daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High temperature Sintering of Molybdenum Alloys Containing 3 wt% Rhenium AITranslate

Zhongnan University of Technology;Zhongnan University of Technology;Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High temperature sintering process of Mo 3% Re alloy by dry hydrogen and final vertical system was investigated. It was shown that the Mo 3% Re alloy by dry hydrogen sintering features finer grain sizes, higher tensile strength, elongation and microhardness values than the alloy by final vertical sintering.

KeyWords AITranslate

Low Re Mo alloy high temperature sintering grain structure mechanical property

1刘沙.-[J].稀有金属与硬质合金,1997,(4):26-26.

1刘仁智,安耿,杨秦莉,庄飞,王引婷,崔玉清,王娜,曹维成.钼-铼-镧合金微观组织及力学性能研究[J].粉末冶金技术,2018,0(6):429-432. 被引量:6

2谭拴斌,郭让民,杨升红,张廷杰.钼铼合金的结构和性能[J].稀有金属,2003,27(6):788-793. 被引量:25

3谭栓斌,张小明,任吉文,郭让民,张廷杰,李中奎.钼铼合金带材的组织和性能[J].稀有金属,2004,28(1):127-130. 被引量:3

1谭望,陈畅,汪明朴,郭明星,张真.不同因素对钼及钼合金塑脆性能影响的研究[J].材料导报,2007,21(8):80-83. 被引量:35

2张军良,李中奎,张小明,张清,周军,付洁,王东辉.制备方式对MORe合金组织性能的影响[J].稀有金属材料与工程,2007,36(A03):355-358. 被引量:6

3陈畅,汪明朴,谭望,郭明星,张娟.粉末冶金方法制备钼铼合金的研究[J].材料导报,2008,22(5):74-77. 被引量:12

4韩帅,赵锴,楼琅洪.一种含铼多晶铸造高温合金的凝固行为[J].材料研究学报,2009,23(1):98-102.

5张军良,李中奎,付洁,张清.MoRe_(41)合金冷轧过程的压缩模拟[J].稀有金属材料与工程,2008,37(A04):613-617.

6张军良,李中奎,付洁,夏明星,殷涛,刘辉.电子束悬浮熔炼钼铼合金铸锭的热加工方法[J].中国钼业,2010,34(5):38-40. 被引量:1

7刘辉,巨建辉,张军良,李中奎.钼铼合金铸锭热加工方式的研究[J].热加工工艺,2011,40(9):89-91. 被引量:2

8王健,余志明,吴晓斌,刘倩.沉积参数对Mo-Re合金基体上沉积金刚石薄膜的影响[J].中国有色金属学报,2011,21(6):1415-1421. 被引量:3

9任成,杨星团,李聪新,孙艳飞.高温气冷堆球床等效导热系数实验研究进展[J].科学技术与工程,2013,21(7):1905-1914. 被引量:5

10张盘龙,倪锋,赵晶晶,魏世忠.钼基掺杂合金的研究现状[J].硬质合金,2013,30(2):107-112. 被引量:10

1刘沙.粉末冶金法制取低铼钼合金的研究[J].稀有金属与硬质合金,1997,25(4):26-29.

2刘沙.低铼钼合金加工性能的研究[J].稀有金属与硬质合金,1998,26(1):33-36. 被引量:1

3刘沙,曹昱,舒金波.低铼钼合金力学性能的研究[J].稀有金属与硬质合金,1999,27(3):33-36. 被引量:4

4庞绍冬,庞绍熙.微型计算机在垂熔控制中的应用[J].微型机与应用,1989(2):28-30.

5陈荣.钼条垂熔电气控制[J].冶金自动化,1993,17(3):47-49.

6陈荣.单片机控制钼条垂熔[J].工业仪表与自动化装置,1994(3):44-48. 被引量:1

7徐志昌,张萍.液—固掺杂垂熔钨坯中改性元素的行为[J].粉末冶金技术,1992,10(4):243-247. 被引量:5

8彭金剑,崔千红.生产工艺对钼粉平均粒径及其加工性能的影响[J].中国钼业,1997,21(1):35-36. 被引量:8

9刘光耀.掺杂钨垂熔工艺的研究[J].钨钼材料,1996(3):9-12.

10刘载清.垂熔工序微机群控系统通过省级鉴定[J].有色设备,1992,0(1):60-60.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料];TF125.241[冶金工程—粉末冶金]

Citation Information:

High temperature sintering process of Mo 3% Re alloy by dry hydrogen and final vertical system was investigated. It was shown that the Mo 3% Re alloy by dry hydrogen sintering features finer grain sizes, higher tensile strength, elongation and microhardness values than the alloy by final vertical sintering.

quote

GB/T 7714-2015 [1] LIU Sha, CAO Yu, SHU Jin-bo. High temperature Sintering of Molybdenum Alloys Containing 3 wt% Rhenium[J]. Rare Metals and Cemented Carbides, 1999(4): 18-20.
MLA [1] LIU Sha, et al., "High temperature Sintering of Molybdenum Alloys Containing 3 wt% Rhenium." Rare Metals and Cemented Carbides, no. 4, 1999, pp. 18-20.
APA [1] LIU Sha, CAO Yu, & SHU Jin-bo. (1999). High temperature Sintering of Molybdenum Alloys Containing 3 wt% Rhenium. Rare Metals and Cemented Carbides(4), 18-20.
IEEE [1] LIU Sha, CAO Yu, and SHU Jin-bo, "High temperature Sintering of Molybdenum Alloys Containing 3 wt% Rhenium," Rare Metals and Cemented Carbides, no. 4, pp. 18-20, 1999. keywords: {Low Re Mo alloy;high temperature sintering;grain structure;mechanical property}