Experimental Study on Improvement of Tellurium Leaching Rate from the Pb-Te Slag AITranslate

Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on the character and composition of lead-tellurium slag, the two-stage leaching process was applied of alkaline leaching-washing-acid leaching. Influences of alkali concentration, leaching temperature, leaching time and liquid to solid ratio were investigated on the leaching rate of lead-tellurium slag. The re-sults show that the optimum alkaline leaching conditions are sodium hydroxide concentration of 100 g/L, leaching temperature of 90 ℃ ,leaching time of 4 h and liquid to solid ration of 10 : 1. Under the above con-ditions, tellurium leaching rate is 88.80 %. The optimum acid leaching conditions are as follows:hydrochlo-ric acid concentration of 2.5 mol/L,leaching temperature of 75 ℃ ,leaching time of 4 h,and liquid to solid ratio of 5 : 1 ,and the total tellurium leaching rate is 98.9%.

KeyWords AITranslate

lead-tellurium slag sodium hydroxide hydrochloric acid tellurium leaching

1谢明辉,王兴明,陈后兴,罗仙平.碲的资源、用途与提取分离技术研究现状[J].四川有色金属,2005(1):5-8. 被引量:51

2聂保生.对从除碲渣中回收碲的工艺改进[J].稀有金属与硬质合金,1997,25(2):15-17. 被引量:4

3王清宏,陈平,黄淑芳.从低品位原料中提取碲的工艺[J].上海有色金属,2008,29(3):123-126. 被引量:9

4何从行.碲渣综合回收工艺研究[J].有色冶炼,2001,30(1):41-42. 被引量:12

5陈芳兰,车文婷.从铋碲矿中回收碲[J].稀有金属与硬质合金,1995,23(2):4-7. 被引量:5

6王英,陈少纯,顾珩,叶富兴.从铜阳极泥回收碲的工艺研究[J].材料研究与应用,2009,3(2):131-133. 被引量:17

1徐卫东,胡欣雷,汪维.冶锌工业铜镉渣的综合回收与利用研究[J].冶金管理,2021(23):153-154.

2钱俊杰,杨易,俞鹰,方支灵,潘荣选,申其新.粗碲化铜碱浸工艺实验研究[J].广州化工,2018,46(2):66-68. 被引量:4

3薛超群,郭敏,张婵.超声提取-三氯化钛还原-原子荧光光谱法对土壤样品中不同价态碲的测定[J].中国测试,2018,44(4):53-56. 被引量:2

4宋旭俊,施辉献.浮选渣中碲的浸出研究[J].有色金属设计,2022,49(2):18-22.

5雷晓明.碲化铜渣快速处理生产二氧化碲的工艺研究[J].中国资源综合利用,2023,41(3):29-34.

1杨世莹,范兴祥,徐刚芳,李英伟.碲化铜渣的硫酸化焙烧—碱浸碲试验研究[J].湿法冶金,2019,38(3):177-181. 被引量:2

2徐小娟.氢化物发生-原子荧光光谱法在化探样品测试中的应用进展[J].安徽化工,2020,46(2):12-16. 被引量:3

3范兴祥,李英伟,杨坤彬,王家和.冶炼碱性渣制备高纯碲联产粗硒试验[J].有色金属:冶炼部分,2020(8):72-77. 被引量:1

4曾颜亮,彭珊,廖春发,刘付朋.水浸分铜渣超声波外场强化碱浸分碲动力学研究[J].稀有金属与硬质合金,2023,51(3):30-36. 被引量:1

5鲁海妍,谢海东,胡兰基,孔晓彦,刘玉川.湿法消解-电感耦合等离子体质谱法测定多金属矿中碲[J].桂林理工大学学报,2023,43(2):211-217.

