Abstract AITranslate
Experiments were carried out to research the hardness, tensile strength and fracture toughness of high volume fraction SiCp/A1 composite. The results show that with the volume fraction of SiC particles increasing,Vickers hardness of the composite monotonically increases, but tensile strength and fracture toughness increase at first and then decrease, both up to the maximum value when SiC volume fraction is 55%.
KeyWords AITranslate
1Ren Shu-bin, He Xin-bo,Qu Xuan-hui,et al. Effect of controlled inierfacial reaction on the microstructure and properties of the SiCp/Al composites prepared by pres sureless infihration[J]. Journal of Alloys and Com- pounds,2008,455(1/2) :424-431.
2Ren Shu-bin, He Xin-bo,Qu Xtmn-hui,et al. Effect of Si addition to Al-8Mg alloy on the microstructure and ther- too-physical properties of SiCp/Al composites prepared by pressureless infiltration[J]. Materials Science and En gineering B, 2007,138 (3) : 263-270.
3张强,武高辉,孙东立,韩杰才.高体积分数SiCp/Al复合材料的微观组织与导热性能[J].材料科学与工艺,2006,14(5):474-477. 被引量:10
4褚克,贾成厂,尹法章,梅雪珍,曲选辉.高体积分数SiC_P/Al复合材料电子封装盒体的制备[J].复合材料学报,2006,23(6):108-113. 被引量:20
5宋旼,谢灿强,贺跃辉.颗粒失效对SiC增强铝基复合材料屈服应力的影响模型[J].中国有色金属学报,2010,20(2):244-249. 被引量:12
6Miller W S, Humphreys F J. Strengtening mechanisms in particulate metal matrix composites [J]. Scripta Metall, 1991,25:33-38.
7Liu G, Sun J, Nan C W, et al. Experiment andmultiscale modeling of the coupled influence of constituents and- precipitates on the ductile fracture of heat-treatable alu- minumalloys[J]. Acta Mater, 2005, 53 (10): 3 459- 3 468.
1马天飞.玻璃/铝复合材料断裂性能的研究[J].光学精密工程,1994,2(1):9-13.
2侯大寅.纤维增强复合材料的断裂韧性探讨[J].天津纺织科技,1998,36(3):22-24. 被引量:1
3孟庆国,靳征谟.“材料损伤断裂机理和宏微观力学理论”研究获硕果[J].中国科学基金,1998,12(4):258-260.
4何梅琼.SiC颗粒强化铝基复合材料及其断裂韧性[J].铝加工,1998,21(2):55-58.
5毕豫,朱鸣峰,王日初,谭敦强,黎文献.SiC_(p(w))/Al 复合材料的研究现状[J].材料导报,2004,18(6):51-54. 被引量:4
6陈达强.倡导人性化的包装设计[J].中国包装,2007,27(4):48-49. 被引量:1
7郭英奎,赵晓华,周玉,李东波.ZrO_2/316L不锈钢复合材料的SEM分析[J].哈尔滨理工大学学报,2002,7(1):50-52. 被引量:3
8崔照雯,刘建金,王聪聪,梁栋,高鹏,贾成厂.碳纳米管和氧化铝颗粒在铜基复合材料中的协同作用[J].粉末冶金技术,2014,32(5):346-351. 被引量:6
9袁平.日出日落方位的判断及应用[J].考试周刊,2012(20):136-137. 被引量:3
10宋德风,徐凤芝,何春生.振动时效的试验研究[J].哈尔滨电工学院学报,1994,17(4):396-409.
Basic Information:
DOI:
Chinese Library Classification Number:TB333[一般工业技术—材料科学与工程]
Citation Information:
Experiments were carried out to research the hardness, tensile strength and fracture toughness of high volume fraction SiCp/A1 composite. The results show that with the volume fraction of SiC particles increasing,Vickers hardness of the composite monotonically increases, but tensile strength and fracture toughness increase at first and then decrease, both up to the maximum value when SiC volume fraction is 55%.
quote
| GB/T 7714-2015 | [1] FANG Ling, CHEN Kang-hua. Research on Fracture Behavior and Mechanism of High Volume Fraction SiC_P/Al Composite[J]. Rare Metals and Cemented Carbides, 2012(3): 39-43. |
| MLA | [1] FANG Ling, and CHEN Kang-hua. "Research on Fracture Behavior and Mechanism of High Volume Fraction SiC_P/Al Composite." Rare Metals and Cemented Carbides, no. 3, 2012, pp. 39-43. |
| APA | [1] FANG Ling, & CHEN Kang-hua. (2012). Research on Fracture Behavior and Mechanism of High Volume Fraction SiC_P/Al Composite. Rare Metals and Cemented Carbides(3), 39-43. |
| IEEE | [1] FANG Ling and CHEN Kang-hua, "Research on Fracture Behavior and Mechanism of High Volume Fraction SiC_P/Al Composite," Rare Metals and Cemented Carbides, no. 3, pp. 39-43, 2012. keywords: {high volume fraction;SiCe/A1 composite;tensile strength;fracture toughness;fracture mecha-nism} |