Effects of Different Heat Treatment on Creeping Property of GH4169 Alloy AITranslate

School of Mechanical Engineering, Donghua University;School of Mechanical Engineering, Donghua University;School of Mechanical Engineering, Donghua University;School of Mechanical Engineering, Donghua University;School of Mechanical Engineering, Donghua University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the effects of different heat treatment on creeping property of GH4169 alloy through the testing of creeping property and microstructure observation. The results show that the hot continuous rolled alloy after standard heat treatment precipitates less 8 phase and has better creeping property than the radial forged alloy after the standard heat treatment. The hot continuous rolled alloy after di- rect-aged treatment precipitates little 8 phase with longer creeping life, which is twice as much as that of the radial forged alloy after standard heat treatment. The radial forged alloy produces transgranular fracture during creeping,while the hot continuous rolled alloy produces intergranular fracture.

KeyWords AITranslate

GH4169 alloy heat treatment creeping property δ phase radial forged alloy hot continuousrolled alloy

1Yeh A C,Lu K W,Kuo C M,et al. Effect of serrated grain boundaries on the creep property of Inconel 718 superalloy[J].Materials Science and Engineering A, 2011,530..525-529.

2Kuo C M, Yang Y T,Bor H Y,et al. Aging e{fects on the microstructure and creep behavior of Inconel 718 su peralloy[J]. Materials Science and Engineering A, 2009, 510-511 ..289-294.

3Sundararaman M, Mukhopadhyay P, Banerjee S. Some aspects of the precipitation of metastable intermetallic phases in Inconel 718[J]. Metallurgical Transactions A, 1992,23:2 015-2 028.

4Sims C T, Hagel W C. The superalloys[M]. New York: John Wiley &Sons,1972.

5Sims C T, Stoloff N S, Hagel W C. The superalloys Ⅱ [M]. New York:John Wiley & Sons,1987.

6Ping D H,Gu Y F,Cui C Y,etal. Grain boundary segre- gation in a Ni-Fe-based (Alloy 718) superalloy[J]. Ma- terials Science and Engineering A, 2007,456:99-102.

7Xiao F R,Liu W C,Yao M. The influence of cold rolling on the precipitation of delta phase in Inconel 718 alloy [J]. Scripta Meterialia. 1997,37 ( 1 ) : 53-57.

8Huang Y,Langdon T G. The evolution of delta-phase in a superplastic Inconel 718 alloy[J]. Journal of Materials Science, 2007,42 : 421-427.

9Azadian S, Liu Y W, Warren R. Delta phase precipitati- on in Inconel 718[J]. Materials Characterization, 2004, 53:7-16.

10Sridhar N,Rickman J M,Srolovitz D J. Microstructural stability of stressed lamellar and fiber composites[J]. Acta Materialia,1997,45(7) :2 735-2 746.

1卞宏友,赵翔鹏,杨光,钦兰云,王维,王世杰,任宇航.激光沉积修复GH4169合金热处理的组织及性能[J].中国激光,2015,42(12):153-160. 被引量:10

2牛静,张凡云,杨树林,王蔓,赵智,刘晶.不同时效处理对GH4169合金组织性能的影响[J].航空制造技术,2016,59(20):45-48. 被引量:6

3李祚军,白云瑞,吴晨,田伟.GH4169G合金叶盘叶尖裂纹失效分析[J].燃气涡轮试验与研究,2020,33(5):54-58.

4张国铭,刘峰,张莹莹,李荣华,张爽.基于预形变热处理对GH4169蠕变性能影响的研究[J].合成材料老化与应用,2021,50(1):29-31.

5韦康,王涛,张明军,张勇,李钊,万志鹏.重复固溶对Inconel 718合金组织性能的影响[J].航空材料学报,2021,41(1):53-59. 被引量:1

6方海鹏,刘拥军,张小枫,孙亚非.热处理对GH4169电子束焊接头性能的影响研究[J].热加工工艺,2021,50(1):44-48. 被引量:5

7刘博志,邱丰,徐倩,林中楠,佟文伟,韩振宇.航空发动机涡轮盘轮缘凸块塑性变形失效分析[J].航空发动机,2022,48(3):121-126.

1王京.GH4169氩弧焊接头组织及力学性能研究[J].装备制造技术,2022(9):244-247.

