Resistive Switching Properties in Memristors for Optoelectronic Synaptic Memristors: Deposition Techniques, Key Performance Parameters, and Applications Resistive Switching Properties in Memristors for Optoelectronic Synaptic Memristors: Deposition Techniques, Key Performance Parameters, and Applications AITranslate

University of Lakki Marwat; University of Lakki Marwat; University of Wisconsin; Tashkent State Pedagogical University Named after Nizami; United Arab Emirates University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Due to the fast evolution of information technology, high-speed and scalable memory devices are being investigated for data storage and data-driven computation. Resistive switching random access memory (RRAM) is one of the very popular types of memristors, because of its quick program/erase speed and high density as a result of its simple two-terminal structure, low power consumption, and low cost of fabrication. In this review, the market for promising memristor-based memories for smart systems is examined. The switching memory devices are described and classified according to their I–V behavior to underline the physical switching mechanisms. The various filament mechanisms of the RRAM memristor, including the valence change mechanism (VCM), electrochemical metallization mechanism (ECM), and thermochemical mechanism (TCM), are especially highlighted in various structures. The performance of resistive switching devices with different reported electrode materials and resistive layers is summarized. This study provides a detailed review of materials of the different deposition techniques used for surface modification and coating. The two major areas of interest, physical and chemical vapor deposition techniques and the influence parameter on the resistive switching, are discussed in detail. The prospective applications of RRAM memristors to various fields such as security, neuromorphic computing, and non-volatile logic systems for artificial intelligence are addressed briefly as well as the future outlook.

KeyWords AITranslate

hybrid heterostructures nanostructured materials optoelectronic synaptic device neuromorphic photonicsShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01323

Chinese Library Classification Number:

Citation Information:

Due to the fast evolution of information technology, high-speed and scalable memory devices are being investigated for data storage and data-driven computation. Resistive switching random access memory (RRAM) is one of the very popular types of memristors, because of its quick program/erase speed and high density as a result of its simple two-terminal structure, low power consumption, and low cost of fabrication. In this review, the market for promising memristor-based memories for smart systems is examined. The switching memory devices are described and classified according to their I–V behavior to underline the physical switching mechanisms. The various filament mechanisms of the RRAM memristor, including the valence change mechanism (VCM), electrochemical metallization mechanism (ECM), and thermochemical mechanism (TCM), are especially highlighted in various structures. The performance of resistive switching devices with different reported electrode materials and resistive layers is summarized. This study provides a detailed review of materials of the different deposition techniques used for surface modification and coating. The two major areas of interest, physical and chemical vapor deposition techniques and the influence parameter on the resistive switching, are discussed in detail. The prospective applications of RRAM memristors to various fields such as security, neuromorphic computing, and non-volatile logic systems for artificial intelligence are addressed briefly as well as the future outlook.

quote

GB/T 7714-2015 [1] Rajwali Khan, Naveed Ur Rehman, Shahid Iqbal, et al. ACS Applied Electronic Materials, 2024(6). DOI:10.1021/acsaelm.3c01323.
MLA [1] Rajwali Khan, et al., ACS Applied Electronic Materials, no. 6, 2024, https://doi.org/10.1021/acsaelm.3c01323.
APA [1] Rajwali Khan, Naveed Ur Rehman, Shahid Iqbal, Sherzod Abdullaev, & Haila M. Aldosari. (2024). ACS Applied Electronic Materials(6). https://doi.org/10.1021/acsaelm.3c01323
IEEE [1] Rajwali Khan, Naveed Ur Rehman, Shahid Iqbal, Sherzod Abdullaev, and Haila M. Aldosari, ACS Applied Electronic Materials, no. 6, 2024, doi: 10.1021/acsaelm.3c01323. keywords: {hybrid heterostructures nanostructured materials optoelectronic synaptic device neuromorphic photonicsShow More}