daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Three-Dimensional Printing with Waste High-Density Polyethylene AITranslate

CSIR-National Chemical Laboratory; CSIR-National Chemical Laboratory;ANSYS Software India Pvt. Ltd.;ANSYS Software India Pvt. Ltd.; CSIR-National Chemical Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Fused filament fabrication (FFF) three-dimensional (3D) printing of semicrystalline polymers such as high-density polyethylene (HDPE) is challenging because crystallization-induced shrinkage of the filament, as it cools, results in stresses that warp the printed part and debond it from the print substrate. Here, we demonstrate that waste-derived HDPE can be successfully 3D printed by (i) blending with a small fraction (<0.5% by weight) of dimethyl dibenzylidene sorbitol (DMDBS) and (∼10%) linear low density polyethylene (LLDPE) and (ii) printing the object with a thin “brim” around it that is adhered to the print substrate using common polyvinyl acetate-based glue. We match our experimental results with FEM simulations that provide insight into the origin of the stresses developed during printing. Because HDPE forms a significant fraction of the plastic waste stream, conversion of waste-derived HDPE to 3D printing filament has important technological implications.

KeyWords AITranslate

3d printing polyethylene printing recyclability warpage polymer blend
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00813

Chinese Library Classification Number:

Citation Information:

Fused filament fabrication (FFF) three-dimensional (3D) printing of semicrystalline polymers such as high-density polyethylene (HDPE) is challenging because crystallization-induced shrinkage of the filament, as it cools, results in stresses that warp the printed part and debond it from the print substrate. Here, we demonstrate that waste-derived HDPE can be successfully 3D printed by (i) blending with a small fraction (<0.5% by weight) of dimethyl dibenzylidene sorbitol (DMDBS) and (∼10%) linear low density polyethylene (LLDPE) and (ii) printing the object with a thin “brim” around it that is adhered to the print substrate using common polyvinyl acetate-based glue. We match our experimental results with FEM simulations that provide insight into the origin of the stresses developed during printing. Because HDPE forms a significant fraction of the plastic waste stream, conversion of waste-derived HDPE to 3D printing filament has important technological implications.

quote

GB/T 7714-2015 [1] Aniket Gudadhe, Nirmalya Bachhar, Anil Kumar, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00813.
MLA [1] Aniket Gudadhe, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00813.
APA [1] Aniket Gudadhe, Nirmalya Bachhar, Anil Kumar, Prem Andrade, & Guruswamy Kumaraswamy. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00813