenge to make artificial muscles with tunable stiffness capacities. The key is to develop a composite with tunable stiffness as well as self-healing properties and stretchability. In this work, we design a composite with amorphous TiO2 particles and poly(dimethylsiloxane) (PDMS) matrix cross-linked with metal–ligand interactions. The PDMS matrix enables the composite to have self-healing properties and excellent stretchability, while the interactions between the TiO2 particles can be enhanced by applying an electric field, which provides the composite with an electric field-controlled stiffness. The tunable storage modulus increased by 180% at 4 kV/mm. The stiffness of a simply supported beam increased by 10.8% at 6 kV with respect to that at 0 kV. Based on its tunable stiffness, self-healing properties and stretchability, this composite can mimic many functions of human muscles and has promising applications as an artificial muscle.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01937
Chinese Library Classification Number:
Citation Information:
It is a challenge to make artificial muscles with tunable stiffness capacities. The key is to develop a composite with tunable stiffness as well as self-healing properties and stretchability. In this work, we design a composite with amorphous TiO2 particles and poly(dimethylsiloxane) (PDMS) matrix cross-linked with metal–ligand interactions. The PDMS matrix enables the composite to have self-healing properties and excellent stretchability, while the interactions between the TiO2 particles can be enhanced by applying an electric field, which provides the composite with an electric field-controlled stiffness. The tunable storage modulus increased by 180% at 4 kV/mm. The stiffness of a simply supported beam increased by 10.8% at 6 kV with respect to that at 0 kV. Based on its tunable stiffness, self-healing properties and stretchability, this composite can mimic many functions of human muscles and has promising applications as an artificial muscle.
quote
| GB/T 7714-2015 | [1] Zenghui Zhao, Sufeng Zhu, Bo Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01937. |
| MLA | [1] Zenghui Zhao, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01937. |
| APA | [1] Zenghui Zhao, Sufeng Zhu, Bo Li, Chenguang Niu, Yu Tong, Ning Ma, Xufeng Dong, Baoguo Han, Hao Huang, & Min Qi. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01937 |
| IEEE | [1] Zenghui Zhao, Sufeng Zhu, Bo Li, Chenguang Niu, Yu Tong, Ning Ma, Xufeng Dong, Baoguo Han, Hao Huang, and Min Qi, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01937. keywords: {selfhealing;tunable stiffness;stretchability;electrorheological elastomer;artificial muscles} |