Moiré Pattern Dislocation in Continuous Atomic Lattice of Monolayer h-BN Moiré Pattern Dislocation in Continuous Atomic Lattice of Monolayer h-BN AITranslate
Abstract AITranslate
Dislocations widely exist in two-dimensional (2D) materials and play an important role in the tunability of various properties. Although the atomic dislocations of 2D materials have been well analyzed, little is known about the dislocations of moiré patterns. Here, we report the atomic-resolution scanning tunneling microscopy studies of the moiré pattern dislocation in monolayer hexagonal boron nitride (h-BN) on Pt(111). The h-BN moiré pattern has three phases with different orientations. Intriguingly, the moiré pattern dislocations are observed, while the atomic lattices of h-BN are continuous across the step edges. These dislocations are related to the atomic lattice translation of the underneath Pt(111) substrate. Our findings provide an effective way to explore the moiré pattern dislocations, which could promote the research and application of 2D stacking superlattices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00013
Chinese Library Classification Number:
Citation Information:
Dislocations widely exist in two-dimensional (2D) materials and play an important role in the tunability of various properties. Although the atomic dislocations of 2D materials have been well analyzed, little is known about the dislocations of moiré patterns. Here, we report the atomic-resolution scanning tunneling microscopy studies of the moiré pattern dislocation in monolayer hexagonal boron nitride (h-BN) on Pt(111). The h-BN moiré pattern has three phases with different orientations. Intriguingly, the moiré pattern dislocations are observed, while the atomic lattices of h-BN are continuous across the step edges. These dislocations are related to the atomic lattice translation of the underneath Pt(111) substrate. Our findings provide an effective way to explore the moiré pattern dislocations, which could promote the research and application of 2D stacking superlattices.
quote
| GB/T 7714-2015 | [1] Huixia Yang, Teng Zhang, Meng Liu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00013. |
| MLA | [1] Huixia Yang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00013. |
| APA | [1] Huixia Yang, Teng Zhang, Meng Liu, Liwei Liu, Xu Wu, & Yeliang Wang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00013 |