Rhenium(I) N-Heterocyclic Carbene Complexes in Photoinitiating Systems for Polymerization upon Visible Light: Development of Photosensitive Resins for 3D and 4D Applications AITranslate

Université de Haute-Alsace;Université de Haute-Alsace; Université de Strasbourg;Université de Haute-Alsace; Université de Strasbourg;Université de Haute-Alsace
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two fac-rhenium tris-carbonyl complexes bearing a π-accepting pyridoannelated N-heterocyclic carbene (NHC) ligand with general formula Re(CO)3(pyipy)X, where pyipy is 2-pyridil-imidazo[1,5-a]pyridine-3-ylidene and X = Cl (Re1) and Br (Re2), are investigated as photoredox catalytic systems in light-promoted polymerization reactions. Both rhenium(I) complexes are able to efficiently generate radicals to initiate free radical polymerization. Remarkably, excellent radical polymerization profiles and final conversions are obtained under soft irradiations (LED lamp, λexc = 405 nm) by using the proposed complexes with iodonium salt and amine as photoinitiating systems (PISs) for polyethyleneglycol (PEG)-acrylate monomers. The involved mechanism is investigated by means of different spectroscopic techniques and further supported by electrochemical data. In addition, using the prepared three-component PISs, outstanding 3D patterns with spatial resolution could be obtained through direct laser write experiments. Remarkably, the resulting material displays reversible deformation that can be controlled with heating–hydration cycles due to stimuli-responsiveness of PEG chains of the polymeric network, thus opening the way for innovative smart and stimuli-responsive 4D-printed materials and soft actuators.

KeyWords AITranslate

rhenium complexes Nheterocyclic carbene free radical photopolymerization (FRP) 3D resins soft actuators
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01207

Chinese Library Classification Number:

Citation Information:

Two fac-rhenium tris-carbonyl complexes bearing a π-accepting pyridoannelated N-heterocyclic carbene (NHC) ligand with general formula Re(CO)3(pyipy)X, where pyipy is 2-pyridil-imidazo[1,5-a]pyridine-3-ylidene and X = Cl (Re1) and Br (Re2), are investigated as photoredox catalytic systems in light-promoted polymerization reactions. Both rhenium(I) complexes are able to efficiently generate radicals to initiate free radical polymerization. Remarkably, excellent radical polymerization profiles and final conversions are obtained under soft irradiations (LED lamp, λexc = 405 nm) by using the proposed complexes with iodonium salt and amine as photoinitiating systems (PISs) for polyethyleneglycol (PEG)-acrylate monomers. The involved mechanism is investigated by means of different spectroscopic techniques and further supported by electrochemical data. In addition, using the prepared three-component PISs, outstanding 3D patterns with spatial resolution could be obtained through direct laser write experiments. Remarkably, the resulting material displays reversible deformation that can be controlled with heating–hydration cycles due to stimuli-responsiveness of PEG chains of the polymeric network, thus opening the way for innovative smart and stimuli-responsive 4D-printed materials and soft actuators.

quote

GB/T 7714-2015 [1] Hong Chen, Yijun Zhang, Anna Bonfiglio, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01207.
MLA [1] Hong Chen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01207.
APA [1] Hong Chen, Yijun Zhang, Anna Bonfiglio, Fabrice MorletSavary, Matteo Mauro, & Jacques Lalevée. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01207
IEEE [1] Hong Chen, Yijun Zhang, Anna Bonfiglio, Fabrice MorletSavary, Matteo Mauro, and Jacques Lalevée, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01207. keywords: {rhenium complexes;Nheterocyclic carbene;free radical photopolymerization (FRP);3D resins;soft actuators}