6王冲,范兴祥,罗劲松,李英伟,徐刚芳,杨世莹.氧化焙烧碲化铜渣——碱浸碲试验[J].有色金属:冶炼部分,2019(3):40-43. 被引量:4

1赵宏,洪艳霞.回收铁矾渣中铟的试验研究[J].甘肃冶金,2014,36(5):30-31. 被引量:3

2徐永新,杨欢.石煤提钒的最佳焙烧酸浸条件[J].有色金属,2008,60(3):74-76. 被引量:7

3吕国志,张廷安,赵爱春,王红星.酸浸及萃取对高铁铝土矿中有价元素分离特性的影响[J].东北大学学报:自然科学版,2013,34(10):1442-1445. 被引量:5

4刘俊峰.酸浸条件对炼铜烟灰铁浸出的影响[J].湿法冶金,1999(1):56-58. 被引量:1

5库建刚,王安理,乔翠杰,张文彬.氯离子对硫化铜精矿浸出的影响[J].湿法冶金,2008,27(2):113-116. 被引量:5

6佟志芳,邹燕飞,李英杰.从粉煤灰提取铝铁新工艺研究[J].轻金属,2009(1):13-16. 被引量:13

7汪平,冯雅丽,李浩然,张萍,刘欣伟.采用氧化焙烧-酸浸法从高碳石煤中提钒试验研究[J].中南大学学报:自然科学版,2011,42(10):2917-2921. 被引量:10

8刘俊峰,易平贵,陈安国.炼铜烟灰生产硫酸锌酸浸条件对锌浸出率的影响[J].无机盐工业,2000,32(1):38-39.

9刘志宏,张登凯,李玉虎,李启厚,艾侃.海绵铁中提取镓的研究[J].有色金属:冶炼部分,2005(3):33-35. 被引量:1

10张培育,郭强,宋云霞,曲景奎,齐涛.从红土镍矿镍铁渣中分离浸取镍铬工艺[J].过程工程学报,2013,13(4):608-614. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TF111.31[冶金工程—冶金物理化学]

Citation Information:

Based on the character and composition of lead-tellurium slag, the two-stage leaching process was applied of alkaline leaching-washing-acid leaching. Influences of alkali concentration, leaching temperature, leaching time and liquid to solid ratio were investigated on the leaching rate of lead-tellurium slag. The re-sults show that the optimum alkaline leaching conditions are sodium hydroxide concentration of 100 g/L, leaching temperature of 90 ℃ ,leaching time of 4 h and liquid to solid ration of 10 : 1. Under the above con-ditions, tellurium leaching rate is 88.80 %. The optimum acid leaching conditions are as follows:hydrochlo-ric acid concentration of 2.5 mol/L,leaching temperature of 75 ℃ ,leaching time of 4 h,and liquid to solid ratio of 5 : 1 ,and the total tellurium leaching rate is 98.9%.

quote

GB/T 7714-2015 [1] BAO Xin-jun, LIU Ji-bo, SU Zheng-fu, et al. Experimental Study on Improvement of Tellurium Leaching Rate from the Pb-Te Slag[J]. Rare Metals and Cemented Carbides, 2013(2): 10-12.
MLA [1] BAO Xin-jun, et al., "Experimental Study on Improvement of Tellurium Leaching Rate from the Pb-Te Slag." Rare Metals and Cemented Carbides, no. 2, 2013, pp. 10-12.
APA [1] BAO Xin-jun, LIU Ji-bo, SU Zheng-fu, DENG Zhi-jun, HUANG Shi, & QIAN Dong. (2013). Experimental Study on Improvement of Tellurium Leaching Rate from the Pb-Te Slag. Rare Metals and Cemented Carbides(2), 10-12.
IEEE [1] BAO Xin-jun, LIU Ji-bo, SU Zheng-fu, DENG Zhi-jun, HUANG Shi, and QIAN Dong, "Experimental Study on Improvement of Tellurium Leaching Rate from the Pb-Te Slag," Rare Metals and Cemented Carbides, no. 2, pp. 10-12, 2013. keywords: {lead-tellurium slag;sodium hydroxide;hydrochloric acid;tellurium;leaching}