Abstract AITranslate

The D76.2 mm and L50 mm-size LaB6 polycrystal was prepared by pre-pressing of LaB6 powder, followed by repeated hot-pressing sintering. The product has a relative density of more than 95 %,and its shape is complete without defects.

KeyWords AITranslate

LaB6 polycrystal high density pre-pressing forming repeated hot-pressing sintering

1Paderno Y B,Paderno V,Filippov V. Some crystal chem-istry relation ships in eutectic crystallization of d- and f- transition metals borides[J]. J Alloys and Compounds, 1995, (219) : 116-118.

2Paderno V,Paderno Y. Features of the real structure of LaB6 single crystals[J]. J Alloys and Compounds, 1995, (219) :228-231.

3Paderno Y,Paderno V, Filippov V. Some peculiarities of structure formation in eutectic d- and f-transition metals boride alloys[J]. J Alloys and Compounds, 1990, (163) : 561-569.

4《稀有金属应用》编写组.稀有金属应用[M].北京:冶金工业出版社,1985.

5XB/T501--2008,六硼化镧[s].

6高瑞兰,于化顺,于普涟,韩建德,闵光辉,杨晓亮.LaB_6多晶材料的制备工艺研究[J].山东大学学报:工学版,2002,32(6):593-596. 被引量:13

1成维,黄美松,杨露辉,张耀斌,陈云志,黄志.低压固相烧结制备高致密度LaB_6多晶体[J].矿冶工程,2014,34(2):122-124. 被引量:3

2梁超龙,张忻,张久兴,张繁星,王杨.La_(1-x)Nd_xB_6阴极材料的制备及性能研究[J].无机材料学报,2015,30(4):363-368. 被引量:2

3马飞文,王吉林,廖和杰,郑国源,龙飞,邹正光.放电等离子体烧结六硼化镧(LaB_(6))及其工艺研究[J].中国陶瓷,2021,57(2):17-23.

1梁超龙,张忻,张久兴,张繁星,王杨.La_(1-x)Nd_xB_6阴极材料的制备及性能研究[J].无机材料学报,2015,30(4):363-368. 被引量:2

2马飞文,王吉林,廖和杰,郑国源,龙飞,邹正光.放电等离子体烧结六硼化镧(LaB_(6))及其工艺研究[J].中国陶瓷,2021,57(2):17-23.

3余艺平,王松,李伟.Ce元素固溶掺杂对LaB6阴极材料电子逸出功的影响[J].稀有金属材料与工程,2021,50(6):2201-2207. 被引量:2

4余艺平,王松,李伟.具有(100)择优取向的高致密LaB_(6)多晶材料的制备与表征[J].中南大学学报:英文版,2022,29(4):1118-1123.

5余艺平,王松,李伟.多元镧基六硼化物固溶体材料研究进展[J].稀有金属材料与工程,2023,52(5):1954-1962.

1成维,黄美松,杨露辉,张耀斌,陈云志,黄志.低压固相烧结制备高致密度LaB_6多晶体[J].矿冶工程,2014,34(2):122-124. 被引量:3

2成维,黄美松,苏正夫,王志坚,贾帅广,杨露辉.高纯高致密度LaB_6多晶体的制备[J].中国稀土学报,2015,33(3):323-327. 被引量:3

3李志红,谭勇.光电直读光谱仪同时测定精锡中杂质元素[J].云锡科技,1999,26(3):46-51.

4龙卧云,卢安贤.添加剂对低压烧结Zr50Al15Ni10Cu25非晶态粉末力学性能的影响[J].铸造工程,2012(4):8-12.

5肖代红,李秀秀,申婷婷,宋旼.添加LaB_6对超细晶WC-Ni_3Al合金的组织与力学性能影响[J].中南大学学报:自然科学版,2015,46(1):81-87. 被引量:8

6常明清,张良,李广.五轴双铣刀数控组合机床[J].机械,2014,41(11):64-68.

7刘俊,张平,张国根,李新涛.基于LabVIEW的大圆环平面在线检测系统的研究与开发[J].组合机床与自动化加工技术,2016(7):111-113. 被引量:2

8Tsinghua University Computer-aided Casting Engineering Lab Casting CAE Lab of CIMS/ERC[J].中国铸造:英文版,2005,0(1):74-74.

9王桂森,万熠,宋明大,孙菲菲.基于LabVIEW的铁磁性材料无损检测系统开发[J].工具技术,2016,50(11):96-99. 被引量:2

10陶兆胜,杨文果.基于Lab VIEW的数控轧辊车床车刀检测系统[J].工具技术,2006,40(7):73-75.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.454[金属学及工艺—金属材料]

Citation Information:

The D76.2 mm and L50 mm-size LaB6 polycrystal was prepared by pre-pressing of LaB6 powder, followed by repeated hot-pressing sintering. The product has a relative density of more than 95 %,and its shape is complete without defects.

quote

GB/T 7714-2015 [1] HUANG Mei-song, CHEN Yun-zhi, ZHANG Yao-bin, et al. Preparation of High-density LaB_6 Polycrystal[J]. Rare Metals and Cemented Carbides, 2012(3): 33-34.
MLA [1] HUANG Mei-song, et al., "Preparation of High-density LaB_6 Polycrystal." Rare Metals and Cemented Carbides, no. 3, 2012, pp. 33-34.
APA [1] HUANG Mei-song, CHEN Yun-zhi, ZHANG Yao-bin, ZHANG Ke-xiang, & LIU Shu-ping. (2012). Preparation of High-density LaB_6 Polycrystal. Rare Metals and Cemented Carbides(3), 33-34.
IEEE [1] HUANG Mei-song, CHEN Yun-zhi, ZHANG Yao-bin, ZHANG Ke-xiang, and LIU Shu-ping, "Preparation of High-density LaB_6 Polycrystal," Rare Metals and Cemented Carbides, no. 3, pp. 33-34, 2012. keywords: {LaB6 polycrystal;high density;pre-pressing forming;repeated hot-pressing sintering}