Research on Preparation Method of Hard Metals Metallographic Specimen AITranslate
Abstract AITranslate
Basic requirements for the quality of hard metals metallographic specimen are introduced. The problems of the existing preparation method for the said specimen are ana lyzed, some modification and research are made.The author thinks it quite necessary to work at the research, experince exchange, technical demonstration and populatrization of achievement of advanced specimen preparation methods.
KeyWords AITranslate
1孙文友.关于硬质合金中石墨夹杂的探讨[J]稀有金属与硬质合金,1994(04).
1王微,李颖,郭昌龙.梯度结构硬质合金脱β层的检测[J].世界有色金属,2017,42(20):244-245. 被引量:2
2廖诗兰.硬质合金金相制样方法研究[J].中国钨业,2018,33(1):60-65. 被引量:3
1李巨,樊湘芳,王冲,孙萌,于文博.金相制样的几点技巧和常见问题的解决方法[J].科技视界,2020(13):59-61. 被引量:7
2雒飞飞.硬质合金分析检测技术分析[J].中国设备工程,2020(16):153-154.
3魏恒生,沈金城,姚蕾,杨海涛.高速重载火车轮毂加工刀片的材质分析[J].硬质合金,2021,38(3):165-170.
4陈宗福,刘新乐,傅兴达,樊湘芳.新型排气门材料Ni30高温合金的金相试样制备及表面形貌观察[J].机械工程师,2022(6):9-11.
5周杨,杨娥,张军,董浩,李波.全自动磨抛机在钢铁金相制样中的应用[J].物理测试,2022,40(5):32-36. 被引量:1
1George Blann,George Vander Voort.热喷涂涂层的制备[J].冶金标准化与质量,2004,42(5):14-17. 被引量:1
2李颖,徐国祥.TC4钛合金激光焊接接头金相试样的制备与显微组织分析[J].热加工工艺,2016,45(13):187-189. 被引量:2
3姚永红,燕样样,李红莉,王艳芳.铝合金钎焊接头金相试样制备方法初探[J].陕西工业职业技术学院学报,2008,3(4):6-8.
4姚永红,燕样样,李红莉,王艳芳.铝合金钎焊接头金相试样制备方法[J].金属热处理,2009,34(11):113-115. 被引量:1
5郑楠,宋琳.半固态镁合金金相试样制备[J].新乡学院学报,2008,0(2):35-37.
6李荣锋,龚桂仙.稀土处理钢用混合稀土金属丝(棒)金相试样制备与观察[J].稀土,1993,14(1):50-51.
7燕样样,李红莉.金相试样制备技术与技巧[J].理化检验:物理分册,2013,49(3):162-165. 被引量:21
8王明瑞.浅谈锆基非晶合金的制作方法[J].电子制作,2013,21(24):207-207.
9谢希文.一次别有特色的金相试样制备技术培训班[J].物理测试,2000,18(3):47-48. 被引量:1
10朱峰,伍超群,刘英坤.电解抛光在6063铝合金金相试样制备中的应用[J].理化检验:物理分册,2010,46(11):692-694. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TG115.211[金属学及工艺—物理冶金];TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Basic requirements for the quality of hard metals metallographic specimen are introduced. The problems of the existing preparation method for the said specimen are ana lyzed, some modification and research are made.The author thinks it quite necessary to work at the research, experince exchange, technical demonstration and populatrization of achievement of advanced specimen preparation methods.
quote
| GB/T 7714-2015 | [1] SUN Wen-you. Research on Preparation Method of Hard Metals Metallographic Specimen[J]. Rare Metals and Cemented Carbides, 1997(3): 30-34. |
| MLA | [1] SUN Wen-you. "Research on Preparation Method of Hard Metals Metallographic Specimen." Rare Metals and Cemented Carbides, no. 3, 1997, pp. 30-34. |
| APA | [1] SUN Wen-you. (1997). Research on Preparation Method of Hard Metals Metallographic Specimen. Rare Metals and Cemented Carbides(3), 30-34. |
| IEEE | [1] SUN Wen-you, "Research on Preparation Method of Hard Metals Metallographic Specimen," Rare Metals and Cemented Carbides, no. 3, pp. 30-34, 1997. keywords: {hard metal, metallographic specimen, grinding, erosion} |