Modification of the Co-assembly Behavior of Double-Hydrophilic Block Polyelectrolytes by Hydrophobic Terminal Groups: Ordered Nanostructures with Interpolyelectrolyte Complex Domains AITranslate
Abstract AITranslate
We report here the influence of hydrophobic terminal groups from RAFT chain transfer agent 4-cyano-4-[(dodecylsulfanylthiocarbonyl) sulfanyl]pentanoic acid on the co-assembly behavior of two oppositely charged double-hydrophilic block polyelectrolytes (DHBPs), poly{[2-(methacryloyloxy)ethyl]trimethyl ammonium iodide}-b-poly(N-isopropyl acrylamide) (QPDMAEMA-PNIPAm), with the dodecyl group at the end of the PNIPAm block, and poly(acrylic acid)-b-poly(N-isopropyl acrylamide) (PAA-PNIPAm). The co-assembly process was investigated using dynamic light scattering (DLS), differential scanning calorimetry (DSC), time-resolved small-angle X-ray scattering (SAXS), and cryo-transmission electron microscopy (TEM). The terminal dodecyl group of QPDMAEMA-PNIPAm induced hydrophobic association of PNIPAm coronas of QPDMAEMA-PNIPAm/PAA-PNIPAm core–corona particles into micrometer-sized aggregates. In ca. 2 s after mixing the DHBPs, the aggregates formed an ordered structure with constant distances (∼30 nm) between interpolyelectrolyte complex cores of the core–corona particles. This paper thus shows that a modification of double-hydrophilic block polyelectrolytes by low-molecular-weight hydrophobic terminal groups is a simple route for preparation of nanostructured networks of physically cross-linked nanoparticles with potential application as containers for encapsulation and delivery of multivalent ions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00033
Chinese Library Classification Number:
Citation Information:
We report here the influence of hydrophobic terminal groups from RAFT chain transfer agent 4-cyano-4-[(dodecylsulfanylthiocarbonyl) sulfanyl]pentanoic acid on the co-assembly behavior of two oppositely charged double-hydrophilic block polyelectrolytes (DHBPs), poly{[2-(methacryloyloxy)ethyl]trimethyl ammonium iodide}-b-poly(N-isopropyl acrylamide) (QPDMAEMA-PNIPAm), with the dodecyl group at the end of the PNIPAm block, and poly(acrylic acid)-b-poly(N-isopropyl acrylamide) (PAA-PNIPAm). The co-assembly process was investigated using dynamic light scattering (DLS), differential scanning calorimetry (DSC), time-resolved small-angle X-ray scattering (SAXS), and cryo-transmission electron microscopy (TEM). The terminal dodecyl group of QPDMAEMA-PNIPAm induced hydrophobic association of PNIPAm coronas of QPDMAEMA-PNIPAm/PAA-PNIPAm core–corona particles into micrometer-sized aggregates. In ca. 2 s after mixing the DHBPs, the aggregates formed an ordered structure with constant distances (∼30 nm) between interpolyelectrolyte complex cores of the core–corona particles. This paper thus shows that a modification of double-hydrophilic block polyelectrolytes by low-molecular-weight hydrophobic terminal groups is a simple route for preparation of nanostructured networks of physically cross-linked nanoparticles with potential application as containers for encapsulation and delivery of multivalent ions.
quote
| GB/T 7714-2015 | [1] Anastasiia Fanova, Irina Davidovich, Yeshayahu Talmon, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00033. |
| MLA | [1] Anastasiia Fanova, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00033. |
| APA | [1] Anastasiia Fanova, Irina Davidovich, Yeshayahu Talmon, Athanasios Skandalis, Stergios Pispas, & Miroslav Štěpánek. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00033 |
| IEEE | [1] Anastasiia Fanova, Irina Davidovich, Yeshayahu Talmon, Athanasios Skandalis, Stergios Pispas, and Miroslav Štěpánek, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00033. keywords: {micelles;hydrophilic block copolymers;electrostatic coassembly;polyelectrolytes;smallangle Xray scattering;cryogenic;Show More} |