2卞宏友,翟泉星,曲伸,杨光,王伟,王维.激光沉积修复GH738合金时效热处理组织及性能[J].稀有金属材料与工程,2019,48(1):317-322. 被引量:5

3张尧成,黄希望,杨莉,陈洪洲,戴军,张宁.热处理前后镍基高温合金激光熔覆层的组织和力学性能[J].机械工程材料,2016,40(11):22-26. 被引量:15

4方金祥,王玉江,董世运,徐滨士,闫世兴,宋超群,舒凤远,何鹏.激光熔覆Inconel718合金涂层与基体界面的组织及力学性能[J].中国机械工程,2019,30(17):2108-2113. 被引量:14

5张杰,张群莉,李栋,童文华,姚建华,冷志斌.δ时效处理对激光增材修复Inconel 718合金组织与性能的影响[J].中国激光,2020,47(1):66-73. 被引量:15

6张群莉,张杰,李栋,童文华,Liu Rong,宋立军,姚建华.不同时效温度下激光增材再制造IN718合金层的组织与性能研究[J].稀有金属材料与工程,2020,49(5):1785-1792. 被引量:5

7蔺永诚,陈小敏,陈明松.镍基合金的热变形行为及智能热加工技术研究进展[J].精密成形工程,2021,13(1):1-18. 被引量:5

8张小枫,刘拥军,张思远.GH4169高温合金螺柱失效分析[J].电焊机,2021,51(3):64-69. 被引量:2

9李维,高丙爽,翟心语,胥春燕,于耀华,刘威,张喆.时效工艺对GH4169合金弹簧丝微观组织及力学性能的影响[J].热加工工艺,2021,50(16):126-130. 被引量:1

10周庆军,赵彦广,谢勇,衣凤,严振宇,倪江涛.激光熔化沉积成形/修复GH4169合金组织性能调控研究进展[J].稀有金属,2022,46(5):636-651. 被引量:3

1王喜琴,张贵一,王业伟.2195铝锂合金热处理工艺研究[J].上海航天,2014,31(B06):53-55. 被引量:8

2刘风雷,钟群鹏.一个新的蠕变寿命估算公式的推出[J].北京航空航天大学学报,1990(4):53-57.

3刘雪峰,汪凌云,涂铭旌.铝锂合金热变形穿晶韧性断裂原因分析[J].机械强度,2003,25(2):219-221. 被引量:1

4李振荣,田素贵,赵忠刚,陈礼清,刘相华.热连轧对GH4169合金蠕变行为的影响[J].中国有色金属学报,2011,21(7):1541-1546. 被引量:8

5冯秋元,李廷举,丁志敏,金俊泽.闪光对焊技术研究现状及发展趋势[J].材料科学与工艺,2008,16(1):49-53. 被引量:32

6为什么某些金属和合金较难去预处理?(上)[J].国际表面处理,2003(3):31-35.

7汤少凌,汤立群.产品零件的裂纹分析与创新热处理工艺研究[J].机械工程师,2015(11):95-97.

8舒震.提高高铝锌合金的力学性能和耐磨性[J].湖南大学学报:自然科学版,1995,22(1):98-102. 被引量:7

9李伟,刘平,苏娟华,刘勇,康布熙,田保红.时效与形变对Cu-Cr-Zr合金性能的影响[J].特种铸造及有色合金,2004(6):25-26. 被引量:22

10邹明,马春江,赵旭峰.挤压AZ63A合金固溶处理工艺的确定[J].机械工程材料,2007,31(10):32-34. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG156.9[金属学及工艺—热处理]

Citation Information:

Study is made of the effects of different heat treatment on creeping property of GH4169 alloy through the testing of creeping property and microstructure observation. The results show that the hot continuous rolled alloy after standard heat treatment precipitates less 8 phase and has better creeping property than the radial forged alloy after the standard heat treatment. The hot continuous rolled alloy after di- rect-aged treatment precipitates little 8 phase with longer creeping life, which is twice as much as that of the radial forged alloy after standard heat treatment. The radial forged alloy produces transgranular fracture during creeping,while the hot continuous rolled alloy produces intergranular fracture.

quote

GB/T 7714-2015 [1] KONG Yong-hua, LI Hu-yan, CHEN Guo-sheng, et al. Effects of Different Heat Treatment on Creeping Property of GH4169 Alloy[J]. Rare Metals and Cemented Carbides, 2014(1): 52-56.
MLA [1] KONG Yong-hua, et al., "Effects of Different Heat Treatment on Creeping Property of GH4169 Alloy." Rare Metals and Cemented Carbides, no. 1, 2014, pp. 52-56.
APA [1] KONG Yong-hua, LI Hu-yan, CHEN Guo-sheng, XIE Li-xiong, & ZHU Shi-gen. (2014). Effects of Different Heat Treatment on Creeping Property of GH4169 Alloy. Rare Metals and Cemented Carbides(1), 52-56.
IEEE [1] KONG Yong-hua, LI Hu-yan, CHEN Guo-sheng, XIE Li-xiong, and ZHU Shi-gen, "Effects of Different Heat Treatment on Creeping Property of GH4169 Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 52-56, 2014. keywords: {GH4169 alloy;heat treatment;creeping property;δ phase;radial forged alloy;hot continuousrolled alloy}