Self-Healing Luminescent Elastomers with Ultrahigh Mechanical Strength, Superior Toughness, and Stimuli-Responsive Luminescence AITranslate
Abstract AITranslate
It remains an inherent challenge to simultaneously endow the self-healing materials with robust mechanical properties and extra functions, such as luminescence. Herein, a series of ultrastrong and tough elastomers were synthesized by simultaneously introducing multiple hydrogen bonds and polydentate chelating lanthanide-terpyridine (Ln3+-Tpy) coordination interactions into polymer chains. The optimal materials (noted as HMPU-Tpy0.1-Ln) show a record-high tensile strength of 40.9 MPa and a superior toughness of 308.63 MJ m–3 with a large extensibility of 2067%. In particular, the true fracture stress (0.91 GPa) of the HMPU-Tpy0.1-Ln polymer is comparable to that of typical spider silk (0.80–1.50 GPa) and its toughness is about 1.9 times that of typical spider silk (≈160 MJ m–3). The dynamic nature of the multiple hydrogen bonds and Ln3+-Tpy coordination also endow the material with acceptable self-healing performance, which can be improved by heating. Superior luminescence performance of the characteristic emission of the corresponding Ln3+ ions can be observed under the excitation of UV light. Besides, the break/recovery of energy transfer between Ln3+ and polymer–ligands triggered by acid–base gas endows HMPU-Tpy0.1-Ln with luminescence off/on switching behavior. We believe that the adopted approach in this work paves the way to prepare ultrastrong self-healing luminescent materials with stimulus-response performance.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01837
Chinese Library Classification Number:
Citation Information:
It remains an inherent challenge to simultaneously endow the self-healing materials with robust mechanical properties and extra functions, such as luminescence. Herein, a series of ultrastrong and tough elastomers were synthesized by simultaneously introducing multiple hydrogen bonds and polydentate chelating lanthanide-terpyridine (Ln3+-Tpy) coordination interactions into polymer chains. The optimal materials (noted as HMPU-Tpy0.1-Ln) show a record-high tensile strength of 40.9 MPa and a superior toughness of 308.63 MJ m–3 with a large extensibility of 2067%. In particular, the true fracture stress (0.91 GPa) of the HMPU-Tpy0.1-Ln polymer is comparable to that of typical spider silk (0.80–1.50 GPa) and its toughness is about 1.9 times that of typical spider silk (≈160 MJ m–3). The dynamic nature of the multiple hydrogen bonds and Ln3+-Tpy coordination also endow the material with acceptable self-healing performance, which can be improved by heating. Superior luminescence performance of the characteristic emission of the corresponding Ln3+ ions can be observed under the excitation of UV light. Besides, the break/recovery of energy transfer between Ln3+ and polymer–ligands triggered by acid–base gas endows HMPU-Tpy0.1-Ln with luminescence off/on switching behavior. We believe that the adopted approach in this work paves the way to prepare ultrastrong self-healing luminescent materials with stimulus-response performance.
quote
| GB/T 7714-2015 | [1] Di Zhao, Chunmei Yue, Qianrui Li, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01837. |
| MLA | [1] Di Zhao, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01837. |
| APA | [1] Di Zhao, Chunmei Yue, Qianrui Li, Lei Guo, Jing Yang, & Huanrong Li. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01837 |
| IEEE | [1] Di Zhao, Chunmei Yue, Qianrui Li, Lei Guo, Jing Yang, and Huanrong Li, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01837. keywords: {luminescence;superior toughness;ultrahigh strength;selfhealing;stimulus response;multicolor emission} |