Abstract AITranslate

3D-printing technology has brought light to the large-scale and sustainable production of a wide range of low-cost electronic devices with custom forms on-demand. Despite the current availability of mainstream carbon-based nanocomposite filaments, 3D-printing of noble metals is nowadays a challenge. Herein, a one-step functionalization approach has been devised for the straightforward and cost-effective manufacturing of functional metal-based 3D-printed electronics by galvanically replacing Cu-based 3D-printed (3D-Cu) electrodes with nobler metal counterparts, viz. Ag and Au. As a first demonstration of applicability, two appealing bio-electroanalytical approaches, such as the chiral discrimination of amino acids and the supramolecular determination of uranium have been considered —by taking advantage of the capability of noble metals to physically/chemically accommodate several molecular components—, reaching enhanced performances when compared with the pristine 3D-Cu counterpart. Consequently, this alchemy-inspired approach, which combines (i) 3D-Cu electrodes as sacrificial platforms with (ii) noble metals via a galvanic exchange reaction, provides a robust pathway to harbor molecular components in order to exploit metal-based 3D-printed electronics in real tasks. Graphical abstract Download : Download high-res image (128KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2022.101519

Chinese Library Classification Number:

Citation Information:

3D-printing technology has brought light to the large-scale and sustainable production of a wide range of low-cost electronic devices with custom forms on-demand. Despite the current availability of mainstream carbon-based nanocomposite filaments, 3D-printing of noble metals is nowadays a challenge. Herein, a one-step functionalization approach has been devised for the straightforward and cost-effective manufacturing of functional metal-based 3D-printed electronics by galvanically replacing Cu-based 3D-printed (3D-Cu) electrodes with nobler metal counterparts, viz. Ag and Au. As a first demonstration of applicability, two appealing bio-electroanalytical approaches, such as the chiral discrimination of amino acids and the supramolecular determination of uranium have been considered —by taking advantage of the capability of noble metals to physically/chemically accommodate several molecular components—, reaching enhanced performances when compared with the pristine 3D-Cu counterpart. Consequently, this alchemy-inspired approach, which combines (i) 3D-Cu electrodes as sacrificial platforms with (ii) noble metals via a galvanic exchange reaction, provides a robust pathway to harbor molecular components in order to exploit metal-based 3D-printed electronics in real tasks. Graphical abstract Download : Download high-res image (128KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Jose Muñoz, Edurne Redondo, Martin Pumera. Applied Materials Today, 2022(28). DOI:10.1016/j.apmt.2022.101519.
MLA [1] Jose Muñoz, et al., Applied Materials Today, no. 28, 2022, https://doi.org/10.1016/j.apmt.2022.101519.
APA [1] Jose Muñoz, Edurne Redondo, & Martin Pumera. (2022). Applied Materials Today(28). https://doi.org/10.1016/j.apmt.2022.101519
IEEE [1] Jose Muñoz, Edurne Redondo, and Martin Pumera, Applied Materials Today, no. 28, 2022, doi: 10.1016/j.apmt.2022.101519.