daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Phenothiazine-Based 2D Covalent Organic Framework for Efficient Visible-Light-Induced Free Radical Polymerization AITranslate

Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Jilin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Phenothiazine derivatives have attracted tremendous research attention due to their rich redox-active properties. In this work, a phenothiazine-based, highly crystalline, and two-dimensional covalent organic framework (PTz-An-COF) was developed. PTz-An-COF exhibited a low bandgap of 1.92 eV with a broad visible-light absorption. Interestingly, PTz-An-COF can serve as an efficient photoinitiator for visible-light-induced radical polymerization of methyl acrylate. Remarkably, PTz-An-COF as a photoinitiator can be easily recycled and maintains the same catalytic activity as that of pristine PTz-An-COF. This work provides new insights into the development of high-performance heterogeneous photocatalysts for radical polymerization.

KeyWords AITranslate

covalent organic frameworks crystalline porous materials photoinitiator radical polymerization heterogeneous photocatalyst
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02051

Chinese Library Classification Number:

Citation Information:

Phenothiazine derivatives have attracted tremendous research attention due to their rich redox-active properties. In this work, a phenothiazine-based, highly crystalline, and two-dimensional covalent organic framework (PTz-An-COF) was developed. PTz-An-COF exhibited a low bandgap of 1.92 eV with a broad visible-light absorption. Interestingly, PTz-An-COF can serve as an efficient photoinitiator for visible-light-induced radical polymerization of methyl acrylate. Remarkably, PTz-An-COF as a photoinitiator can be easily recycled and maintains the same catalytic activity as that of pristine PTz-An-COF. This work provides new insights into the development of high-performance heterogeneous photocatalysts for radical polymerization.

quote

GB/T 7714-2015 [1] Ziqiang Zhao, Junyu Ren, Yuan Yuan, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02051.
MLA [1] Ziqiang Zhao, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02051.
APA [1] Ziqiang Zhao, Junyu Ren, Yuan Yuan, Zeying Sun, Weiben Chen, Xi Su, Guang Zhang, & Long Chen. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02051
IEEE [1] Ziqiang Zhao, Junyu Ren, Yuan Yuan, Zeying Sun, Weiben Chen, Xi Su, Guang Zhang, and Long Chen, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02051. keywords: {covalent organic frameworks;crystalline porous materials;photoinitiator;radical polymerization;heterogeneous photocatalyst}