Preliminary Research on the Extraction of Rare Earth Elements from Phosphate Rock with Ion Exchange Method AITranslate
Abstract AITranslate
Rare earth associated phosphate rock was dissolved with 55% nitric acid to obtain the digested solution,where rare earth elements were extracted with ion exchange method.Effects were studied of ion exchange time,eluent pH,EDTA concentration and calcium ion in the digested solution on rare earth extraction.The results show that the optimum technological conditions are as follows:ion exchange time of 50 min,eluent pH of 9.0,EDTA concentration of 0.020 mol/L and elution time of 50 min.Under the above conditions,rare earth adsorption rate of the resin can be up to 50%from the digested solution by one step ion exchange,and rare earth elution rate is beyond 94% by one step elution.Rare earth adsorption rate significantly increases after calcium is removed from the digested solution by concentrating and freezing.
KeyWords AITranslate
1金会心,王华,李军旗.磷矿资源及从磷矿中提取稀土的研究现状[J].湿法冶金,2007,26(4):179-183. 被引量:40
2殷宪国.贵州织金含稀土磷矿的开发与加工[J].磷肥与复肥,2010,25(1):76-78. 被引量:19
3ALY M M, MOHAMMED N A. Recovery of lantha- nides from Abu Tartur phosphate rock, Egypt[J]. Hy- drometallurgy, 1999,52(2) : 199-206.
4TORVALL M G, KHARALD S. Method of extracting rare earth elements from apatite.. US 764607[P]. 1980- 06-12.
5GALINAV Z, TATYANAN O. Method of extracting rare earth elements from apatite: US 1636337[P]. 1991- 06-19.
6TATYANAN G, GALINAV Z. Method of extracting rare earth elements from apatite: US 1736933[P]. 1992- 11-26.
7赵丽君,聂登攀,何灏,王振杰,薛安,吴素彬.盐酸浸出中低品位胶磷矿中稀土的研究[J].有色金属:冶炼部分,2014(4):45-47. 被引量:12
8谢子楠,陈前林,赵丽君.乳状液膜对磷矿酸解液中稀土离子的提取研究[J].中国稀土学报,2013,31(3):269-274. 被引量:12
9JAROSINSKI A, KOWALCZYK J, MAZANEK C Z. Development of the Polish wasteless technology of apa- tite phosphogypsum utilization with recovery of rare earths[J]. Journal of Alloys and Compounds, 1993,200 (1/2) :147-150.
10PRESTON J S, COLE P M, CRAIG W M, et al. The recovery of rare earth oxides from a phosphoric acid by- product[J]. Hydrometallurgy, 1996,41(1) : 1-19.
1曹佳伟,周夏芝,嵇友迪,葛谣,范佳俊,周钰康,彭银仙.稀土元素冶金技术研究进展[J].广州化工,2018,46(4):17-18. 被引量:1
2唐林旺,陆柳鲜,李雪蓉,麻欣宇,王俊峰,钟常明.低浓度稀土废水资源回收技术研究进展[J].现代矿业,2021,37(7):97-102. 被引量:3
3胡小洣,周洁英,伍莺,赖兰萍,张积锴,陈冬英.转型TP207树脂从低浓度稀土溶液中富集稀土的研究[J].中国稀土学报,2022,40(4):633-640.
4贺亚飞,弓爱君,孙金娥.稀土萃取分离技术方法研究[J].化学通报,2023,86(4):386-396.
1杨亚,欧梅桂,胡燕燕,罗定生,李仲卿,王涛.离子掺杂对纳米氧化钆发光强度及驰豫性能的影响[J].化工新型材料,2019,47(8):237-240.
2陈强.稀土生产线废水产出处理及其回收方法[J].数字农业与智能农机,2022(7):114-116.
3罗小娟,雷琼.基于膜技术处理离子型稀土矿开采废水的研究[J].有色金属科学与工程,2022,13(6):145-154.
