西藏谷露含铯硅华提铯及硅的综合利用研究 AITranslate

Zhengzhou Mineral Comprehensive Utilization Research Institute of the Ministry of Geology and Mineral Resources;Zhengzhou Mineral Comprehensive Utilization Research Institute of the Ministry of Geology and Mineral Resources;Zhengzhou Mineral Comprehensive Utilization Research Institute of the Ministry of Geology and Mineral Resources;Zhengzhou Mineral Comprehensive Utilization Research Institute of the Ministry of Geology and Mineral Resources;Zhengzhou Mineral Comprehensive Utilization Research Institute of the Ministry of Geology and Mineral Resources;Zhengzhou Mineral Comprehensive Utilization Research Institute of the Ministry of Geology and Mineral Resources
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

本文介绍了从新型铯资源——西藏谷露含铯硅华提铯及硅渣制白炭黑的试验研究结果。

KeyWords AITranslate

含铯硅华 综合利用

1金栋.白炭黑的生产及表面改性技术进展[J].无机盐技术,2009(2):1-8.

2宓岚.E70C—6M H4焊丝对硅渣的利用[J].金属加工:热加工,2008(12):58-59.

3谭伟,钟俊林,熊文杰.西藏角笼坝大桥焊接H型钢的组合焊接工艺[J].金属加工:热加工,2009(2):42-44.

4金属纳米材料开发前景广阔[J].广东涂料与胶粘剂,2004(1):21-21.

5郑丽华,刘钦甫,程宏飞.白炭黑表面改性研究现状[J].无机硅化合物(天津),2008(4):16-21. 被引量:6

6涂春根.“第2届钽铌产品暨原料市场研讨会”在西藏举行[J].稀有金属快报,2004(9):41-41.

7李玉芳.橡胶填充剂白炭黑的生产及改性技术进展[J].精细化工原料及中间体,2009(6):22-25.

8王小宝.神秘的西藏 潜行的焊接[J].现代焊接,2014,0(11):20-21.

9唐家举.西藏印象[J].城乡建设,2006(7):71-74.

10澹凡忠,姜军生.高速钢钻头磨屑回收及综合利用研究[J].新技术新工艺,2000(5):20-21. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TF84[冶金工程—有色金属冶金];TG135.5[一般工业技术—材料科学与工程]

Citation Information:

本文介绍了从新型铯资源——西藏谷露含铯硅华提铯及硅渣制白炭黑的试验研究结果。

quote

GB/T 7714-2015 [1] WANG Qiu-xia, WANG Qi, ZHANG Da-wei, et al. Rare Metals and Cemented Carbides, 1993(1): 237-241.
MLA [1] WANG Qiu-xia, et al., Rare Metals and Cemented Carbides, no. 1, 1993, pp. 237-241.
APA [1] WANG Qiu-xia, WANG Qi, ZHANG Da-wei, YANG Shao-wen, ZHANG Su-chun, & YANG Hui. (1993). Rare Metals and Cemented Carbides(1), 237-241.
IEEE [1] WANG Qiu-xia, WANG Qi, ZHANG Da-wei, YANG Shao-wen, ZHANG Su-chun, and YANG Hui, Rare Metals and Cemented Carbides, no. 1, pp. 237-241, 1993.