Amphiphobic, Thermostable, and Stretchable PTFE Nanofibrous Membranes with Breathable and Chemical-Resistant Performances for Protective Applications AITranslate

Donghua University; Donghua University; Donghua University; Donghua University; Donghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Waterproof and breathable membranes (WBM) have diverse applications in outdoor apparel, wearable electronics, and medical hygiene because they can withstand liquid water penetration while simultaneously transmitting water vapor. Nevertheless, developing potential nontoxic WBM based on ecologically friendly solvents remains a significant issue. Therefore, we prepared polytetrafluoroethylene (PTFE) waterproof and permeable membranes (PWBM) with a remarkable moisture transfer rate of 11.9 kg m–2 d–1, a high hydrostatic pressure of 81.5 kPa, and an astonishing tensile strain of 554%, so the produced PWBM demonstrates great capabilities. Besides, the obtained PWBM also has outstanding chemical resistance and appealing superhydrophobicity. The development of the subsequent generation of environmentally friendly WBM for protective garments may be therefore beneficial to the successful fabrication of such green smart fibrous membranes.

KeyWords AITranslate

PTFE electrospinning green solvents amphiphobic chemicalresistant breathable stretchable
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01964

Chinese Library Classification Number:

Citation Information:

Waterproof and breathable membranes (WBM) have diverse applications in outdoor apparel, wearable electronics, and medical hygiene because they can withstand liquid water penetration while simultaneously transmitting water vapor. Nevertheless, developing potential nontoxic WBM based on ecologically friendly solvents remains a significant issue. Therefore, we prepared polytetrafluoroethylene (PTFE) waterproof and permeable membranes (PWBM) with a remarkable moisture transfer rate of 11.9 kg m–2 d–1, a high hydrostatic pressure of 81.5 kPa, and an astonishing tensile strain of 554%, so the produced PWBM demonstrates great capabilities. Besides, the obtained PWBM also has outstanding chemical resistance and appealing superhydrophobicity. The development of the subsequent generation of environmentally friendly WBM for protective garments may be therefore beneficial to the successful fabrication of such green smart fibrous membranes.

quote

GB/T 7714-2015 [1] Shuangyan Liu, Li Xu, Jianyong Yu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01964.
MLA [1] Shuangyan Liu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01964.
APA [1] Shuangyan Liu, Li Xu, Jianyong Yu, Yang Si, & Bin Ding. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01964
IEEE [1] Shuangyan Liu, Li Xu, Jianyong Yu, Yang Si, and Bin Ding, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01964. keywords: {PTFE electrospinning;green solvents;amphiphobic;chemicalresistant;breathable;stretchable}