Synthesis and Properties of α-1,3-Glucan with Branched and Linear Mixed Ester Side Chains AITranslate

The University of Tokyo; Kyung Hee University; The University of Tokyo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two series of α-1,3-glucan with branched and linear mixed ester side chains, namely α-1,3-glucan pivalate hexanoate (α-1,3-glucan-Pi-Hex) and α-1,3-glucan isobutyrate hexanoate (α-1,3-glucan-iBu-Hex), were synthesized as biomass-based thermoplastic resins via an enzymatic polymerization and a heterogeneous chemical esterification using trifluoroacetic acid anhydride and carboxylic acids. The degree of substitution (DS) ratio of two types of ester groups was precisely controlled by adjusting the initial dosages of the two corresponding carboxylic acids. Although α-1,3-glucan homobranched esters, i.e., α-1,3-glucan pivalate and α-1,3-glucan isobutyrate, were crystalline and their cast films were brittle, the cast films of the mixed esters gradually lost crystallinity and finally became amorphous in proportion to increasing DS of hexanoate (DSHex), and their flexibility improved significantly. Specifically, α-1,3-glucan-Pi-Hex and α-1,3-glucan-iBu-Hex with DSHex = 1.5 had high film flexibilities and high glass-transition temperatures of 120 and 93 °C, respectively. These are comparable to the properties of conventional oil-based amorphous plastics such as polystyrene and poly(methyl methacrylate). The processing window widened with increasing DSHex, which led to less thermal decomposition during thermal processing. The mixed ester method was effective for controlling the physical properties of α-1,3-glucan esters. Furthermore, α-1,3-glucan-Pi-Hex and α-1,3-glucan-iBu-Hex showed promise as transparent and flexible films with high thermal stability for electric devices of designability.

KeyWords AITranslate

α1 3glucan branched and linear mixed ester biomass plastic polysaccharide thermal property mechanical property
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01180

Chinese Library Classification Number:

Citation Information:

Two series of α-1,3-glucan with branched and linear mixed ester side chains, namely α-1,3-glucan pivalate hexanoate (α-1,3-glucan-Pi-Hex) and α-1,3-glucan isobutyrate hexanoate (α-1,3-glucan-iBu-Hex), were synthesized as biomass-based thermoplastic resins via an enzymatic polymerization and a heterogeneous chemical esterification using trifluoroacetic acid anhydride and carboxylic acids. The degree of substitution (DS) ratio of two types of ester groups was precisely controlled by adjusting the initial dosages of the two corresponding carboxylic acids. Although α-1,3-glucan homobranched esters, i.e., α-1,3-glucan pivalate and α-1,3-glucan isobutyrate, were crystalline and their cast films were brittle, the cast films of the mixed esters gradually lost crystallinity and finally became amorphous in proportion to increasing DS of hexanoate (DSHex), and their flexibility improved significantly. Specifically, α-1,3-glucan-Pi-Hex and α-1,3-glucan-iBu-Hex with DSHex = 1.5 had high film flexibilities and high glass-transition temperatures of 120 and 93 °C, respectively. These are comparable to the properties of conventional oil-based amorphous plastics such as polystyrene and poly(methyl methacrylate). The processing window widened with increasing DSHex, which led to less thermal decomposition during thermal processing. The mixed ester method was effective for controlling the physical properties of α-1,3-glucan esters. Furthermore, α-1,3-glucan-Pi-Hex and α-1,3-glucan-iBu-Hex showed promise as transparent and flexible films with high thermal stability for electric devices of designability.

quote

GB/T 7714-2015 [1] Yuya Fukata, Satoshi Kimura, Tadahisa Iwata. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01180.
MLA [1] Yuya Fukata, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01180.
APA [1] Yuya Fukata, Satoshi Kimura, & Tadahisa Iwata. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01180
IEEE [1] Yuya Fukata, Satoshi Kimura, and Tadahisa Iwata, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01180. keywords: {α1;3glucan;branched and linear mixed ester;biomass plastic;polysaccharide;thermal property;mechanical property}