Preparation and Characterization of Ce0.8Sm0.1Gd0.1O1.9 Electrolyte AITranslate

Department of Materials Science and Engineering, Nanchang Academy of Aeronautics Industry;Department of Materials Science and Engineering, Nanchang Academy of Aeronautics Industry;Department of Materials Science and Engineering, Nanchang Academy of Aeronautics Industry;Department of Materials Science and Engineering, Nanchang Academy of Aeronautics Industry;Department of Materials Science and Engineering, Nanchang Academy of Aeronautics Industry
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sm and Gd co-doped CeO2 electrolyte powders were prepared by co-precipitation. The phase composition,morphology and particle size of the powders were characterized. At the same time, the properties of the sintered SGC materials were also characterized. The results showed that the SGC electrolyticpowder prepared by the co-precipitation had good sintering characteristic with relative density〉93% when sintering at 1 400℃. The electrical :property testing also showed that the sintered SGC materials had the higher oxygen ion electrical conductivity at medium-temperature.

KeyWords AITranslate

IT-SOFC doped CeO2 co-precipitation sintering property electrical conductivity

1孟广耀.开发陶瓷膜燃料电池(CMFC)大有可为[J].电池,2002,32(3):142-145. 被引量:10

2孟广耀,付清溪,彭定坤.中温固态氧化物燃料电池[J].太阳能学报,2002,23(3):378-382. 被引量:15

3Zhu B. Advantage of intermediate temperature solid oxide fuel cells for tractionary applications[J]. Journal of Power Sources, 2002,93: 82-86.

4Kim N,Kim B H,Lee D. Effect of co-dopant addition on properties of gadolinia-doped ceria electrolyte[J]. Journal of Power Sources,2000,90: 139-143.

5Zhang T S, Ma J. Dense submicron-grained Ce0.8Gd0.2O2 -δ ceramics for SOFC applications[J]. Scripta Material, 2004,50:1 127-1 130.

6Zhu B, Liu X G, Sun M T,et al. Calcium doped ceriabased materials for cost-effective intermediate temperature solid oxide fuel cells[J]. Solid State Sciences, 2003, 5:1 127-1 134.

7Mori T, Wang Y R, Drennan J, et al. Influence of particle morphology on nanostructural feature and conducting property in Sm-doped CeO2 sintered body[J]. Solid State Ionics, 2004,175: 641-649.

8Gu Y F,Li G,Meng,G Y, et al. Sintering and electrical properties of coprecipitation prepared Ce0.8Y0.2O1.9 ceramics[J]. Materials Research Bulletin, 2000, 35: 297- 304.

9尹艳红,杨书廷,夏长荣,孟广耀.不同方法制备的Ce_(0.8)Sm_(0.2)O_(1.9)(SDC)性能对比[J].河南师范大学学报:自然科学版,2005,33(2):56-59. 被引量:5

1许亮,侯书恩,靳洪允,赵新颖,黄玉娟,张涛.SDC电解质致密化研究[J].材料导报:纳米与新材料专辑,2009,23(2):313-315.

1史文方.如意SGC-4703彩电故障检修[J].家电检修技术,1994(10):11-11.

2单丹,曲远方,张晨,宋建静,郭晓琨.掺杂CeO2和CuO对BaTiO3陶瓷介电性能的影响[J].稀有金属材料与工程,2005(z2):777-779.

3孙明涛,孙俊才,季世军.CeO_2基固体电解质材料研究进展[J].稀土,2006,27(4):78-82. 被引量:3

4郑益锋,周明,陈涵,郭露村.Al_2O_3对Ce_(0.8)La_(0.2)O_(1.9)电解质材料性能的影响[J].南京工业大学学报:自然科学版,2010,32(6):1-5.

5黄金,王延忠,刘炜,胡保全.中低温固体氧化物燃料电池复相固体电解质的研究进展[J].电池,2013,43(3):178-181. 被引量:10

6徐丹,李柯慧,高阳,周永军,徐世峰.CeO_2基中温复合电解质材料的研究进展[J].电源技术,2017,41(4):647-650. 被引量:2

7田宁.如意牌SGC—4703型彩电稳压电源分析与维修[J].如意广播电视,1992(1):46-49.

8黄英才,刘毅,劳令耳,唐道文,邰贵江,刘大卫.纳米Y_2O_3掺杂CeO_2固体电解质导电性能及机理研究[J].贵州工业大学学报:自然科学版,2004,33(2):14-17. 被引量:3

9邓莉萍,罗军明,袁永瑞,缪全辉.Ce_(0.8)Sm_(0.1)Gd_(0.1)O_(1.9)电解质的制备及其性能研究[J].稀有金属,2008,32(2):195-198. 被引量:5

10谢淑红,崔崑,夏风,谢光远.阳极支撑型固体氧化物燃料电池的研制[J].华中科技大学学报:自然科学版,2004,32(6):72-74. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TM911.4[电气工程—电力电子与电力传动]

Citation Information:

Sm and Gd co-doped CeO2 electrolyte powders were prepared by co-precipitation. The phase composition,morphology and particle size of the powders were characterized. At the same time, the properties of the sintered SGC materials were also characterized. The results showed that the SGC electrolyticpowder prepared by the co-precipitation had good sintering characteristic with relative density〉93% when sintering at 1 400℃. The electrical :property testing also showed that the sintered SGC materials had the higher oxygen ion electrical conductivity at medium-temperature.

quote

GB/T 7714-2015 [1] YUAN Yong-rui, DENG Li-ping, LUO Jun-ming, et al. Preparation and Characterization of Ce0.8Sm0.1Gd0.1O1.9 Electrolyte[J]. Rare Metals and Cemented Carbides, 2007(2): 11-13.
MLA [1] YUAN Yong-rui, et al., "Preparation and Characterization of Ce0.8Sm0.1Gd0.1O1.9 Electrolyte." Rare Metals and Cemented Carbides, no. 2, 2007, pp. 11-13.
APA [1] YUAN Yong-rui, DENG Li-ping, LUO Jun-ming, ZHANG Jian-ping, & ZHANG Guo-guang. (2007). Preparation and Characterization of Ce0.8Sm0.1Gd0.1O1.9 Electrolyte. Rare Metals and Cemented Carbides(2), 11-13.
IEEE [1] YUAN Yong-rui, DENG Li-ping, LUO Jun-ming, ZHANG Jian-ping, and ZHANG Guo-guang, "Preparation and Characterization of Ce0.8Sm0.1Gd0.1O1.9 Electrolyte," Rare Metals and Cemented Carbides, no. 2, pp. 11-13, 2007. keywords: {IT-SOFC;doped CeO2;co-precipitation;sintering property;electrical conductivity}