Latest Development of Transitional Metal Carbide Additives in Ti(C,N)-based Cermet AITranslate

National Key Laboratory of Powder Metallurgy of Central South University;National Key Laboratory of Powder Metallurgy of Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Description is made of the typical structure of the Ti(C, N)-based cermet, focusing on the influ- ence of the additives of transitional metal carbide, such as nano-crystal TiC/TiN, Mo2C,WC,TaC, NbC, VC,CraC2 on the microstructure and mechanical property of Ti(C,N)-based cermet. It is feasible to pro- duce Ti(C,N)-based cermet with excellent performance by proper addition of carbide additives.

KeyWords AITranslate

Ti (C N) cermet transitional metal carbide additive latest development

1Mari D,Bolognini S,Feusier G,etal. TiMoCN based cermets part Ⅱ microstructure and room temperature mechanical properties[J]. International Journal of Refractory Metals & Hard Materials,2003,21:47-53.

2Mari D, Bolognini S, Feusier G, et al. TiMoCN based cermets part Ⅰ morphology and phase composition[J]. Inter national Journal of Refractory Metals & Hard Materials,2003,21:37-46.

3Ning Liu,Sheng Chao, Xinming Huang. Effects of TiC/ TiN addition on the microstructure and mechanical properties of ultra-fine grade Ti (C,N)-Ni cermets[J]. Journal of the European Ceramic-Society, 2006,26:3 861- 3 870.

4Yong Zheng, Weihao Xiong, Wenjun Liu,et al. Effect of nano addition on the microstructures and mechanical properties of Ti ( C, N) - based cermets[J]. Ceramics International, 2005,31 : 165-170.

5Yong Zheng,Shengxiang Wang, Min You,et al. Fabrication of nanocomposite Ti (C, N)-based cermet by spark plasma sintering[J]. Materials Chemistry and Physics, 2005,92:64-70.

6Russias J, Cardinal S, Aguni Y, et al. Influence of titanium nitride addition on the microstructure and mechanical properties of TiC-based cermets[J]. International Journal of Refractory Metals & Hard Materials, 2005,23: 358-362.

7WANG Saiyu,XIONG Weihao,YAN Mingshuang,FAN Chou.Effects of molybdenum on the microstructure and mechanical properties of Ti(C,N)-based cermets with low Ni[J].稀有金属:英文版,2006,25(1):90-95. 被引量:17

8Ji Xiong, Zhixing Guo, Baoluo Shen, et al. The effect of WC, Mo2 C, TaC content on the microstructure and properties of ultra-fine TIC0.7 N0.3 cermet [J]. Materials and Design,2007,28(5) :1 689-1 694.

9何林,黄传真,黄勤,宋世学,王随莲,艾兴.Mo_2C含量对Ti(C,N)基陶瓷力学性能和显微结构的影响[J].材料科学与工程学报,2003,21(2):238-241. 被引量:10

10Jinkwan Jung,Shinhoo Kang. Effect of ultra-fine powders on the microstructure of Ti(CN)-xWC-Ni cermets [J]. Acta Materialia,2004,52:1 379-1 386.

1李平平,叶金文,刘颖,邹洪伟,杨嘉.低压烧结温度对Ti(C,N)基金属陶瓷显微结构和力学性能的影响[J].功能材料,2010,41(10):1724-1726. 被引量:6

2张正权,金永中,陈建,杨林,徐永琼,余明婷.纳米(Ti,50W)C固溶体粉末的制备研究[J].稀有金属与硬质合金,2016,44(3):29-31.

3卢蕾蓉,谭贤志,徐勇戈.基于协整理论的钼价格预测研究[J].稀有金属与硬质合金,2016,44(3):67-72. 被引量:1

4黄建华,康希越,张鹛媚,贺跃辉,吝楠,颜焰,邱嵩,刘毅.ZrC添加量对Ti(C,N)基金属陶瓷组织结构及耐腐蚀性能的影响[J].硬质合金,2020,37(1):30-37. 被引量:1

1朱运锋,叶金文,刘颖,俞海军.开放体系下碳热还原氮化法制备(Ti、W、Mo、V)CN固溶体粉末的研究[J].功能材料,2012,43(17):2385-2388.

