Interpenetrating lattices with enhanced mechanical functionality AITranslate

Materials;Materials;Materials;Materials
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metamaterials derive their unusual properties from their architected structure, which generally consists of a repeating unit cell designed to perform a particular function. However, existing metamaterials are, with few exceptions, physically continuous throughout their volume, and thus cannot take advantage of multi-body behavior or contact interactions. Here we introduce the concept of multi-body interpenetrating lattices, where two or more lattices interlace through the same volume without any direct connection to each other. This new design freedom allows us to create architected interpenetrating structures where energy transfer is controlled by surface interactions. As a result, multifunctional or composite-like responses can be achieved even with only a single print material. While the geometry defining interpenetrating lattices has been studied since the days of Euclid, additive manufacturing allows us to turn these mathematical concepts into physical objects with programmable interface-dominated properties. In this first study on interpenetrating lattices, we reveal remarkable mechanical properties including improved toughness, multi-stable/negative stiffness behavior, and electromechanical coupling.

KeyWords AITranslate

Metamaterial Interface engineering lattice Polyhedra Geometry Additive manufacturing
No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2020.101741

Chinese Library Classification Number:

Citation Information:

Metamaterials derive their unusual properties from their architected structure, which generally consists of a repeating unit cell designed to perform a particular function. However, existing metamaterials are, with few exceptions, physically continuous throughout their volume, and thus cannot take advantage of multi-body behavior or contact interactions. Here we introduce the concept of multi-body interpenetrating lattices, where two or more lattices interlace through the same volume without any direct connection to each other. This new design freedom allows us to create architected interpenetrating structures where energy transfer is controlled by surface interactions. As a result, multifunctional or composite-like responses can be achieved even with only a single print material. While the geometry defining interpenetrating lattices has been studied since the days of Euclid, additive manufacturing allows us to turn these mathematical concepts into physical objects with programmable interface-dominated properties. In this first study on interpenetrating lattices, we reveal remarkable mechanical properties including improved toughness, multi-stable/negative stiffness behavior, and electromechanical coupling.

quote

GB/T 7714-2015 [1] Benjamin C. White, Anthony Garland, Ryan Alberdi, et al. Additive Manufacturing, 2021(38). DOI:10.1016/j.addma.2020.101741.
MLA [1] Benjamin C. White, et al., Additive Manufacturing, no. 38, 2021, https://doi.org/10.1016/j.addma.2020.101741.
APA [1] Benjamin C. White, Anthony Garland, Ryan Alberdi, & Brad L. Boyce. (2021). Additive Manufacturing(38). https://doi.org/10.1016/j.addma.2020.101741
IEEE [1] Benjamin C. White, Anthony Garland, Ryan Alberdi, and Brad L. Boyce, Additive Manufacturing, no. 38, 2021, doi: 10.1016/j.addma.2020.101741. keywords: {Metamaterial;Interface engineering;lattice;Polyhedra;Geometry;Additive manufacturing}