Study on Microstructure and Properties of WC Reinforced Mo_2FeB_2-based Cermets AITranslate
Abstract AITranslate
Different amounts of WC was added to the ternary boride Mo2FeB2-based cermet and then vacuum liquid phase sintering was carried out.The sintered samples were characterized.The results show that WC addition doesn't affect the in-situ liquid phase reaction process to generate the ternary boride Mo2FeB2.WC can be the nucleation center of Mo2FeB2 particle to promote material densification during sintering.WC particles and Mo2FeB2 particles well combine to form dual hard phase,dispersing in Fe-based binder phase and effectively enhancing hardness and wear resistance of the Mo2FeB2-based cermet.When mass fraction of the added WC is 20%,the sintered sample has the highest hardness of HRA87.9improved by 7.2%,and the best wear resistance increased by 10 times under the experimental conditions of wheel grinding.
KeyWords AITranslate
1牛立斌,郭建光,赵勇,弓旭东,刘丹,龙裕轩.外加电磁场对原位合成WC机制的影响[J].中国钨业,2016,31(3):55-58.
2从善海,彭家健,陶则旭,张志伟.TiC含量对Mo_2FeB_2基金属陶瓷的组织与力学性能的影响[J].粉末冶金工业,2017,27(3):49-52. 被引量:5
3陶则旭,从善海,彭家健,王晓峰.多组元硬质相增强Mo2FeB2基金属陶瓷的组织和性能研究[J].粉末冶金工业,2018,28(3):44-47. 被引量:4
4陶则旭,从善海,彭家健.添加C、Si元素对Mo_2FeB_2基金属陶瓷组织及力学性能的影响[J].武汉科技大学学报,2018,41(3):174-179. 被引量:1
5闫东东,余海洲,刘文俊.Ni添加剂对Mo2FeB2基金属陶瓷的显微组织和力学性能的影响[J].硬质合金,2020,37(1):38-42. 被引量:2
6杨欣,尹海清,汤益纯,徐斌,张聪,张瑞杰,王永伟,姜雪,杨国强,曲选辉.TiB_(2)添加对MoCoB基金属陶瓷组织及性能的影响[J].硬质合金,2021,38(5):307-316. 被引量:1
7刘宇,魏祥,魏修宇,彭广威,刘宝刚,孔令男,汪力,吴吉文.Mo_(2)FeB_(2)基金属陶瓷的研究进展[J].硬质合金,2021,38(5):376-385. 被引量:1
8牛立斌,郭建光,赵勇,弓旭东,刘丹,龙裕轩.外加电磁场对原位合成WC机制的影响[J].精密成形工程,2016,8(3):21-24.
1庞立娟,邓刚,张雪峰,肖洪.Ti1-xWxC(x=0~1.00)固溶体型碳化物弹性性质的第一性原理研究[J].粉末冶金工业,2018,28(2):25-29. 被引量:1
2陶则旭,从善海,彭家健.添加C、Si元素对Mo_2FeB_2基金属陶瓷组织及力学性能的影响[J].武汉科技大学学报,2018,41(3):174-179. 被引量:1
3李万发,周佳,王浩,吕学鹏,郑勇.钒添加量对Mo2FeB2基金属陶瓷显微组织和力学性能的影响[J].机械工程材料,2019,43(11):32-36.
4耿文霞,王秋林,万斌,徐如涛,李昂,赵龙志.TiC_p/Fe复合材料的界面反应[J].粉末冶金工业,2020,30(4):51-56. 被引量:2
5宋杰光,杨雪晴,吴春晓,骆辉辉,何春艳,林国坚,官志强,王瑞花,陈爱霞.包裹型SiO_(2)/Al复合粉体的制备及烧结性能研究[J].粉末冶金技术,2021,39(1):62-68.
6魏祥,彭广威,鱼宏斌,刘宝刚,汪力,孔令男.硼含量对Fe_(2)B-Mo_(2)FeB_(2)基金属陶瓷微观组织与性能的影响[J].金属热处理,2021,46(10):58-64. 被引量:2
7杨欣,尹海清,汤益纯,徐斌,张聪,张瑞杰,王永伟,姜雪,杨国强,曲选辉.TiB_(2)添加对MoCoB基金属陶瓷组织及性能的影响[J].硬质合金,2021,38(5):307-316. 被引量:1
8刘宇,魏祥,魏修宇,彭广威,刘宝刚,孔令男,汪力,吴吉文.Mo_(2)FeB_(2)基金属陶瓷的研究进展[J].硬质合金,2021,38(5):376-385. 被引量:1
9李文戈,张博文,邓伟涛.船机修造用Mo_(2)FeB_(2)金属陶瓷涂层的有限元模拟及性能分析[J].上海海事大学学报,2022,43(1):119-126.
