daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research on Preparation of Titanium Dioxide Ceramic Film on Titanium Alloy Surface by Micro-arc Oxidation AITranslate

School of Mechanical Engineering, Shanghai Institute of Technology;School of Social Sciences, University of Shanghai for Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Titanium dioxide films (i. e. biomedical ceramic films) were prepared on titanium alloy surface by micro-arc oxidation,and their structure, morphology and elemental composition were analyzed by XRD, SEM and EDX. The influences of electrolyte pH and micro-arc oxidation voltage on micro-arc oxidation process were investigated. The results show that with electrolyte pH and micro-arc oxidation voltage in- creasing,the film is more homogenous and its surface pores are of larger number and size. The film is mainly composed of anatase and rutile Ti02 and the content of anatase phase increases with the increase of micro-arc voltage. The current density increases at first and then decreases with oxidation time increasing, and meanwhile it increases as electrolyte pH increases. The porous ceramic film can be obtained under the conditions of electrolyte pH value of 11 and micro-arc oxidation voltage of 500 V,and the obtained film has homogeneous-distribution pores.

KeyWords AITranslate

titanium dioxide ceramic film micro-arc oxidation titanium alloy electrolyte pH voltage

1张玉梅.钛及钛合金在口腔科应用的研究方向[J].生物医学工程学杂志,2000,17(2):206-208. 被引量:80

2Long M,Rack H J. Titanium alloys in total joint replace ment-a materials science perspective[J]. Biomateri- als,1998,19(18) :1 621-1 639.

3Brunette D M,Tengvall P,Textor M,et al. Titanium in medicine : material science, surface science, engineering, biological response and medical applications [M]. Ber- lin: Springer, 2001.

4Wen H B,Wolke J G C, Wijn J R, etal. Fast precipita- tion of calcium phosphate layers on titanium induced by simple chemical treatment[J]. Biomaterials, 1997, 18 (22);1 471-1 478.

5Sehreckenbach J P, Marx G, Schlottig F, et al. Charac- terization o{ anodic spark-converted titanium surface forbiomedical applications[J] Journal of Materials Science, 1999,10 (8) :453-457.

6唐光昕,张人佶,颜永年.钙盐浓度对复合氧化法制备多孔二氧化钛涂层表面结构的影响[J].钛工业进展,2005,22(2):38-42. 被引量:4

7刘亮,郭锋,李鹏飞,张娟娟,刘存弟,申元.电解液钙磷含量对医用TC4钛合金微弧氧化膜的影响[J].金属热处理,2010,35(1):77-80. 被引量:12

8Fini M,Cigada A,Rondelli G,et al. In vitro and in vivo behaviour of Ca- and P-enriched anodized titanium[J]. Biomaterials,1999,20:1 587-1 594.

9SuI Y T. The significance of the surface properties o{ oxidized titanium to the bone response: special emphasis on potential biochemical bonding of oxidized titanium implant[J]. Biomaterials, 2003 , 24 (22) : 3 893-3 907.

10Hench L L. An introduction to bio-ceramics[M]. Sin- gapore: World Scientific Publishing Co Pte Ltd, 1993. 181-186.

1李斌锋,吴浚郊.灰铸铁缸体、缸盖铸件某些表面孔洞类缺陷的消除[J].中国铸造装备与技术,2004,39(4):34-36. 被引量:2

2徐双钱.脉冲占空比对钛合金微弧氧化膜的影响[J].甘肃科技,2017,33(3):15-16. 被引量:2

3颜炳祥,马新初.凸轮轴重熔淬火表面孔洞缺陷形成原因分析[J].机械工程材料,2004,28(6):49-50. 被引量:5

4徐志辉,杜希刚,张守丰,麻硕.HT250铸件表面孔洞缺陷分析[J].失效分析与预防,2011,6(4):229-231. 被引量:2

5蒙晓涓,李卫京,崔世海,韩建民.Ti6Al4V合金微弧氧化陶瓷膜的组织结构研究[J].航空材料学报,2009,29(2):39-42. 被引量:21

6刘东杰,蒋百灵,刘政,李红杰.纳米SiO_2添加剂对镁合金微弧氧化陶瓷层组织结构及耐蚀性的影响[J].材料保护,2013,46(7):8-10. 被引量:5

7荣晖,马凤仓,刘平,李伟,刘新宽,陈小红,何代华.微弧氧化工艺对Ti-6Al-4V钛合金表面氧化膜厚度及表面形态的影响[J].金属热处理,2014,39(12):23-27. 被引量:8

8刘志勇,孟根巴根,王丽云,宋苓芝,尹绍江.Q235B中厚板表面孔洞缺陷分析[J].河北冶金,2012(7):56-58.

9郭永彦.建筑用钢表面电弧喷涂铝涂层的耐蚀性[J].铸造技术,2013,34(9):1160-1162. 被引量:5

10张建民,李世琼,邹敦叙,仲增塘.表面涂层对等温锻造TiAl合金超塑性的影响[J].材料研究学报,1997,11(5):503-506. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

Titanium dioxide films (i. e. biomedical ceramic films) were prepared on titanium alloy surface by micro-arc oxidation,and their structure, morphology and elemental composition were analyzed by XRD, SEM and EDX. The influences of electrolyte pH and micro-arc oxidation voltage on micro-arc oxidation process were investigated. The results show that with electrolyte pH and micro-arc oxidation voltage in- creasing,the film is more homogenous and its surface pores are of larger number and size. The film is mainly composed of anatase and rutile Ti02 and the content of anatase phase increases with the increase of micro-arc voltage. The current density increases at first and then decreases with oxidation time increasing, and meanwhile it increases as electrolyte pH increases. The porous ceramic film can be obtained under the conditions of electrolyte pH value of 11 and micro-arc oxidation voltage of 500 V,and the obtained film has homogeneous-distribution pores.

quote

GB/T 7714-2015 [1] CHEN Yin, WANG Pei. Research on Preparation of Titanium Dioxide Ceramic Film on Titanium Alloy Surface by Micro-arc Oxidation[J]. Rare Metals and Cemented Carbides, 2013(1): 41-44.
MLA [1] CHEN Yin, and WANG Pei. "Research on Preparation of Titanium Dioxide Ceramic Film on Titanium Alloy Surface by Micro-arc Oxidation." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 41-44.
APA [1] CHEN Yin, & WANG Pei. (2013). Research on Preparation of Titanium Dioxide Ceramic Film on Titanium Alloy Surface by Micro-arc Oxidation. Rare Metals and Cemented Carbides(1), 41-44.
IEEE [1] CHEN Yin and WANG Pei, "Research on Preparation of Titanium Dioxide Ceramic Film on Titanium Alloy Surface by Micro-arc Oxidation," Rare Metals and Cemented Carbides, no. 1, pp. 41-44, 2013. keywords: {titanium dioxide ceramic film;micro-arc oxidation;titanium alloy;electrolyte pH;voltage}