Microfluidic Channels Fabrication Based on Underwater Superpolymphobic Microgrooves Produced by Femtosecond Laser Direct Writing AITranslate

Xi’an Jiaotong University; University of Rochester; University of Rochester; Xi’an Jiaotong University; University of Rochester
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A strategy is proposed here to fabricate microfluidic channels based on underwater superpolymphobic microgrooves with nanoscale rough surface structure on glass surface produced by femtosecond (fs) laser processing. The fs laser-induced micro/nanostructure on glass surface can repel liquid polydimethylsiloxane (PDMS) underwater, with the contact angle (CA) of 155.5 ± 2.5° and CA hysteresis of 2.7 ± 1.5° to a liquid PDMS droplet. Such a phenomenon is defined as the underwater “superpolymphobicity”. Microchannels as well as microfluidic systems are easily prepared and formed between the underwater superpolymphobic microgroove-textured glass substrate and the cured PDMS layer. Because the tracks of the laser scanning lines are programmable, arbitrary-shaped microchannels and complex microfluidic systems can be potentially designed and prepared through fs laser direct writing technology. The concept of “underwater superpolymphobicity” presented here offers us a new strategy for selectively avoiding the adhesion at the polymer/substrate interface and controlling the shape of cured polymers; none of these applications can find analogues in previously reported superwetting materials.

KeyWords AITranslate

underwater superpolymphobicity microfluidic channels microfluidic systems femtosecond laser PDMS
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00269

Chinese Library Classification Number:

Citation Information:

A strategy is proposed here to fabricate microfluidic channels based on underwater superpolymphobic microgrooves with nanoscale rough surface structure on glass surface produced by femtosecond (fs) laser processing. The fs laser-induced micro/nanostructure on glass surface can repel liquid polydimethylsiloxane (PDMS) underwater, with the contact angle (CA) of 155.5 ± 2.5° and CA hysteresis of 2.7 ± 1.5° to a liquid PDMS droplet. Such a phenomenon is defined as the underwater “superpolymphobicity”. Microchannels as well as microfluidic systems are easily prepared and formed between the underwater superpolymphobic microgroove-textured glass substrate and the cured PDMS layer. Because the tracks of the laser scanning lines are programmable, arbitrary-shaped microchannels and complex microfluidic systems can be potentially designed and prepared through fs laser direct writing technology. The concept of “underwater superpolymphobicity” presented here offers us a new strategy for selectively avoiding the adhesion at the polymer/substrate interface and controlling the shape of cured polymers; none of these applications can find analogues in previously reported superwetting materials.

quote

GB/T 7714-2015 [1] Jiale Yong, Zhibing Zhan, Subhash C. Singh, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00269.
MLA [1] Jiale Yong, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00269.
APA [1] Jiale Yong, Zhibing Zhan, Subhash C. Singh, Feng Chen, & Chunlei Guo. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00269