Flame Retardant Combinations with Expandable Graphite/Phosphorus/CuO/Castor Oil in Flexible Polyurethane Foams AITranslate
Abstract AITranslate
A series of flexible polyurethane foams (FPUFs) were prepared with single and different combinations of flame retardants and additives. Expandable graphite (EG), phosphorous polyol (OP), copper (II) oxide (CuO), and/or castor oil (CAS) were added to FPUF during the foam preparation in a one-step process. The purpose of the study is to evaluate the synergistic effects of the flame retardants, additives, and the presence of bio-based content on the mechanical properties, flame retardancy, and smoke behavior of FPUFs. The combination of 10 wt % EG and 5 wt % OP in FPUF significantly improves the char yield. In the cone calorimeter experiment, the char yield is nearly three times higher than that with 10 wt % EG alone. The smoke behavior is additionally evaluated in a smoke density chamber (SDC). Comparing the samples with a single flame retardant, 10 wt % EG in FPUF considerably reduces the amount of smoke released and the emission of toxic gases. Replacing the amount of 10 wt % polyether polyol in FPUF with CAS maintains the physical and mechanical properties and fire behavior and enhances the bio-based content. The presence of 0.1 wt % CuO in FPUF effectively reduces the emission of hydrogen cyanide. As a result, this study proposes a multicomponent flame retardant strategy for FPUF to enhance the biomass content and address the weaknesses in flame retardancy, smoke, and toxic gas emissions. A starting point is disclosed for future product development.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01969
Chinese Library Classification Number:
Citation Information:
A series of flexible polyurethane foams (FPUFs) were prepared with single and different combinations of flame retardants and additives. Expandable graphite (EG), phosphorous polyol (OP), copper (II) oxide (CuO), and/or castor oil (CAS) were added to FPUF during the foam preparation in a one-step process. The purpose of the study is to evaluate the synergistic effects of the flame retardants, additives, and the presence of bio-based content on the mechanical properties, flame retardancy, and smoke behavior of FPUFs. The combination of 10 wt % EG and 5 wt % OP in FPUF significantly improves the char yield. In the cone calorimeter experiment, the char yield is nearly three times higher than that with 10 wt % EG alone. The smoke behavior is additionally evaluated in a smoke density chamber (SDC). Comparing the samples with a single flame retardant, 10 wt % EG in FPUF considerably reduces the amount of smoke released and the emission of toxic gases. Replacing the amount of 10 wt % polyether polyol in FPUF with CAS maintains the physical and mechanical properties and fire behavior and enhances the bio-based content. The presence of 0.1 wt % CuO in FPUF effectively reduces the emission of hydrogen cyanide. As a result, this study proposes a multicomponent flame retardant strategy for FPUF to enhance the biomass content and address the weaknesses in flame retardancy, smoke, and toxic gas emissions. A starting point is disclosed for future product development.
quote
| GB/T 7714-2015 | [1] Yin Yam Chan, Andreas Korwitz, Doris Pospiech, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01969. |
| MLA | [1] Yin Yam Chan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01969. |
| APA | [1] Yin Yam Chan, Andreas Korwitz, Doris Pospiech, & Bernhard Schartel. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01969 |
| IEEE | [1] Yin Yam Chan, Andreas Korwitz, Doris Pospiech, and Bernhard Schartel, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01969. keywords: {flexible polyurethane foam;flame retardancy;synergistic effect;smoke behavior;expandable graphite;biobased} |