Research on the Influence of Shot Blasting on Titanium Strip Pickling AITranslate
Abstract AITranslate
The influence of shot blasting on titanium strip pickling was investigated through the surface morphology analysis and the contrast pickling experiments of shot-blasted and non-shot-blasted titanium strips. The results show that with the decrease of the volume ratio of hydrofluoric acid to nitric acid, the weight loss rates of both shot-blasted and non-shot-blasted titanium strips gradually decrease, while the needed pickling times for both are gradually increased. Under the optimum conditions, the volume ratio of hydrofluoric acid to nitric acid of shot-blasted titanium strip is slightly bigger than that of non-shot-blasted one, but its pickling time is slightly longer. Thus, the strengthening effects of shot blasting on titanium strip pickling is not obvious.
KeyWords AITranslate
1杜礼章.工业纯钛板材生产工艺研究[J].特钢技术,2008,14(4):19-21. 被引量:6
2薛小莲.工业纯钛带材的加工工艺[J].冶院科技,1994(4):43-46. 被引量:5
3黄德明.工业纯钛TA2的氧化行为研究[J].钢铁钒钛,2010,31(1):11-16. 被引量:8
4赵义,任妍利.钛板材生产过程中表面酸洗的试验研究[J].甘肃冶金,2011,33(2):45-47. 被引量:7
5徐信.纯钛卷工业化酸洗工艺浅析[J].化学工程与装备,2011(7):163-164. 被引量:5
6Johnson J W, Shen K S, James W J. A kinetic study of the oxidation of Ti (IlI ) to Ti ( IV ) in hydrofluoric acid solutions[J]. Journal of the Less Common Metals, 1968,15(2) .. 177-182.
7Sutter E M M, Goetz-Grandmont G J. The behaviour of titanium in nitric hydrofluoric acid solutions[J]. Corro sion Science, 1990,30(4 5): 461-476.
8郑锋,程挺宇,张巧云.钛及钛合金的酸洗技术[J].稀有金属与硬质合金,2009,37(3):26-28. 被引量:28
9雷霆,周林,李双寿,张玉林,方树铭,陈昆,童学斌.精密异型钛材热处理工艺研究[J].有色金属:冶炼部分,2006(2):35-37. 被引量:5
10朱立,孙本良.钢铁酸洗技术[M].北京:化学工业出版社,2007.
1王国富,周庆军,江录豹.钛及钛合金中厚板在线酸洗工艺探讨[J].物理测试,2017,35(6):47-53. 被引量:1
1王国富,余海峰.特种金属及合金中厚板在线酸洗技术探讨[J].物理测试,2020,0(1):18-23. 被引量:1
1史政敏,贾东海.钛带工艺技术的发展[J].钛工业进展,1996(4):1-2. 被引量:1
2陆大魁.建立齿轮自身的抛丸规范(二)[J].柴油机设计与制造,1995(4):57-61.
3林素贞.高效抛丸轮[J].国外机车车辆工艺,1998(5):12-12. 被引量:1
4杨文甲.TA1钛带织构的研究[J].有色矿冶,1992(5):32-36.
5服部成雄,文凡.抗硝酸不锈钢的制造方法[J].国外低合金钢:合金钢,1994(14):54-57.
6王春英,张瑞,杨季龙,伊岩,杨晓东.表面工程技术在工程机械中的应用[J].建筑机械,2012,32(11):89-93. 被引量:5
7孟凡义.丸灰分离器工作原理及其应用[J].铁道机车车辆工人,1999(11):14-15.
8孙少纯.国内外抛丸器研究的发展概况[J].铸造设备研究,1991(1):37-39.
9蒋海燕.Q365抛丸清理室改造[J].铸造设备研究,2006(1):15-15.
10余存烨.关于不锈钢设备与零部件酸洗配方讨论[J].清洗世界,2006,22(11):8-12. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG178[金属学及工艺—金属表面处理]
Citation Information:
The influence of shot blasting on titanium strip pickling was investigated through the surface morphology analysis and the contrast pickling experiments of shot-blasted and non-shot-blasted titanium strips. The results show that with the decrease of the volume ratio of hydrofluoric acid to nitric acid, the weight loss rates of both shot-blasted and non-shot-blasted titanium strips gradually decrease, while the needed pickling times for both are gradually increased. Under the optimum conditions, the volume ratio of hydrofluoric acid to nitric acid of shot-blasted titanium strip is slightly bigger than that of non-shot-blasted one, but its pickling time is slightly longer. Thus, the strengthening effects of shot blasting on titanium strip pickling is not obvious.
quote
| GB/T 7714-2015 | [1] LIU Zi-lian, PENG Jin-hui, GUO Sheng-hui, et al. Research on the Influence of Shot Blasting on Titanium Strip Pickling[J]. Rare Metals and Cemented Carbides, 2013(3): 36-40. |
| MLA | [1] LIU Zi-lian, et al., "Research on the Influence of Shot Blasting on Titanium Strip Pickling." Rare Metals and Cemented Carbides, no. 3, 2013, pp. 36-40. |
| APA | [1] LIU Zi-lian, PENG Jin-hui, GUO Sheng-hui, CHANG Jun, CAO Zhan-yuan, & SHI Ya-ming. (2013). Research on the Influence of Shot Blasting on Titanium Strip Pickling. Rare Metals and Cemented Carbides(3), 36-40. |
| IEEE | [1] LIU Zi-lian, PENG Jin-hui, GUO Sheng-hui, CHANG Jun, CAO Zhan-yuan, and SHI Ya-ming, "Research on the Influence of Shot Blasting on Titanium Strip Pickling," Rare Metals and Cemented Carbides, no. 3, pp. 36-40, 2013. keywords: {titanium strip;pickling;shot blasting;oxide layer;weight loss rate} |