Research on the Solution Treatment Process for SiC_P/Al Compositeswith Large Volume Fraction AITranslate
Abstract AITranslate
Study is made on the effect of solution heat treatment process on mechanical properties,the tensile curve and fracture morphology of SiCP/Al composites with the high volume fraction by means of metallographic analysis,Vickers hardness test,tensile test and TEM.The results show that the strength and toughness of composites are in the best condition when the solution temperature is 528 ℃,and the notch bending resistance displacement curve appears flat at high stress,indicating the possibility of improving the material strength and toughness and reducing tendency of the instantaneous destructive fracture through the optimization of the soild-solution treatment parameters.
KeyWords AITranslate
1Ibrahim I A,Mohamed F A,Lavernia E J.Particle reinforced metal matrix composites-review[J].J Mater Sci,1991,26:1137-1156.
2Carl Zweben.Metalmatrix composites for electronic packaging[J].JOM,1992,44(7):15-23.
3吴洁君,王殿斌,桂满昌,袁广江.SiC颗粒增强铝基复合材料磨损表层、亚表层形貌分析[J].材料科学与工程,1999,17(3):74-77. 被引量:27
4Chena Z Z,Tokajib K.Effects of particle size on fatigue crack initiation and small crack growth in SiC particulate-reinforced aluminium alloy composites[J].Mater Let,2004,58:2314-2321.
5谢盛辉,刘红卫,陈康华,李均钦,汤皎宁.固溶时效对高体积比SiC_p/6013Al复合材料导热性能及强度的影响[J].湖南冶金,2003,31(3):16-19. 被引量:4
1张建会,雷玉成,李贤.SiC_p/Al基复合材料等离子弧原位焊接研究[J].热加工工艺,2006,35(23):1-4.
2万薇薇.论自然的生机美[J].才智,2016,0(7):196-197.
3苑敏.赫哲族鱼皮服饰与制作工艺研究[J].边疆经济与文化,2013(5):31-32. 被引量:5
4牛奔玉.分析哲学中的“分析”之意义[J].重庆科技学院学报:社会科学版,2009(12):34-35.
5王妍,罗跃嘉.面孔表情的ERP研究进展[J].中国临床心理学杂志,2004,12(4):428-431. 被引量:16
6刘刚.良丝点染 绣采绚丽 顾绣花鸟鱼虫探微[J].收藏家,2008(1):7-16.
7仪德刚.中国古代计量弓力的方法及相关经验认识[J].力学与实践,2005,27(2):86-90. 被引量:6
8刘吉华,周桂源,陈水友,刘启跃.车轮显微组织对车轮摩擦学性能的影响[J].润滑与密封,2016,41(12):31-36. 被引量:5
9曲墨,邱智东,王伟楠.灵芝菌固体发酵三七药渣工艺研究[J].长春中医药大学学报,2016,32(2):263-265. 被引量:8
10石建高,王鲁民,徐君卓.高强度聚乙烯菱形网目经编网片的力学性能初步研究[J].中国海洋大学学报:自然科学版,2006,36(3):410-414. 被引量:12
Basic Information:
DOI:
Chinese Library Classification Number:B333[哲学宗教—外国哲学]
Citation Information:
Study is made on the effect of solution heat treatment process on mechanical properties,the tensile curve and fracture morphology of SiCP/Al composites with the high volume fraction by means of metallographic analysis,Vickers hardness test,tensile test and TEM.The results show that the strength and toughness of composites are in the best condition when the solution temperature is 528 ℃,and the notch bending resistance displacement curve appears flat at high stress,indicating the possibility of improving the material strength and toughness and reducing tendency of the instantaneous destructive fracture through the optimization of the soild-solution treatment parameters.
quote
| GB/T 7714-2015 | [1] FANG Ling, ZHANG Xiao-lian. Research on the Solution Treatment Process for SiC_P/Al Compositeswith Large Volume Fraction[J]. Rare Metals and Cemented Carbides, 2010(2): 42-44. |
| MLA | [1] FANG Ling, and ZHANG Xiao-lian. "Research on the Solution Treatment Process for SiC_P/Al Compositeswith Large Volume Fraction." Rare Metals and Cemented Carbides, no. 2, 2010, pp. 42-44. |
| APA | [1] FANG Ling, & ZHANG Xiao-lian. (2010). Research on the Solution Treatment Process for SiC_P/Al Compositeswith Large Volume Fraction. Rare Metals and Cemented Carbides(2), 42-44. |
| IEEE | [1] FANG Ling and ZHANG Xiao-lian, "Research on the Solution Treatment Process for SiC_P/Al Compositeswith Large Volume Fraction," Rare Metals and Cemented Carbides, no. 2, pp. 42-44, 2010. keywords: {SiCP/Al composites with high volume fraction;solution treatment;tensile curve;tensile strength;fracture toughness} |