10尹海清,汤益纯,张聪,徐斌,袁强强,吴灵芝,曲选辉.金属陶瓷材料的国内外研究进展[J].硬质合金,2022,39(5):327-334. 被引量:1
1李玉柱,赵文广.镍和铬对Mo_2FeB_2基金属陶瓷高温抗氧化性能的影响[J].机械工程材料,2011,35(10):91-94. 被引量:3
2张志伟,从善海,胡梅.NbC含量对Mo_2FeB_2基金属陶瓷的显微组织和力学性能的影响[J].粉末冶金工业,2015,25(5):52-55. 被引量:8
3郑建智,承新,郑勇,严永林,赵能伟.烧结工艺和碳加入量对Mo_2FeB_2基金属陶瓷显微组织和力学性能的影响[J].机械工程材料,2009,33(3):31-34. 被引量:8
4魏祥,陈志国,黄奇胜.Fe_2B-Mo_2FeB_2基金属陶瓷的显微组织与性能[J].中国有色金属学报,2015,25(4):1012-1017. 被引量:3
5余海洲,刘文俊,张明松,郑勇.Mo_2FeB_2基金属陶瓷的相变及其显微组织演变研究Ⅰ:相变[J].硬质合金,2011,28(3):137-142. 被引量:10
6严孟凯,季根顺,马文林,孟军虎.合金元素对Mo_2FeB_2基金属陶瓷组织及性能的影响[J].粉末冶金技术,2014,32(4):243-247. 被引量:7
7庞旭明,郑勇,王少刚,王秋红.Mn对Mo_2FeB_2基金属陶瓷组织和力学性能的影响[J].中国有色金属学报,2009,19(9):1618-1624. 被引量:7
8陈继欣,郑勇,程鹏,吕学鹏,王秋红.硬质相晶粒尺寸对Mo_2FeB_2基金属陶瓷断裂韧性的影响[J].硬质合金,2013,30(5):237-241. 被引量:3
9庞旭明,郑勇,承新.反应烧结法制备Mo_2FeB_2基金属陶瓷的研究[J].硬质合金,2008,25(2):73-77. 被引量:10
10王秋红,郑勇,余海洲.烧结气氛对Mo_2FeB_2基金属陶瓷显微组织和力学性能的影响[J].硬质合金,2010,27(5):281-286. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
Different amounts of WC was added to the ternary boride Mo2FeB2-based cermet and then vacuum liquid phase sintering was carried out.The sintered samples were characterized.The results show that WC addition doesn't affect the in-situ liquid phase reaction process to generate the ternary boride Mo2FeB2.WC can be the nucleation center of Mo2FeB2 particle to promote material densification during sintering.WC particles and Mo2FeB2 particles well combine to form dual hard phase,dispersing in Fe-based binder phase and effectively enhancing hardness and wear resistance of the Mo2FeB2-based cermet.When mass fraction of the added WC is 20%,the sintered sample has the highest hardness of HRA87.9improved by 7.2%,and the best wear resistance increased by 10 times under the experimental conditions of wheel grinding.
quote
| GB/T 7714-2015 | [1] HU Mei, CONG Shan-hai, ZHANG Zhi-wei. Study on Microstructure and Properties of WC Reinforced Mo_2FeB_2-based Cermets[J]. Rare Metals and Cemented Carbides, 2015(4): 29-33. |
| MLA | [1] HU Mei, et al., "Study on Microstructure and Properties of WC Reinforced Mo_2FeB_2-based Cermets." Rare Metals and Cemented Carbides, no. 4, 2015, pp. 29-33. |
| APA | [1] HU Mei, CONG Shan-hai, & ZHANG Zhi-wei. (2015). Study on Microstructure and Properties of WC Reinforced Mo_2FeB_2-based Cermets. Rare Metals and Cemented Carbides(4), 29-33. |
| IEEE | [1] HU Mei, CONG Shan-hai, and ZHANG Zhi-wei, "Study on Microstructure and Properties of WC Reinforced Mo_2FeB_2-based Cermets," Rare Metals and Cemented Carbides, no. 4, pp. 29-33, 2015. keywords: {Mo2FeB2-based cermet;WC reinforcement;microstructure;hardness;wear resistance} |