Achieving Highly Conductive, Stretchable, and Washable Fabric from Reactive Silver Ink and Increased Interfacial Adhesion AITranslate

University of Pittsburgh; University of Pittsburgh; University of Pittsburgh;Electroninks Inc.; University of Pittsburgh; University of Pittsburgh
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

There is a major need to manufacture highly electrically conductive fabrics with stretch- and wash-durability. In this work, we provide both modeling and experiments of the mechanical failure of silver ink coatings on knitted fabric. Large thickness metal films are needed for high conductance but tend to debond from the underlying fabric microfibers that lead to cracking and failure. Strong adhesion between the metal film and microfiber is thus key to achieving high thickness films with good mechanical robustness. The use of a reactive silver ink addresses this need due to in situ silver reduction and conformal coverage. Furthermore, a chemical etchant pretreatment of the textile microfibers functionalizes the surface to enable covalent bonding with the surface and increases theinterface area. The use of a polymer provides for an additional protective barrier during washing. Treated fabrics demonstrate low sheet resistance <100 mΩ per square with only two coats and <200 mΩ per square after 1000 stretching cycles or 300 min of ultrasonic washing with detergent.

KeyWords AITranslate

conductive fabric etextile ink durability coating adhesion resistance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00768

Chinese Library Classification Number:

Citation Information:

There is a major need to manufacture highly electrically conductive fabrics with stretch- and wash-durability. In this work, we provide both modeling and experiments of the mechanical failure of silver ink coatings on knitted fabric. Large thickness metal films are needed for high conductance but tend to debond from the underlying fabric microfibers that lead to cracking and failure. Strong adhesion between the metal film and microfiber is thus key to achieving high thickness films with good mechanical robustness. The use of a reactive silver ink addresses this need due to in situ silver reduction and conformal coverage. Furthermore, a chemical etchant pretreatment of the textile microfibers functionalizes the surface to enable covalent bonding with the surface and increases theinterface area. The use of a polymer provides for an additional protective barrier during washing. Treated fabrics demonstrate low sheet resistance <100 mΩ per square with only two coats and <200 mΩ per square after 1000 stretching cycles or 300 min of ultrasonic washing with detergent.

quote

GB/T 7714-2015 [1] Anthony J. Galante, Brady C. Pilsbury, Mingxuan Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00768.
MLA [1] Anthony J. Galante, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00768.
APA [1] Anthony J. Galante, Brady C. Pilsbury, Mingxuan Li, Melbs LeMieux, Qihan Liu, & Paul W. Leu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00768
IEEE [1] Anthony J. Galante, Brady C. Pilsbury, Mingxuan Li, Melbs LeMieux, Qihan Liu, and Paul W. Leu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00768. keywords: {conductive;fabric;etextile;ink;durability;coating;adhesion;resistance}