Research and Development of Rare Metal Fine Chemicals─Inorganic Non-metal Material AITranslate
Abstract AITranslate
Rare metal fine chemicals are widely used for new inorganicnon-metal materials,so they are very important for the developmentof modern advanced scientific technology.This paper briefly describesthe recent research and development of new rare metal-containinginorganic non-me tal ma tenals and corresponding fine chemicals.Somerelated literatures are presented for reference.
KeyWords AITranslate
1张文朴.含稀有金属元素的陶瓷颜料和釉料──稀有金属精细化学品系列研究(Ⅱ)[J].稀有金属与硬质合金,1998,26(3):52-58.
2山内昭.日本电渗析技术研究与开发进展[J].水处理技术,1995,21(4):203-207. 被引量:1
3陈旭峰.“八五”期间陶瓷窑用耐火材料的新进展[J].硅酸盐通报,1997,16(1):15-20. 被引量:1
4王杰曾,袁林.新形势下水泥窑用耐火材料的研究与开发进展[J].硅酸盐通报,2016,35(10):3219-3223. 被引量:4
5彭新战,胡道和.磷石膏分解炉的研究与开发进展[J].硫酸工业,1993(5):43-48. 被引量:4
6王存文,张俊峰,孙炜.液相甲醇合成新工艺的工业化研究与开发进展[J].湖北化工,2001,18(1):13-15.
7李春利,孙玉春,王志英,方静.新型立体传质塔板CTST的研究与开发进展[J].河北工业大学学报,2004,33(2):155-162. 被引量:13
8任叶果,黄明智,侯仲轲.四氢酞酰亚胺类除草剂的研究与开发进展[J].精细化工中间体,2004,34(6):7-9. 被引量:5
9金子林,梅建庭,蒋景阳.两相(水-有机)烯烃氢甲酰化研究与开发进展[J].大连理工大学学报,1999,39(2):221-227. 被引量:4
10王强,陈铁亮,周鑫.新型玻璃金水的研制[J].河北陶瓷,1999,27(4):3-8.
Basic Information:
DOI:
Chinese Library Classification Number:TQ13[化学工程—无机化工];TQ174.758[化学工程—陶瓷工业]
Citation Information:
Rare metal fine chemicals are widely used for new inorganicnon-metal materials,so they are very important for the developmentof modern advanced scientific technology.This paper briefly describesthe recent research and development of new rare metal-containinginorganic non-me tal ma tenals and corresponding fine chemicals.Somerelated literatures are presented for reference.
quote
| GB/T 7714-2015 | [1] ZHANG Wen-pu. Research and Development of Rare Metal Fine Chemicals─Inorganic Non-metal Material[J]. Rare Metals and Cemented Carbides, 1995(2): 37-41. |
| MLA | [1] ZHANG Wen-pu. "Research and Development of Rare Metal Fine Chemicals─Inorganic Non-metal Material." Rare Metals and Cemented Carbides, no. 2, 1995, pp. 37-41. |
| APA | [1] ZHANG Wen-pu. (1995). Research and Development of Rare Metal Fine Chemicals─Inorganic Non-metal Material. Rare Metals and Cemented Carbides(2), 37-41. |
| IEEE | [1] ZHANG Wen-pu, "Research and Development of Rare Metal Fine Chemicals─Inorganic Non-metal Material," Rare Metals and Cemented Carbides, no. 2, pp. 37-41, 1995. keywords: {fine chemicals;fine ceramics;rare metal} |