Acetic Anhydride Polymerization as a Pathway to Functional Porous Organic Polymers and Their Application in Acid–Base Catalysis AITranslate
Abstract AITranslate
Acetic anhydride (AA) is usually considered a stable molecule but is shown here to be able to polymerize in closed reactors to a cross-linked polyketone condensate. By using this chemistry, it was possible to copolymerize AA with l-histidine, which gives a nitrogen-doped functional nanoporous polymer that can act as an acid–base heterogeneous catalyst. The polymer acidic and basic sites were screened by running an acetal hydrolysis Knoevenagel condensation reaction cascade to optimize catalyst synthesis. Furthermore, it was possible to catalyze CO2 cycloaddition to epoxides to the corresponding cyclic carbonate with complete conversion without cocatalysts.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00202
Chinese Library Classification Number:
Citation Information:
Acetic anhydride (AA) is usually considered a stable molecule but is shown here to be able to polymerize in closed reactors to a cross-linked polyketone condensate. By using this chemistry, it was possible to copolymerize AA with l-histidine, which gives a nitrogen-doped functional nanoporous polymer that can act as an acid–base heterogeneous catalyst. The polymer acidic and basic sites were screened by running an acetal hydrolysis Knoevenagel condensation reaction cascade to optimize catalyst synthesis. Furthermore, it was possible to catalyze CO2 cycloaddition to epoxides to the corresponding cyclic carbonate with complete conversion without cocatalysts.
quote
| GB/T 7714-2015 | [1] Sylvain Rat, Angeles ChavezSanchez, Mariá Jerigová, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00202. |
| MLA | [1] Sylvain Rat, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00202. |
| APA | [1] Sylvain Rat, Angeles ChavezSanchez, Mariá Jerigová, Daniel Cruz, & Markus Antonietti. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00202 |
| IEEE | [1] Sylvain Rat, Angeles ChavezSanchez, Mariá Jerigová, Daniel Cruz, and Markus Antonietti, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00202. keywords: {porous organic polymer;copolymerization;heterogeneous catalysis;cascade reactions;carbon dioxide fixation;cyclic carbonate} |