daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Revealing Cycling Rate-Dependent Structure Evolution in Ni-Rich Layered Cathode Materials AITranslate

Pacific Northwest National Laboratory; Xiamen University; University of Pittsburgh; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; University of Pittsburgh; Xiamen University; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High-rate cycling of a battery often leads to a compromised performance, such as reduced capacity, rapid voltage decay, and thermal runaway. Although the cycling rate-dependent performance is generally perceived to be associated with the equilibrium state of systems, the correlation between cycling rate and cathode degradation, in terms of structure evolution, has not been established. Using scanning transmission electron microscopy, we demonstrate that varying cycling rate alters phase transition products in the Ni-rich materials. Under low cycling rates, the sufficient Li vacancies favor the thorough mixing between transition metal and Li layers, resulting in the formation of a disordered rock salt structure; at high cycling rates, the significant kinetic barrier arising from the Li retention impedes Ni migration, leading to the growth of the spinel phase. Our subtle characterizations at atomic scale bridge the gap between the structure evolution and cycling rate and provide mechanistic insight into tailoring the battery rate capability.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01490

Chinese Library Classification Number:

Citation Information:

High-rate cycling of a battery often leads to a compromised performance, such as reduced capacity, rapid voltage decay, and thermal runaway. Although the cycling rate-dependent performance is generally perceived to be associated with the equilibrium state of systems, the correlation between cycling rate and cathode degradation, in terms of structure evolution, has not been established. Using scanning transmission electron microscopy, we demonstrate that varying cycling rate alters phase transition products in the Ni-rich materials. Under low cycling rates, the sufficient Li vacancies favor the thorough mixing between transition metal and Li layers, resulting in the formation of a disordered rock salt structure; at high cycling rates, the significant kinetic barrier arising from the Li retention impedes Ni migration, leading to the growth of the spinel phase. Our subtle characterizations at atomic scale bridge the gap between the structure evolution and cycling rate and provide mechanistic insight into tailoring the battery rate capability.

quote

GB/T 7714-2015 [1] Lianfeng Zou, Wengao Zhao, Zhenyu Liu, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01490.
MLA [1] Lianfeng Zou, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01490.
APA [1] Lianfeng Zou, Wengao Zhao, Zhenyu Liu, Haiping Jia, Jianming Zheng, Guofeng Wang, Yong Yang, JiGuang Zhang, & Chongmin Wang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01490
IEEE [1] Lianfeng Zou, Wengao Zhao, Zhenyu Liu, Haiping Jia, Jianming Zheng, Guofeng Wang, Yong Yang, JiGuang Zhang, and Chongmin Wang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01490.