Discussion on the Theoretical Problems from the Leaching of Molybdenite AITranslate
Abstract AITranslate
Thes-pH diagram of Mo-S-H2O system can not satisfactorily explains the leaching process of molybdenite, thus it has beenreconstructed on the basis of the latest r.search work in this paper.Some theoretical problems from the leaching of molybdenite are analyzedaccording to the new diagram.The reason of the difficulty in molybdenite'oxidization by wet process is discussed.Possible technical ways are pointed out to enhance the leaching process.
KeyWords AITranslate
1曹占芳,钟宏,闻振乾,符剑刚,陈娜.Ultrasonic Electro-oxidation Process of Molybdenite Concentrate[J].过程工程学报,2008,8(5):926-931. 被引量:1
2赵中伟,刘大学.使用氧逸度-pH图对辉钼矿浸出过程的热力学分析[J].中国钼业,2009,33(1):18-21. 被引量:3
3曹占芳,钟宏,闻振乾,符剑刚,丁超.超声电氧化辉钼精矿研究[J].中国矿业大学学报,2009,38(2):229-233. 被引量:7
4康绍辉,孟晋,王洪明,王平,杨剑飞.钼矿物湿法处理技术研究进展[J].湿法冶金,2012,31(6):333-337. 被引量:2
5旷林雄,颜文斌,周晓江.高碳镍钼矿制备钼酸铵[J].广州化工,2011,39(6):60-62.
6旷林雄,颜文斌,周晓江.高碳镍钼矿催化氧化镍钼分离工艺条件[J].吉首大学学报:自然科学版,2011,32(3):100-102.
7曹占芳,钟宏,姜涛,刘广义,王帅.德兴铜矿辉钼矿精矿的选择性电氧化浸出与分离过程[J].中国有色金属学报,2013,23(8):2290-2295. 被引量:14
8卜春阳,曹维成,王璐,张国华,常贺强,周国治,何凯.辉钼矿冶炼工艺综述及展望[J].中国钼业,2017,41(6):5-11. 被引量:8
9符剑刚,钟宏.具有发展前景的辉钼矿湿法分解工艺[J].稀有金属与硬质合金,2003,31(4):22-26. 被引量:17
10彭建蓉,杨大锦,陈加希,阎江峰.原生钼矿加压碱浸试验研究[J].稀有金属,2007,31(S1):110-113. 被引量:24
1都基峻,田刚,张凡.钼冶炼工艺的循环经济探讨[J].环境工程,2011,29(S1):381-384. 被引量:3
2杨大锦.2007年云南冶金年评[J].云南冶金,2008,37(2):40-51.
3于常武,许士国,陈国伟,周立岱.矽卡岩型钼矿尾砂中重金属Mo的淋滤实验研究[J].生态环境,2008,17(2):636-640. 被引量:7
4于常武,许士国,陈国伟,周立岱.酸碱度温度对钼尾矿中Mo静态浸出的影响[J].环境科学与技术,2008,31(7):1-3. 被引量:2
5曹占芳,钟宏,闻振乾,符剑刚,陈娜.Ultrasonic Electro-oxidation Process of Molybdenite Concentrate[J].过程工程学报,2008,8(5):926-931. 被引量:1
6于常武,周立岱,陈国伟.钼污染物的产生及在环境中的迁移[J].化工环保,2008,28(5):413-417. 被引量:10
7陈洁,李典军,刘大春,杨斌.辉钼矿冶炼技术研究进展[J].甘肃冶金,2009,31(1):25-28. 被引量:10
8康绍辉,孟晋,王洪明,王平,杨剑飞.钼矿物湿法处理技术研究进展[J].湿法冶金,2012,31(6):333-337. 被引量:2
9闻振乾,钟宏,曹占芳,符剑刚,肖燕飞,张文轩.电氧化法湿法分解辉钼矿工艺条件的研究[J].稀有金属,2009,33(2):267-271. 被引量:3
10吴贤,李来平,张新,张文钲.用矿浆电解法分解辉钼矿试验研究[J].现代矿业,2009(10):61-64. 被引量:1
1秦玉楠.离子交换法自含铜钼精矿生产纯MoO_3新工艺[J].中国钼业,1996,20(1):47-50.
2绪小鹏.优质钼酸铵是钼条生产的质量保证[J].中国钼业,1997,21(2):107-108. 被引量:8
3陈庭章,周勤俭,银瑰.从萃取钼余液中回收铜[J].中国钼业,1997,21(2):80-82. 被引量:4
4顾珩,李洪桂,刘茂盛.热球磨苏打法处理钼渣新工艺研究[J].中国钼业,1997,21(4):16-18. 被引量:5
5万华.南钢高炉长寿途径之浅见[J].江苏冶金,1996,24(2):29-30.
6文志平.铜电解设计问题浅见[J].重冶科技,1990(12):1-5.
7覃岚,张后鼎.对唐钢开发生产海绵铁的浅见[J].冶金矿山与冶金设备,1996(6):16-17.
8金真,敖翔.改善新钢炼铁技术指标的浅见[J].江西冶金,1996,16(6):13-14.
9王献科,王德勇.利用中频感应电炉生产硅铝铁合金[J].中国钼业,1999,23(2):11-13.
10董桑林.美国钼工业的现状与发展[J].稀有金属,1993,17(6):455-459. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.203[冶金工程—有色金属冶金]
Citation Information:
Thes-pH diagram of Mo-S-H2O system can not satisfactorily explains the leaching process of molybdenite, thus it has beenreconstructed on the basis of the latest r.search work in this paper.Some theoretical problems from the leaching of molybdenite are analyzedaccording to the new diagram.The reason of the difficulty in molybdenite'oxidization by wet process is discussed.Possible technical ways are pointed out to enhance the leaching process.
quote
| GB/T 7714-2015 | [1] ZHAO Zhong-wei. Discussion on the Theoretical Problems from the Leaching of Molybdenite[J]. Rare Metals and Cemented Carbides, 1995(2): 1-3. |
| MLA | [1] ZHAO Zhong-wei. "Discussion on the Theoretical Problems from the Leaching of Molybdenite." Rare Metals and Cemented Carbides, no. 2, 1995, pp. 1-3. |
| APA | [1] ZHAO Zhong-wei. (1995). Discussion on the Theoretical Problems from the Leaching of Molybdenite. Rare Metals and Cemented Carbides(2), 1-3. |
| IEEE | [1] ZHAO Zhong-wei, "Discussion on the Theoretical Problems from the Leaching of Molybdenite," Rare Metals and Cemented Carbides, no. 2, pp. 1-3, 1995. keywords: {molybdenite;leaching;ε-pH diagram} |