Additive manufacturing of isotropic-grained, high-strength and high-ductility copper alloys AITranslate
Abstract AITranslate
This work reports additive manufacturing of nickel-aluminum-bronze alloys by electron beam powder bed fusion (EB-PBF), with a relatively homogeneous microstructure at the micro- to meso-scale and exhibiting an exceptional combination of tensile strength and ductility — well surpassing that of conventionally wrought counterparts. The attainment of both high yield and ultimate tensile strength are attributed to collective effects of uniformly distributed precipitates, near-equi-axed grains, and a high fraction of high-angle grain boundaries. High tensile ductility originates from a sustainable work-hardening ability via dislocation-dislocation and dislocation-precipitate interactions, enhanced by moderate twinning, stacking faults, and back-stress hardening. Significantly, the EB-PBF alloys exhibit near-isotropic tensile properties in directions parallel and vertical to the build direction due to high-density precipitates enabled by equi-axed grains.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.addma.2020.101751
Chinese Library Classification Number:
Citation Information:
This work reports additive manufacturing of nickel-aluminum-bronze alloys by electron beam powder bed fusion (EB-PBF), with a relatively homogeneous microstructure at the micro- to meso-scale and exhibiting an exceptional combination of tensile strength and ductility — well surpassing that of conventionally wrought counterparts. The attainment of both high yield and ultimate tensile strength are attributed to collective effects of uniformly distributed precipitates, near-equi-axed grains, and a high fraction of high-angle grain boundaries. High tensile ductility originates from a sustainable work-hardening ability via dislocation-dislocation and dislocation-precipitate interactions, enhanced by moderate twinning, stacking faults, and back-stress hardening. Significantly, the EB-PBF alloys exhibit near-isotropic tensile properties in directions parallel and vertical to the build direction due to high-density precipitates enabled by equi-axed grains.
quote
| GB/T 7714-2015 | [1] Wenlong Lu, Wenzheng Zhai, Jian Wang, et al. Additive Manufacturing, 2021(38). DOI:10.1016/j.addma.2020.101751. |
| MLA | [1] Wenlong Lu, et al., Additive Manufacturing, no. 38, 2021, https://doi.org/10.1016/j.addma.2020.101751. |
| APA | [1] Wenlong Lu, Wenzheng Zhai, Jian Wang, Xiaojun Liu, Liping Zhou, Ahmed Mohamed Mahmoud Ibrahim, Xiaochun Li, Dong Lin, & Y. Morris Wang. (2021). Additive Manufacturing(38). https://doi.org/10.1016/j.addma.2020.101751 |
| IEEE | [1] Wenlong Lu, Wenzheng Zhai, Jian Wang, Xiaojun Liu, Liping Zhou, Ahmed Mohamed Mahmoud Ibrahim, Xiaochun Li, Dong Lin, and Y. Morris Wang, Additive Manufacturing, no. 38, 2021, doi: 10.1016/j.addma.2020.101751. |