Interfacial Self-Assembly of Silk Fibroin Polypeptides and α-NiCo(OH)2 Nanocrystals with Tunable Energy Storage Applications Interfacial Self-Assembly of Silk Fibroin Polypeptides and α-NiCo(OH)2 Nanocrystals with Tunable Energy Storage Applications AITranslate
Abstract AITranslate
There is an increasing interest in the self-assembly process from a bottom-up approach to synthesize functional structures for engineering applications. Silk fibroin is a protein extracted from the cocoons of silkworm Bombyx mori that can be processed into various materials generally stabilized by the induction of β-sheet formation through the use of solvents or by physical stretching. In our study, the introduction of cobalt-substituted nickel hydroxide nanoparticles on silk fibroin presented a dual effect causing the stabilization of the α polymorph of nickel hydroxide and promoting a highly connected network of the β-sheet crystalline domain in the fibroin chains. Electrochemical measurements were performed to examine silk fibroin (SF)/NiCo(OH)2 hybrid materials. The optimized sample exhibits a high specific capacity of 362 mA h g–1 at a current density of 1 A g–1, maintaining steady electrochemical performance >75% of the initial value at higher current densities. The presented assembly provides a route for preparing monodisperse inorganic nanoparticles in the presence of SF as an organic matrix with potential energy storage properties.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c01278
Chinese Library Classification Number:
Citation Information:
There is an increasing interest in the self-assembly process from a bottom-up approach to synthesize functional structures for engineering applications. Silk fibroin is a protein extracted from the cocoons of silkworm Bombyx mori that can be processed into various materials generally stabilized by the induction of β-sheet formation through the use of solvents or by physical stretching. In our study, the introduction of cobalt-substituted nickel hydroxide nanoparticles on silk fibroin presented a dual effect causing the stabilization of the α polymorph of nickel hydroxide and promoting a highly connected network of the β-sheet crystalline domain in the fibroin chains. Electrochemical measurements were performed to examine silk fibroin (SF)/NiCo(OH)2 hybrid materials. The optimized sample exhibits a high specific capacity of 362 mA h g–1 at a current density of 1 A g–1, maintaining steady electrochemical performance >75% of the initial value at higher current densities. The presented assembly provides a route for preparing monodisperse inorganic nanoparticles in the presence of SF as an organic matrix with potential energy storage properties.
quote
| GB/T 7714-2015 | [1] Eduardo R. do Nascimento, Barbara B. Gerbelli, Fabio F. Ferreira, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01278. |
| MLA | [1] Eduardo R. do Nascimento, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01278. |
| APA | [1] Eduardo R. do Nascimento, Barbara B. Gerbelli, Fabio F. Ferreira, Fanny N. Costa, Philip A. Chater, & Wendel A. Alves. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01278 |
| IEEE | [1] Eduardo R. do Nascimento, Barbara B. Gerbelli, Fabio F. Ferreira, Fanny N. Costa, Philip A. Chater, and Wendel A. Alves, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01278. keywords: {silk fibroin nickel hydroxide pair function distribution βsheet crystallinity energy storage} |