Effect of Ti Content on Microstructure and Properties of U-Ti Alloy AITranslate

Institute of Materials,China Academy of Engineering Physics;Institute of Materials,China Academy of Engineering Physics;Institute of Materials,China Academy of Engineering Physics;Institute of Materials,China Academy of Engineering Physics;Institute of Materials,China Academy of Engineering Physics
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The samples of U-0.5%Ti,U-0.75%Ti and U-0.95%Ti alloys were prepared by vacuum induction melting,and then the effect of Ti content on alloy microstructure,room-temperature tensile perfor-mance and corrosion resistance was studied.The results show that the U-Ti alloys with the above three compositions have the microstructure mainly composited of acicular and biconvex lenticular martensite,and their main phases areα′and U2Ti.The grains of U-Ti alloy are gradually refined and the content of U2Ti phase increases with the increase of Ti content.As Ti content increases,the strength of U-Ti alloy gradually increases,while the plasticity gradually decreases,and the corrosion resistance slightly decreases.

KeyWords AITranslate

U-Ti alloy Ti content microstructure mechanical property corrosion resistance

1白彬,杨江荣,陆雷,鲜晓斌,郎定木,董平.铀表面Ti/Al复合镀层在腐蚀气体中的腐蚀行为[J].中国有色金属学报,2004,14(6):967-972. 被引量:6

2胡贵超,杨江荣,纪和菲,李丘林.旋转磁场下铀中夹杂物运动行为模拟与实验研究[J].热加工工艺,2015,44(1):69-72. 被引量:4

3邱志聪,邹东利,何立峰,赵雅文,肖大武,郭亚昆.贮存金属铀的力学性能及腐蚀行为[J].功能材料,2017,48(4):4127-4130. 被引量:1

4刘婷婷,张鹏程,何立峰,白彬.U-Ti合金的动态压缩性能及剪切特征[J].稀有金属材料与工程,2010,39(5):800-803. 被引量:5

5李鹏杰,初哲,周刚,王长利,胡玉涛,戴湘晖,杨慧,沈子楷,柯明.挤压态和时效态U-Ti合金动态压缩及绝热剪切性能研究[J].兵器材料科学与工程,2019,0(5):116-120. 被引量:2

1肖传民,舒德龙,谢君,侯桂臣,华涵钰.Hf对一种高W镍基合金组织及拉伸性能的影响[J].沈阳工业大学学报,2021,43(4):396-401. 被引量:1

2孙萌,姜周华,李阳,马帅,陈常勇,刘航.Ce-Mg复合处理对含硫齿轮钢SCr420H洁净度的影响[J].钢铁,2021,56(7):47-55. 被引量:5

3史永刚.交联改性对羽毛球拍胶粘剂性能的影响研究[J].粘接,2021,47(8):42-45. 被引量:2

4王璐钰,李玉琼,蔡榕.空间激光干涉仪光程倾斜耦合噪声抑制[J].光学精密工程,2021,29(7):1491-1498. 被引量:3

5郝建强,张金山,许春香,王红霞.B_(4)C对Mg-Zn-Y-Mn镁合金微观组织和力学性能的影响[J].材料热处理学报,2021,42(8):32-39. 被引量:1

6邹宗轩,刘政军,韩旭.W对Fe-Cr-C-W-B系堆焊合金组织和性能的影响[J].焊接学报,2021,42(7):91-96. 被引量:3

7杨飞雪,沈卓,刘恩泽,郭金花,宁礼奎,佟健,谭政,李海英,郑志.Si含量对选区激光熔化制备GH3536合金样品微观组织影响[J].有色矿冶,2021,37(4):38-40.

8胡家齐,王长军,魏来,杨哲,梁剑雄,董瀚.VIGA法与PREP法制备不锈钢粉末的内部孔洞对比研究[J].粉末冶金工业,2021,31(4):11-15. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG146.8[金属学及工艺—金属材料]

Citation Information:

The samples of U-0.5%Ti,U-0.75%Ti and U-0.95%Ti alloys were prepared by vacuum induction melting,and then the effect of Ti content on alloy microstructure,room-temperature tensile perfor-mance and corrosion resistance was studied.The results show that the U-Ti alloys with the above three compositions have the microstructure mainly composited of acicular and biconvex lenticular martensite,and their main phases areα′and U2Ti.The grains of U-Ti alloy are gradually refined and the content of U2Ti phase increases with the increase of Ti content.As Ti content increases,the strength of U-Ti alloy gradually increases,while the plasticity gradually decreases,and the corrosion resistance slightly decreases.

quote

GB/T 7714-2015 [1] WEI Yi-yun, XU Qing-dong, HU Gui-chao, et al. Effect of Ti Content on Microstructure and Properties of U-Ti Alloy[J]. Rare Metals and Cemented Carbides, 2021(4): 67-70.
MLA [1] WEI Yi-yun, et al., "Effect of Ti Content on Microstructure and Properties of U-Ti Alloy." Rare Metals and Cemented Carbides, no. 4, 2021, pp. 67-70.
APA [1] WEI Yi-yun, XU Qing-dong, HU Gui-chao, TANG Qing-fu, & WANG Zhen-hong. (2021). Effect of Ti Content on Microstructure and Properties of U-Ti Alloy. Rare Metals and Cemented Carbides(4), 67-70.
IEEE [1] WEI Yi-yun, XU Qing-dong, HU Gui-chao, TANG Qing-fu, and WANG Zhen-hong, "Effect of Ti Content on Microstructure and Properties of U-Ti Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 67-70, 2021. keywords: {U-Ti alloy;Ti content;microstructure;mechanical property;corrosion resistance}