Fluorene Derivatives for Efficient Prompt Scintillation in Plastic Scintillators AITranslate

University of California; University of California; University of California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Plastic scintillators have been investigated for γ-ray detection with the promise of fast response, ease of scale up, and mechanical toughness. However, their low light yield has been a major limiting factor in the performance metrics. Herein, we report a cross-linkable fluorene derivative, 9,9-bis(4-vinylbenzyl)-9H-fluorene (SF), copolymerized with the plastic matrix, to facilitate effective Förster resonance energy transfer to boost the light yield. Noncurable 9,9-dimethyl-9H-fluorene (MF) and 9,9′-spirobifluorene (SBF) were also introduced to bridge the energy transfer gap between the polymer matrix and the primary dye. The plastic scintillator comprising 5 wt % SF and 20 wt % MF exhibits a light yield of 11 600 photons/MeV with a scintillation decay time constant of 2.3 ns.

KeyWords AITranslate

fluorene plastic scintillators organic scintillators light yield FRET energy transfer
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00391

Chinese Library Classification Number:

Citation Information:

Plastic scintillators have been investigated for γ-ray detection with the promise of fast response, ease of scale up, and mechanical toughness. However, their low light yield has been a major limiting factor in the performance metrics. Herein, we report a cross-linkable fluorene derivative, 9,9-bis(4-vinylbenzyl)-9H-fluorene (SF), copolymerized with the plastic matrix, to facilitate effective Förster resonance energy transfer to boost the light yield. Noncurable 9,9-dimethyl-9H-fluorene (MF) and 9,9′-spirobifluorene (SBF) were also introduced to bridge the energy transfer gap between the polymer matrix and the primary dye. The plastic scintillator comprising 5 wt % SF and 20 wt % MF exhibits a light yield of 11 600 photons/MeV with a scintillation decay time constant of 2.3 ns.

quote

GB/T 7714-2015 [1] Ziqing Han, Hao Yu, Qibing Pei. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00391.
MLA [1] Ziqing Han, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00391.
APA [1] Ziqing Han, Hao Yu, & Qibing Pei. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00391
IEEE [1] Ziqing Han, Hao Yu, and Qibing Pei, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00391. keywords: {fluorene;plastic scintillators;organic scintillators;light yield;FRET;energy transfer}