2杨杜鹃,叶金文,刘颖,李平平,邓玲.SD成型剂对Ti(C,N)基金属陶瓷显微结构和力学性能的影响[J].功能材料,2012,43(23):3304-3307. 被引量:1

3李延俊,廖立,谢克难,孟祉含.超细WC-Co硬质合金粉末的制备及其致密化研究[J].功能材料,2013,44(8):1102-1105. 被引量:12

4肖水清,刘杰,肖白军,邓欣,伍尚华.实现Ti(C,N)基金属陶瓷强韧化的技术路径[J].材料导报,2018,32(7):1129-1138. 被引量:8

5边璐,王晓贺,张江朋,张璞.稀土产品价格决定:影响因素与预测方法综述[J].稀土,2020,41(4):146-158. 被引量:2

6徐翔宇,郑勇.Ti(C,N)基金属陶瓷强韧化技术的研究进展[J].硬质合金,2021,38(4):286-296. 被引量:4

7秦运,王宗元,王杰,彭卓豪,季思源,万维财.Ti(C,N)基金属陶瓷腐蚀与磨损行为的研究进展[J].材料保护,2022,55(10):162-170.

8李银芝,刘钢,陈信锗,苏振华,颜练武,彭英彪.烧结温度和保温时间对Ti(C,N)基金属陶瓷微观组织结构和性能的影响[J].包装学报,2023,15(3):37-45.

1郑勇,赵兴中,胡镇华,崔昆.Ti(C,N)金属陶瓷中的添加剂[J].硬质合金,1994,11(2):123-127. 被引量:10

2颜练武,吴恩熙,黄伯云.非化学计量化合物与过渡族金属碳化物、氮化物研究进展[J].硬质合金,2008,25(4):261-263. 被引量:5

3占志泽.优质碳化钨粉的研制[J].江西冶金,1996,16(3):19-21. 被引量:1

4专利题录和文摘[J].中国钨业,1993,0(4):33-36.

5张立,朱骥飞,杨洋,熊湘君,徐涛,张忠健,刘向中,姚萍屏.添加剂对特粗晶和超粗晶硬质合金抗高温氧化性能的影响[J].粉末冶金材料科学与工程,2015,20(4):595-602. 被引量:2

6徐智谋,易新建,郑家焱,徐智谋,胡茂中,唐宏翚,江丙武.(Ti,W,Ta)(C,N)_p/Ti(C,N)基金属陶瓷的组织与性能[J].硬质合金,2002,19(4):193-198. 被引量:2

7祝修盛.2007年我国钨品进出口分析[J].中国金属通报,2008,0(8):17-21.

8张立,吴冲浒,陈述,熊湘君,单成.晶粒生长抑制剂在硬质合金中的微观行为[J].粉末冶金材料科学与工程,2010,15(6):667-673. 被引量:22

9专利题录和文摘[J].中国钨业,1989(12):40-41.

10朱俊峰,汪丹丹.陶瓷过滤器在碳化物游离碳测定中的应用[J].粉末冶金技术,1994,12(3):232-233. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF125.31[冶金工程—粉末冶金]

Citation Information:

Description is made of the typical structure of the Ti(C, N)-based cermet, focusing on the influ- ence of the additives of transitional metal carbide, such as nano-crystal TiC/TiN, Mo2C,WC,TaC, NbC, VC,CraC2 on the microstructure and mechanical property of Ti(C,N)-based cermet. It is feasible to pro- duce Ti(C,N)-based cermet with excellent performance by proper addition of carbide additives.

quote

GB/T 7714-2015 [1] ZOU Shi-min, CAO Shun-hua. Latest Development of Transitional Metal Carbide Additives in Ti(C,N)-based Cermet[J]. Rare Metals and Cemented Carbides, 2007(4): 57-60.
MLA [1] ZOU Shi-min, and CAO Shun-hua. "Latest Development of Transitional Metal Carbide Additives in Ti(C,N)-based Cermet." Rare Metals and Cemented Carbides, no. 4, 2007, pp. 57-60.
APA [1] ZOU Shi-min, & CAO Shun-hua. (2007). Latest Development of Transitional Metal Carbide Additives in Ti(C,N)-based Cermet. Rare Metals and Cemented Carbides(4), 57-60.
IEEE [1] ZOU Shi-min and CAO Shun-hua, "Latest Development of Transitional Metal Carbide Additives in Ti(C,N)-based Cermet," Rare Metals and Cemented Carbides, no. 4, pp. 57-60, 2007. keywords: {Ti (C, N);cermet;transitional metal carbide;additive;latest development}