Effects of Electrolyte Concentration on the Growth of CaTi_4(PO_4)_6 Bioceramic Membrane Prepared by Micro-arc Oxidation AITranslate
Abstract AITranslate
CaTi4(PO4)6 bioceramic membrane was directly prepared by micro-arc oxidation,and the effects of electrolyte concentration on the growth of micro-arc oxidized membrane were investigated.The results show that the weight of micro-arc oxidized membrane increases linearly with reaction time prolonged under the same electrolyte concentration.With electrolyte concentration increasing,membrane weight increases faster,membrane formation time shortens and breakdown voltage lowers,and Ca content of membrane surface increases while P content has little change.However,after the electrolyte concentration has increased to a certain extent,increasing electrolyte concentration will result in the decrease of Ca and P content on membrane surface.
KeyWords AITranslate
1赵中伟,陈爱良,陈星宇,孙培梅,李洪桂.脉冲阴极电沉积羟基磷灰石涂层[J].中国有色金属学报,2005,15(12):2023-2027. 被引量:7
2Han Yong, Hong Seong-Hyeon, Xu Kewei. Synthesis of nanocrystalline titania films by micro-arc oxidation[J]. Materials Letters, 2002,56 (5) : 744-747.
3Zhao Zhongwei, Li Honggui, Sun Peimei, et al. Novel electrodeposition process for preparing hydroxyapatite coating on titanium substrate[J]. Transaction Nonfer- rous Metals Social China,2005,15(6):1 368-1 372.
4Gross U, Muller-Mai C, Voigt C,et al. Tissue response in the femur of rabbits after implantation of a new calci- um titanium phosphate eomposition[J]. Key Engineering Materials, 2001, (192-195) : 383-386.
5Smukler-Moncler S, Calcusi G, Delecrin J, et al. Calcium- metallic- phosphates : A new coating biomaterial [J]. Bi- omat- Tissue Interfaces Adv Biomat, 1992, (10) : 377 - 383.
6Knabe C, Berger G, Gildenhaar R, et al. The modulation of osteogenesis in vitro by calcium titanium phosphate coatings[J]. Biomaterials, 2004,25 ( 20 ) : 4 911-4 919.
7Shen Meiling, Zhao Zhongwei, Wen Shimei, et al. Fabri- cation of CTP/HAp novel gradient composite bioceram- ies[J]. Transaction Nonferrous Metals Social China, 2007,17:1 385-1 390.
8Ute Ploska, Georg Berger. Solubility of compositions in the system CaTix Zr4-x (PO4)6 with x=0-4[J]. Biomate- rials,1997,18:1 671-1 675.
9赵玉峰,杨世彦,韩明武.等离子体微弧氧化技术及其发展[J].材料导报,2006,20(6):102-104. 被引量:34
10东青,陈传忠,王德云,雷廷权.铝及其合金的微弧氧化技术[J].中国表面工程,2005,18(6):5-9. 被引量:26
1钱海蓝,朱锋,夏克俭,陈治清,聂蓉蓉.人牙周膜成纤维细胞在微弧氧化陶瓷膜表面的生物相容性研究[J].口腔医学,2011,31(9):513-516. 被引量:1
2杨成,李源莹,吴晓玲,薛文斌.微弧氧化陶瓷膜表面骨髓间充质干细胞生物相容性实验[J].生物骨科材料与临床研究,2008,5(1):12-14. 被引量:2
3董慧敏,王穗海,舒文,徐伟文,吴英松.降钙素原的克隆表达及鉴定[J].广东医学,2009,30(7):1032-1034. 被引量:2
4聂蓉蓉,朱锋,沈丽茹,陈治清.纯钛表面不同厚度微弧氧化膜的形貌及相结构分析[J].生物医学工程学杂志,2010,27(2):354-357. 被引量:5
5陈跃瑜,吴英松,徐伟文,王穗海,姜永玮,彭娟,李明.降钙素原的克隆、表达及多抗制备[J].热带医学杂志,2007,7(3):226-229. 被引量:2
6王磊,陈建治,唐建国,贾暮云,石玉龙,闫凤英.纯钛表面微弧氧化膜的粗糙度与接触角[J].中国组织工程研究与临床康复,2009,13(42):8291-8294. 被引量:4
7陆雨桐,李涛,商晓盼,王亚锋,蔡兴伟.镁合金微弧氧化表面处理研究进展[J].生物医学工程学杂志,2016,33(5):1016-1019. 被引量:2
8张凯军,刘斌,董寅生,郭超,林萍华,盛晓波,储成林.钙磷生物陶瓷多孔骨修复材料的制备[J].生物骨科材料与临床研究,2007,4(2):51-53. 被引量:3
9王健平,李星海,孟祥才,刘杰,王静,卢艳萍.微量元素与钛基种植体微弧氧化陶瓷膜生物活性的关系[J].中国组织工程研究与临床康复,2010,14(3):509-512. 被引量:9
10王新国,袁建国,张丽旦,张思泉,刘雁,刘寿荣.硫化氢对大鼠肝窦内皮细胞凋亡影响[J].国际流行病学传染病学杂志,2012,39(5):297-300.
Basic Information:
DOI:
Chinese Library Classification Number:R318.08[医药卫生—生物医学工程]
Citation Information:
CaTi4(PO4)6 bioceramic membrane was directly prepared by micro-arc oxidation,and the effects of electrolyte concentration on the growth of micro-arc oxidized membrane were investigated.The results show that the weight of micro-arc oxidized membrane increases linearly with reaction time prolonged under the same electrolyte concentration.With electrolyte concentration increasing,membrane weight increases faster,membrane formation time shortens and breakdown voltage lowers,and Ca content of membrane surface increases while P content has little change.However,after the electrolyte concentration has increased to a certain extent,increasing electrolyte concentration will result in the decrease of Ca and P content on membrane surface.
quote
| GB/T 7714-2015 | [1] LUO Ting, ZHAO Zhong-wei, CHEN Xing-yu. Effects of Electrolyte Concentration on the Growth of CaTi_4(PO_4)_6 Bioceramic Membrane Prepared by Micro-arc Oxidation[J]. Rare Metals and Cemented Carbides, 2011(2): 22-25. |
| MLA | [1] LUO Ting, et al., "Effects of Electrolyte Concentration on the Growth of CaTi_4(PO_4)_6 Bioceramic Membrane Prepared by Micro-arc Oxidation." Rare Metals and Cemented Carbides, no. 2, 2011, pp. 22-25. |
| APA | [1] LUO Ting, ZHAO Zhong-wei, & CHEN Xing-yu. (2011). Effects of Electrolyte Concentration on the Growth of CaTi_4(PO_4)_6 Bioceramic Membrane Prepared by Micro-arc Oxidation. Rare Metals and Cemented Carbides(2), 22-25. |
| IEEE | [1] LUO Ting, ZHAO Zhong-wei, and CHEN Xing-yu, "Effects of Electrolyte Concentration on the Growth of CaTi_4(PO_4)_6 Bioceramic Membrane Prepared by Micro-arc Oxidation," Rare Metals and Cemented Carbides, no. 2, pp. 22-25, 2011. keywords: {CaTi4(PO4)6 bioceramic membrane;micro-arc oxidation;electrolyte concentration;(NaPO3)6} |