Research Progress of Preparation Methods of Lithium Manganate Cathode Materials AITranslate
Abstract AITranslate
The research progress of solid phase method and liquid phase method for preparation of lithium manganese cathode materials is reviewed,and the modification methods based on the traditional methods are emphatically introduced,including element doping method and coating modification method.The modification methods can obviously improve the stability and electrochemical performance of lithium manganate cathode materials.
KeyWords AITranslate
1王月磊,张静,吴建宝,刘微,宓一鸣.新型水热改性方法抑制LiMn_2O_4正极材料Jahn-Teller效应[J].电源技术,2015,39(1):37-39. 被引量:3
2田亮,温碧霞,苏长伟,郭俊明.微波液相无焰燃烧法超快制备尖晶石型锰酸锂[J].电池工业,2018,0(1):11-14. 被引量:4
3史晋宜,郑凌,孙立莹.溶剂-凝胶法制备锂离子电池的阴极材料LiMn_2O_4及其性能研究[J].科技创新与应用,2016,6(33):13-14. 被引量:1
4章守权.溶胶—凝胶法制备锰酸锂作为锂离子电池正极材料的研究[J].广东化工,2015,42(18):41-42. 被引量:3
5刘清,段玉珍,刘晓芳,向明武,郭俊明,段开娇.碳包覆改性尖晶石型LiMn2O4正极材料研究进展[J].云南民族大学学报:自然科学版,2019,28(5):439-443. 被引量:4
6崔燕,唐致远,薛建军,南俊民,侯宪鲁,杨敏杰.Li_xMnO_2的熔盐浸渍法合成和性能[J].电池,2006,36(2):101-103. 被引量:2
7王云霞,郎晓珍,常宏涛,翟秀静,储刚.微波合成法制备锂离子电池正极材料LiCoO_2[J].材料与冶金学报,2003,2(3):200-202. 被引量:2
8李春流,闫冠杰,卢道焕,黄炳行,李剑,詹海清.复合掺杂与包覆对尖晶石锰酸锂结构和性能的影响[J].中国锰业,2019,37(2):9-12. 被引量:3
9李贵炎,赵毅.启停锰酸锂电池表面材料改性及性能分析[J].电源技术,2018,42(9):1281-1282. 被引量:1
10马学超,刘艳波,李智.空气气氛中新型锰酸锂电池正极材料的合成[J].电源技术,2018,42(9):1286-1288. 被引量:1
1刘华东,邹兴.Mn3O4锰源中杂质铁对LiMn2O4正极材料电性能的影响研究[J].材料科学,2020,10(9):759-765. 被引量:1
1陈美林,杨茂峰,李春流,詹海青,万维华,黎明,闫冠杰.铝、钴元素共掺杂对尖晶石型锰酸锂高温循环性能的研究[J].中国锰业,2021,39(3):43-47.
1梁力勃,卢德娟,梁晶晶,熊美玉,陈彦辛,赖飞燕.NiFe2O4@LiMn2O4正极材料的制备及其电化学性能研究[J].矿冶工程,2020,40(2):127-130. 被引量:1
2张帅,张隐,张蕤,潘明珠.聚电解质化聚磷酸铵对木塑复合材料性能的影响[J].林业工程学报,2020,5(4):52-59. 被引量:4
3李剑,姚勇,张凯舟,张敏敏,李科褡,靳进波,韦福建.改性PVDF膜在染料废水处理中的应用与进展[J].塑料科技,2020,48(6):74-78. 被引量:5
4梁贺升,霍礼洪.活性炭负载纳米铁的制备及降解2,2’,4,4’-四溴联苯醚的性能[J].韩山师范学院学报,2020,41(3):41-45.
Basic Information:
DOI:
Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动]
Citation Information:
The research progress of solid phase method and liquid phase method for preparation of lithium manganese cathode materials is reviewed,and the modification methods based on the traditional methods are emphatically introduced,including element doping method and coating modification method.The modification methods can obviously improve the stability and electrochemical performance of lithium manganate cathode materials.
quote
| GB/T 7714-2015 | [1] WU Bing-kun, JI Yang-mei, LIANG Jing-long, et al. Research Progress of Preparation Methods of Lithium Manganate Cathode Materials[J]. Rare Metals and Cemented Carbides, 2020(3): 67-72. |
| MLA | [1] WU Bing-kun, et al., "Research Progress of Preparation Methods of Lithium Manganate Cathode Materials." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 67-72. |
| APA | [1] WU Bing-kun, JI Yang-mei, LIANG Jing-long, LI Hui, & YAN Hong-yan. (2020). Research Progress of Preparation Methods of Lithium Manganate Cathode Materials. Rare Metals and Cemented Carbides(3), 67-72. |
| IEEE | [1] WU Bing-kun, JI Yang-mei, LIANG Jing-long, LI Hui, and YAN Hong-yan, "Research Progress of Preparation Methods of Lithium Manganate Cathode Materials," Rare Metals and Cemented Carbides, no. 3, pp. 67-72, 2020. keywords: {cathode material;lithium manganate;solid phase method;liquid phase method;doping;coating;research progress} |