daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Titanium Dioxide Nanoparticle-Decorated Polymer Microcapsules Enclosing Phase Change Material for Thermal Energy Storage and Photocatalysis AITranslate

Indian Institute of Technology; Indian Institute of Technology; Indian Institute of Technology; Indian Institute of Technology; Indian Institute of Technology; Indian Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Titanium dioxide (TiO2) nanoparticle decorated [poly(4-methylstyrene-co-divinylbenzene)] microcapsules enclosing phase change material (PCM) were synthesized following a one-pot non-Pickering emulsion templated suspension polymerization. TiO2 nanoparticles were hydrophobized using a trace amount of tertradecyltrimethylammonium bromide (TTAB, cationic stabilizer) through electrostatic interaction and employed as a particle stabilizer. The resulting microcapsules presented concurrent functionalities of thermal energy storage and photocatalytic activity. Scanning electron microscopy (SEM) identified that microencapsulated PCMs (microPCMs) exhibited a well-defined, core–shell structure with spherical morphology. The existence of TiO2 over the polymeric shell was confirmed by energy-dispersive X-ray (EDX) and X-ray diffraction (XRD) analysis. Differential scanning calorimetry (DSC) analysis demonstrated that microPCM with 2.6 wt % TiO2 achieved maximum phase change enthalpy of 174 J/g with an encapsulation efficiency of 76.6% and could maintain it even after 100 melting–freezing cycles. Thermogravimetric analysis (TGA) revealed that the addition of TiO2 contributed in improving the thermal stability of microPCMs. Most of all, the produced microcapsules exhibited great photocatalytic activity through the synergistic photothermal effect. The bifunctional microcapsules reported in this work would stimulate wide applications in the biomedical field, residential buildings in polluted urban sites, and industrial establishments as thermal energy storage and depollution materials.

KeyWords AITranslate

microencapsulation phase change material nonPickering emulsion thermal energy storage photocatalytic activity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01410

Chinese Library Classification Number:

Citation Information:

Titanium dioxide (TiO2) nanoparticle decorated [poly(4-methylstyrene-co-divinylbenzene)] microcapsules enclosing phase change material (PCM) were synthesized following a one-pot non-Pickering emulsion templated suspension polymerization. TiO2 nanoparticles were hydrophobized using a trace amount of tertradecyltrimethylammonium bromide (TTAB, cationic stabilizer) through electrostatic interaction and employed as a particle stabilizer. The resulting microcapsules presented concurrent functionalities of thermal energy storage and photocatalytic activity. Scanning electron microscopy (SEM) identified that microencapsulated PCMs (microPCMs) exhibited a well-defined, core–shell structure with spherical morphology. The existence of TiO2 over the polymeric shell was confirmed by energy-dispersive X-ray (EDX) and X-ray diffraction (XRD) analysis. Differential scanning calorimetry (DSC) analysis demonstrated that microPCM with 2.6 wt % TiO2 achieved maximum phase change enthalpy of 174 J/g with an encapsulation efficiency of 76.6% and could maintain it even after 100 melting–freezing cycles. Thermogravimetric analysis (TGA) revealed that the addition of TiO2 contributed in improving the thermal stability of microPCMs. Most of all, the produced microcapsules exhibited great photocatalytic activity through the synergistic photothermal effect. The bifunctional microcapsules reported in this work would stimulate wide applications in the biomedical field, residential buildings in polluted urban sites, and industrial establishments as thermal energy storage and depollution materials.

quote

GB/T 7714-2015 [1] Sumit Parvate, Jitendra Singh, Prakhar Dixit, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01410.
MLA [1] Sumit Parvate, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01410.
APA [1] Sumit Parvate, Jitendra Singh, Prakhar Dixit, Jagadeeswara Reddy Vennapusa, Tushar Kanti Maiti, & Sujay Chattopadhyay. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01410
IEEE [1] Sumit Parvate, Jitendra Singh, Prakhar Dixit, Jagadeeswara Reddy Vennapusa, Tushar Kanti Maiti, and Sujay Chattopadhyay, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01410. keywords: {microencapsulation;phase change material;nonPickering emulsion;thermal energy storage;photocatalytic activity}