The prospect of rare earths separation with a new extractantCyanex 272 was predicted by comparison of Cyanex 272 with P204 andP507. The recent study of solvent extraction for rare earths separationby Cyanex 272 has been reviewed. Some suggestions for the study arepresen ted.
KeyWords AITranslate
1张瑞华.用乳状液膜从硫酸铵型浸出液中浓缩稀土[J].稀有金属与硬质合金,1996,24(4):12-16. 被引量:1
1罗仙平,邱廷省,严群,方夕辉.风化壳淋积型稀土矿的化学提取技术研究进展及发展方向[J].南方冶金学院学报,2002,23(5):1-6. 被引量:15
1曹妙康.直流电弧炉底电极及其相关技术的发展[J].上海金属,1995,17(2):13-20.
2王辅忠,李荣华,费英.高密度钨合金中沉淀相的研究进展[J].稀有金属与硬质合金,2002,30(4):39-41. 被引量:1
3朱立光,金山同.连铸保护渣研究动态述评[J].连铸,1997,0(5):38-42.
4张晨,刘世洲.去除废钢中的有色金属[J].钢铁研究,1998(3):60-63.
5王应群.金属萃取/湿法冶金的研究动向[J].世界有色金属,1992(4):9-13.
6高建祥,曲选辉,赵赛.金属粉末注射成形技术的最新研究动态与发展趋势[J].硬质合金,2003,20(1):56-60. 被引量:14
7蔡方寒,唐霞辉,秦应雄,李立波,朱国富.金刚石工具用预合金粉末的研究动态[J].金刚石与磨料磨具工程,2004,24(5):77-80. 被引量:25
8张廷安,赫冀成.自蔓延高温合成研究动态[J].中国有色金属学报,1998,8(S2):272-276. 被引量:2
9杜懋华.国外钢锭塑性加工研究动态[J].锡钢科技,1996(17):64-69.
10张晨,刘世洲.脱除废钢中有色金属的研究动态[J].辽宁冶金,1997(4):29-34.
Basic Information:
DOI:
Chinese Library Classification Number:TF845.042[冶金工程—有色金属冶金]
Citation Information:
The prospect of rare earths separation with a new extractantCyanex 272 was predicted by comparison of Cyanex 272 with P204 andP507. The recent study of solvent extraction for rare earths separationby Cyanex 272 has been reviewed. Some suggestions for the study arepresen ted.
quote
| GB/T 7714-2015 | [1] ZHANG Rui-hua, HU Rong-hua, NIE Da. The Application of New Extractant Cyanex 272 toSolvent Extraction of Rare Earths[J]. Rare Metals and Cemented Carbides, 1995(1): 19-24. |
| MLA | [1] ZHANG Rui-hua, et al., "The Application of New Extractant Cyanex 272 toSolvent Extraction of Rare Earths." Rare Metals and Cemented Carbides, no. 1, 1995, pp. 19-24. |
| APA | [1] ZHANG Rui-hua, HU Rong-hua, & NIE Da. (1995). The Application of New Extractant Cyanex 272 toSolvent Extraction of Rare Earths. Rare Metals and Cemented Carbides(1), 19-24. |
| IEEE | [1] ZHANG Rui-hua, HU Rong-hua, and NIE Da, "The Application of New Extractant Cyanex 272 toSolvent Extraction of Rare Earths," Rare Metals and Cemented Carbides, no. 1, pp. 19-24, 1995. keywords: {Cyanex272;solvent extractions;rare earths} |