Abstract AITranslate

Commercial-scale test is made on Ti slag smelting from Panzhihua Ti ore and Yunnan Ti ore with open-top electric furnace.The results showed that slag and iron are effectively separated and qualified Ti slag is obtained with Ti assaying respectively 79%, 82% and 74% from mixed ore,Yunnan Ti ore and Panzhihua Ti ore.Analysis is made of the feature and parameters of Ti slag smelting with open-top electric furnace.

KeyWords AITranslate

Ti ore smelting Ti slag commercial-scale test

1王铁明.制约我国钛渣生产和应用的原因及对策[J].钛工业进展,2002,19(1):10-12. 被引量:11

2汪镜亮.钛渣生产的发展[J].钛工业进展,2002,19(1):6-9. 被引量:17

1唐昭辉,彭金辉,张世敏,郭胜惠,张利波,李静.钛铁矿的还原技术研究现状[J].钛工业进展,2010,27(2):9-12. 被引量:7

2陈贤幕.全攀枝花钛精矿冶炼钛渣的生产实践[J].四川冶金,2014,36(1):31-33.

3顾静,夏德宏,齐照东,敖雯青.高温碳热还原条件下钛铁矿物相变化的实验研究[J].稀有金属与硬质合金,2017,45(5):17-21. 被引量:2

4Yongfeng Cai,Ningning Song,Yunfei Yang,Lingmin Sun,Peng Hu,Jinshu Wang.Recent progress of efficient utilization of titanium-bearing blast furnace slag[J].矿物冶金与材料学报:英文版,2022,29(1):22-31. 被引量:1

1谢刚,杨大锦.2010年云南冶金年评[J].云南冶金,2011,40(2):41-51.

2王玉明.钛铁矿碳热还原动力学[J].矿冶工程,2011,31(5):66-68. 被引量:8

3罗立群,闫昊天.含铁矿物的微波热处理技术现状[J].中国矿业,2012,21(8):104-109. 被引量:8

4董强,李军旗,徐本军,张莹.用废盐酸从钛铁精矿中浸出钛和铁的试验研究[J].湿法冶金,2013,32(1):38-40. 被引量:2

5李磊,朱红波,张利波,彭金辉,贾景岩,代林晴.微波碳热还原钛铁矿扩试研究[J].材料导报,2015,29(10):124-127. 被引量:5

6刘艺琴,王华,卿山,张爱敏,郈雅丽.富氧顶吹熔融还原全钛铁矿中杂质元素的行为研究[J].材料导报:纳米与新材料专辑,2016,30(2):396-400.

7徐宏达,张新,马艺闻.微波辐照预处理技术在难选铁矿石磨矿中的应用[J].现代矿业,2018,34(10):238-241. 被引量:2

8喻连香,汤优优,刘军,陈雄.含难分离赤铁矿的钛铁粗精矿选冶提质工艺研究[J].金属矿山,2020(5):185-190. 被引量:3

9尹国亮,李仕超,徐慎颖,张丹,金成国,张嫒馨.还原钛制备富钛料工艺现状及应用前景分析[J].铁合金,2022,53(3):34-37. 被引量:3

10黄先良,钟山,唐思扬,宋磊,李红娇,梁斌.盐酸法浸出水淬含钛高炉渣制备高纯金红石型二氧化钛[J].钢铁钒钛,2023,44(3):23-32.

1李雅儒.提高鞍钢酸性球团矿冶金性能的途径[J].烧结球团,1994,19(5):44-47. 被引量:2

2夏岩和.涞源钢铁厂高炉高MgO渣冶炼特性的研讨[J].北方工业大学学报,1989,1(1):20-28.

3蒋叶舟.广钢45t转炉四孔氧枪的设计及应用[J].冶金丛刊,2006(3):21-23. 被引量:1

4冯卫江,张育圣.敞口式硅铁炉电极漏糊事故处理方法的新尝试[J].铁合金,1990(3):24-24.

5佳贝.小方坯连铸机浸入式浇注技术的开发[J].钢铁,1993(3):83-83.

6赵改革,范晓慧,陈许玲,袁礼顺,甘敏.含铁炉料在高炉各区的冶炼特性[J].中南大学学报:自然科学版,2010,41(6):2053-2059. 被引量:14

7韩奕和,杨振南,王保林.65t敞口铁水罐加盖保温及效果[J].炼铁,1992,11(2):35-37. 被引量:2

8钟宇彤.一种敞口式埋弧矿热炉电极控制方法及系统[J].价值工程,2013,32(12):29-30.

9蒋仁全,史江涛,马跃庆,金怀德.提高高碳铬铁冶炼铬元素回收率的实践[J].铁合金,2004,35(4):10-13. 被引量:1

10Ц.,ГВ,李海天.斯达哈诺夫铁合金厂敞口铁合金炉废气热的利用[J].国外钢铁,1989(1):63-64.

Basic Information:

DOI:

Chinese Library Classification Number:TF823[冶金工程—有色金属冶金]

Citation Information:

Commercial-scale test is made on Ti slag smelting from Panzhihua Ti ore and Yunnan Ti ore with open-top electric furnace.The results showed that slag and iron are effectively separated and qualified Ti slag is obtained with Ti assaying respectively 79%, 82% and 74% from mixed ore,Yunnan Ti ore and Panzhihua Ti ore.Analysis is made of the feature and parameters of Ti slag smelting with open-top electric furnace.

quote

GB/T 7714-2015 [1] YU Wei. Commercial-scale Test on Ti Slag Smelting from Ti Concentrate[J]. Rare Metals and Cemented Carbides, 2004(4): 29-32.
MLA [1] YU Wei. "Commercial-scale Test on Ti Slag Smelting from Ti Concentrate." Rare Metals and Cemented Carbides, no. 4, 2004, pp. 29-32.
APA [1] YU Wei. (2004). Commercial-scale Test on Ti Slag Smelting from Ti Concentrate. Rare Metals and Cemented Carbides(4), 29-32.
IEEE [1] YU Wei, "Commercial-scale Test on Ti Slag Smelting from Ti Concentrate," Rare Metals and Cemented Carbides, no. 4, pp. 29-32, 2004. keywords: {Ti ore;smelting;Ti slag;commercial-scale test}