Grain Refinement of γ-TiAl-based Compositesand Their Improved Hot-workability AITranslate
Abstract AITranslate
This article describes grain refinement of γ-TiAl-based composites and their improved hot-workability.Discussion is made on the microstructure,compressive and extensile properties and isothermal casting defrormation of the hot-worked material.
KeyWords AITranslate
1Bohn R,et al.Processing and Properties of Nanocrystalline Materials[M].Warrendale:TMS,1996.355.
2Gerling R,et al.Advances in Powder Metallurgy & Particulate Materials Princeton-1995[M].MPIF,1995.1 291.
3Bohn R,et al.Improved Hot-Workability of γ-TiAl-Based Composites by Grain Refinement,In termetallics and Superalloys [M].Gerrmany:DGM, 2002.271.
1许明圣.含Al_2Y化合物中间合金对AZ31镁合金组织的影响[J].热加工工艺,2015,44(24):68-70.
2孙明,吴国华,戴吉春,庞松,丁文江.Zr在镁合金中晶粒细化行为研究进展[J].铸造,2010,59(3):255-259. 被引量:35
3李立新,刘雪峰,汪凌云.材料热加工组织性能数值模拟的现状及发展[J].特殊钢,2000,21(1):1-6. 被引量:6
4房贵如.材料热加工工艺模拟的研究现状及技术发展趋势[J].中国机械工程,1998,9(11):71-72. 被引量:6
5马晓光,刘相法,丁海民.铝合金中Si含量对Al-Ti-C细化效果的影响[J].铸造,2008,57(5):491-493. 被引量:3
6黄明宇,王典钧,陆惠生.供应态 LD10 铝合金的超塑性试验研究[J].轻合金加工技术,1998,26(4):33-35. 被引量:4
7刘相法,杨阳,边秀房,亓效刚,马家骥.杆状AlTiB中间合金的组织形貌及晶粒细化行为的研究[J].铸造,1996,45(10):6-9. 被引量:16
8于兴哲,赵海燕,宋月清,崔舜.V-5Cr-5Ti合金的热加工性能[J].稀有金属材料与工程,2010,39(3):552-555. 被引量:3
9应上进.材料热加工工艺模拟技术的现状及发展趋势[J].江苏煤炭,2002(3):22-23. 被引量:1
10仲召军,李龙,周德敬.铸造Al-Si合金细化变质处理技术的研究进展[J].铸造,2016,65(3):242-247. 被引量:22
Basic Information:
DOI:
Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]
Citation Information:
This article describes grain refinement of γ-TiAl-based composites and their improved hot-workability.Discussion is made on the microstructure,compressive and extensile properties and isothermal casting defrormation of the hot-worked material.
quote
| GB/T 7714-2015 | [1] HUANG Hong. Grain Refinement of γ-TiAl-based Compositesand Their Improved Hot-workability[J]. Rare Metals and Cemented Carbides, 2004(3): 58-60. |
| MLA | [1] HUANG Hong. "Grain Refinement of γ-TiAl-based Compositesand Their Improved Hot-workability." Rare Metals and Cemented Carbides, no. 3, 2004, pp. 58-60. |
| APA | [1] HUANG Hong. (2004). Grain Refinement of γ-TiAl-based Compositesand Their Improved Hot-workability. Rare Metals and Cemented Carbides(3), 58-60. |
| IEEE | [1] HUANG Hong, "Grain Refinement of γ-TiAl-based Compositesand Their Improved Hot-workability," Rare Metals and Cemented Carbides, no. 3, pp. 58-60, 2004. keywords: {γ-TiAl alloy;composites;grain;hot-workability} |