The Latest Development of Tertiary Layered Machinable Ti_2AlN Ceramic AITranslate
Abstract AITranslate
The study of tertiary layered machinable TizAIN ceramic is reviewed in respect of its electronic structure, mechanical property, oxidation behavior and thermoelectric property. Especially, the reason is explained for the lower fracture toughness and Vickers hardness but higher electrical conductivity of TizAIN compared with Ti2 AIC. Furthermore, the latest preparation and future applications of TizAIN are introduced.
KeyWords AITranslate
1闵新民.Electronic Structures and Bonding Properties of Ti_2AlC and Ti_3AlC_2[J].武汉理工大学学报:材料科学英文版,2007,22(1):27-30. 被引量:1
2梅炳初,徐学文,朱教群,刘俊.Ti_3Si_((1-x))Al_xC_2在900℃~1300℃空气中的氧化行为[J].稀有金属材料与工程,2005,34(6):895-898. 被引量:5
3艾桃桃,王芬,冯小明.Al_2O_3/TiAl基复合材料在空气中的高温氧化行为[J].中国科学:E辑,2009(1):166-173. 被引量:6
4王苹,梅炳初,闵新民,洪小林,周卫兵,严明.Si掺杂放电等离子合成Ti_2AlC/Ti_3AlC_2材料及理论分析[J].中国有色金属学报,2007,17(4):511-517. 被引量:11
5H.B. Zhang Y.W. Bao Y. C. Zhou.Current Status in Layered Ternary Carbide Ti_3SiC_2,a Review[J].材料科学技术:英文版,2009,25(1):1-38. 被引量:15
6梅炳初,徐学文,朱教群,刘俊.含铝Ti_3SiC_2在1100℃和1200℃空气中的循环氧化行为[J].中国有色金属学报,2004,14(5):772-776. 被引量:5
1严明,陈艳林,梅炳初,朱教群.块体Ti_2AlN/TiN复合材料的制备[J].武汉理工大学学报,2011,33(1):28-32.
2梁苏莹,康举,赵霞,战再吉.热压烧结Ti_2AlN金属陶瓷材料的物相及显微结构[J].航空材料学报,2017,37(3):73-77. 被引量:3
1潘兴浩,储茂友,王星明,刘宇阳,白雪,桂涛,张朝.非晶半导体薄膜用Te系化合物靶材制备[J].工程科学学报,2019,41(2):224-229. 被引量:3
2宋丽红,慕利斌.三元层状氮化物Ti2AN(A=Al,Ga)材料的合成及电学性质研究[J].真空科学与技术学报,2020,40(7):692-696.
3江涛.三元层状结构MAX相陶瓷材料的制备技术及其研究发展现状和发展趋势[J].现代技术陶瓷,2023,44(1):1-23.
1郑楠,于开坤,刘国清,张冠军.表面粗糙度对绝缘材料真空闪络特性的影响[J].电工电能新技术,2009,28(2):33-36. 被引量:17
2李杨,魏敦崧,潘卫国.燃料电池发展现状与应用前景[J].能源技术,2001,22(4):158-161. 被引量:13
3唐苏亚.钕铁硼永磁的发展现状与应用市场[J].微特电机,2001,29(4):39-40. 被引量:4
4琚兴宝.电力系统故障限流器的研究现状与应用前景[J].船电技术,2013,33(7):55-57. 被引量:2
5张友军.DC/AC逆变器技术及其应用综述[J].电气开关,2004,42(6):18-22. 被引量:14
6徐德新,诸亦新.燃料电池的开发现状与应用前景[J].江苏冶金,2000,28(2):25-28.
7金嘉琦,高兴.翻车机的技术现状与应用[J].科技视界,2013(30):12-13. 被引量:7
8徐通,王育飞,张宇,时珊珊,刘舒,方陈.直流配电网发展现状与应用前景分析[J].华东电力,2014,42(6):1069-1074. 被引量:14
9张玉卿.200MW火力发电机组PLC控制的现状与应用前景[J].东方电机,2000(2):112-115.
10孟宪军.变频调速技术的现状与应用[J].佳木斯大学学报:自然科学版,2007,25(1):38-40. 被引量:12
Basic Information:
DOI:
Chinese Library Classification Number:TM286[一般工业技术—材料科学与工程]
Citation Information:
The study of tertiary layered machinable TizAIN ceramic is reviewed in respect of its electronic structure, mechanical property, oxidation behavior and thermoelectric property. Especially, the reason is explained for the lower fracture toughness and Vickers hardness but higher electrical conductivity of TizAIN compared with Ti2 AIC. Furthermore, the latest preparation and future applications of TizAIN are introduced.
quote
| GB/T 7714-2015 | [1] AI Tao-tao. The Latest Development of Tertiary Layered Machinable Ti_2AlN Ceramic[J]. Rare Metals and Cemented Carbides, 2010(1): 50-55. |
| MLA | [1] AI Tao-tao. "The Latest Development of Tertiary Layered Machinable Ti_2AlN Ceramic." Rare Metals and Cemented Carbides, no. 1, 2010, pp. 50-55. |
| APA | [1] AI Tao-tao. (2010). The Latest Development of Tertiary Layered Machinable Ti_2AlN Ceramic. Rare Metals and Cemented Carbides(1), 50-55. |
| IEEE | [1] AI Tao-tao, "The Latest Development of Tertiary Layered Machinable Ti_2AlN Ceramic," Rare Metals and Cemented Carbides, no. 1, pp. 50-55, 2010. keywords: {TizAIN;tertiary layered machinable ceramic;electronic structure;performance;preparation;ap- plication} |