Quantifying lithium lost to plating and formation of the solid-electrolyte interphase in graphite and commercial battery components AITranslate

KTH Royal Institute of Technology; KTH Royal Institute of Technology; KTH Royal Institute of Technology; KTH Royal Institute of Technology; KTH Royal Institute of Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Direct quantification of plated Li, dead Li, and lithium in SEI and graphite. • Post mortem method based on 7Li NMR for graphite and commercial battery components. • Case study on materials from commercial cells with complicated aging history. • Verification protocol in digested samples by ICP-OES and liquid-state NMR. • Novel set of electrochemical bounds for SEI formed during lithium plating. A key degradation mechanism in lithium-ion batteries (LIBs) is the irreversible loss of cyclable lithium during cycling. At the graphite negative electrode, this loss occurs through the deposition of lithium-containing compounds in the solid-electrolyte interphase (SEI) and through plating of metallic lithium, resulting in so-called dead lithium. The separate quantification of SEI and dead lithium has so far been a challenge in post mortem analysis of commercial LIBs. Here we report a simple and fast 7Li nuclear magnetic resonance spectroscopy (NMR) protocol applied to solid-state samples derived from lab-built batteries to independently quantify these and other lithium species in graphite electrodes without the need for specialized cell design nor knowledge of prior charging history. The metallic lithium content is corroborated by electrochemical calculations; the total amount of lithium is also determined from 7Li liquid-state NMR and inductively coupled plasma optical emission spectroscopy (ICP-OES) in suitably digested samples. Factors influencing accuracy like the sample handling process, the radiofrequency skin effect, and re-intercalation losses are investigated. Measurements on samples from commercial cells aged under realistic conditions demonstrate quantification of dead lithium and remaining ionic species (SEI), and further reveal lithium dendrites entrained in the separator following cell disassembly. The method uses conventional and widely available NMR instrumentation and is applicable to samples from lab-scale test cells or commercial batteries, thereby presenting a vast improvement over prior post mortem methods. Graphical abstract Download : Download high-res image (151KB) Download : Download full-size image

KeyWords AITranslate

Lithium plating Irreversible Li: solidelectrolyte interphase (SEI) Graphite electrode Post mortem analysis NMR spectroscopy
No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2022.101527

Chinese Library Classification Number:

Citation Information:

Highlights • Direct quantification of plated Li, dead Li, and lithium in SEI and graphite. • Post mortem method based on 7Li NMR for graphite and commercial battery components. • Case study on materials from commercial cells with complicated aging history. • Verification protocol in digested samples by ICP-OES and liquid-state NMR. • Novel set of electrochemical bounds for SEI formed during lithium plating. A key degradation mechanism in lithium-ion batteries (LIBs) is the irreversible loss of cyclable lithium during cycling. At the graphite negative electrode, this loss occurs through the deposition of lithium-containing compounds in the solid-electrolyte interphase (SEI) and through plating of metallic lithium, resulting in so-called dead lithium. The separate quantification of SEI and dead lithium has so far been a challenge in post mortem analysis of commercial LIBs. Here we report a simple and fast 7Li nuclear magnetic resonance spectroscopy (NMR) protocol applied to solid-state samples derived from lab-built batteries to independently quantify these and other lithium species in graphite electrodes without the need for specialized cell design nor knowledge of prior charging history. The metallic lithium content is corroborated by electrochemical calculations; the total amount of lithium is also determined from 7Li liquid-state NMR and inductively coupled plasma optical emission spectroscopy (ICP-OES) in suitably digested samples. Factors influencing accuracy like the sample handling process, the radiofrequency skin effect, and re-intercalation losses are investigated. Measurements on samples from commercial cells aged under realistic conditions demonstrate quantification of dead lithium and remaining ionic species (SEI), and further reveal lithium dendrites entrained in the separator following cell disassembly. The method uses conventional and widely available NMR instrumentation and is applicable to samples from lab-scale test cells or commercial batteries, thereby presenting a vast improvement over prior post mortem methods. Graphical abstract Download : Download high-res image (151KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Yuan Fang, Alexander J. Smith, Rakel Wreland Lindström, et al. Applied Materials Today, 2022(28). DOI:10.1016/j.apmt.2022.101527.
MLA [1] Yuan Fang, et al., Applied Materials Today, no. 28, 2022, https://doi.org/10.1016/j.apmt.2022.101527.
APA [1] Yuan Fang, Alexander J. Smith, Rakel Wreland Lindström, Göran Lindbergh, & István Furó. (2022). Applied Materials Today(28). https://doi.org/10.1016/j.apmt.2022.101527
IEEE [1] Yuan Fang, Alexander J. Smith, Rakel Wreland Lindström, Göran Lindbergh, and István Furó, Applied Materials Today, no. 28, 2022, doi: 10.1016/j.apmt.2022.101527. keywords: {Lithium plating;Irreversible Li: solidelectrolyte interphase (SEI);Graphite electrode;Post mortem analysis;NMR spectroscopy}