4郑嘉辉,彭陈亮,王观石,罗进,秦磊.纤维状磁性二氧化钛复合材料的制备及其对La^(3+)的吸附行为[J].复合材料学报,2023,40(5):2804-2817.
1魏冰霞,刘常青,尹周澜,陈启元.乙二胺四乙酸对铝酸钠溶液种分附聚的影响[J].有色金属:冶炼部分,2010(6):23-25. 被引量:1
2高红霞,张建民.清洗鼓风炉水套水垢的实践[J].有色冶金节能,2010,25(2):16-18. 被引量:1
3孟文.可现场产生的非冷冻氮基烧结气氛[J].国外金属热处理,1995,16(1):55-57.
4文献,喻庆华,马荣骏.液膜萃取在稀土提取中的应用[J].稀有金属与硬质合金,1993,21(2):41-44. 被引量:1
5郎晓川,于秀兰.我国混合稀土精矿处理方法的研究进展[J].稀有金属与硬质合金,2009,37(3):43-47. 被引量:6
6曾令坚.离子型稀土提取工艺及设备的研究近况[J].有色冶金设计与研究,1990,11(3):35-38. 被引量:1
7尹邦跃,王零森,樊毅,张金生.乙二醇在络合物溶胶凝胶法中的作用[J].中南工业大学学报,1999,30(2):172-175. 被引量:6
8王则宏.提高铜电解净化系统能力浅析[J].大冶科技,1997(2):18-20.
9侯兴.新余2号锰铁高炉脱湿鼓风效果分析[J].炼铁技术通讯,2005,0(1):8-11. 被引量:1
10曾天元.关于我国稀土提取分离的进展、存在问题和改进途径初探[J].有色冶炼,1996,25(4):13-18. 被引量:12
Basic Information:
DOI:
Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]
Citation Information:
Rare earth associated phosphate rock was dissolved with 55% nitric acid to obtain the digested solution,where rare earth elements were extracted with ion exchange method.Effects were studied of ion exchange time,eluent pH,EDTA concentration and calcium ion in the digested solution on rare earth extraction.The results show that the optimum technological conditions are as follows:ion exchange time of 50 min,eluent pH of 9.0,EDTA concentration of 0.020 mol/L and elution time of 50 min.Under the above conditions,rare earth adsorption rate of the resin can be up to 50%from the digested solution by one step ion exchange,and rare earth elution rate is beyond 94% by one step elution.Rare earth adsorption rate significantly increases after calcium is removed from the digested solution by concentrating and freezing.
quote
| GB/T 7714-2015 | [1] ZH OU, OU J, J un-hong, et al. Preliminary Research on the Extraction of Rare Earth Elements from Phosphate Rock with Ion Exchange Method[J]. Rare Metals and Cemented Carbides, 2016(5): 11-15. |
| MLA | [1] ZH OU, et al., "Preliminary Research on the Extraction of Rare Earth Elements from Phosphate Rock with Ion Exchange Method." Rare Metals and Cemented Carbides, no. 5, 2016, pp. 11-15. |
| APA | [1] ZH OU, OU J, J un-hong, CAI Xian-j, RUAN Dai-tan, & TIAN Xian-li. (2016). Preliminary Research on the Extraction of Rare Earth Elements from Phosphate Rock with Ion Exchange Method. Rare Metals and Cemented Carbides(5), 11-15. |
| IEEE | [1] ZH OU, OU J, J un-hong, CAI Xian-j, RUAN Dai-tan, and TIAN Xian-li, "Preliminary Research on the Extraction of Rare Earth Elements from Phosphate Rock with Ion Exchange Method," Rare Metals and Cemented Carbides, no. 5, pp. 11-15, 2016. keywords: {rare earth extraction;rare earth associated phosphate rock;ion exchange method;dissolution with nitric acid;elution with EDTA(ethylenediaminetetraacetic acid);calcium removal by freezing} |